The invention concerns a strip or sheet of ferritic stainless steel of the following composition (% by weight): (C+N)<.060; Si<0.9; Mn<1; Cr=15 to 19; Mo<1; Ni<0.5; Ti<0.1; Cu<0.4; S<0.02; P<0.045; Zr=0.10 to 0.40, and 7(C+N)≦Zr≦7(C+N)+0.15; Nb=0.25 to…
Maitrepierre Philippe
1. Screws, bolts, nuts and other components of steel with high mechanical characteristics which are produced by cold or warm die forging from rolled bar or wire characterised in that they are of the following composition in percent by weight : 0.060 to 0120 ; Si 0.30 to 0.70 ;…
The invention concerns a strip or sheet of ferritic stainless steel of the following composition (% by weight): (C+N)<.060; Si<0.9; Mn<1; Cr=15 to 19; Mo<1; Ni<0.5; Ti<0.1; Cu<0.4; S<0.02; P<0.045; Zr=0.10 to 0.40, and 7(C+N)</=Zr</=7(C+N)+0.15;…
1. A process for arc welding steel strips or sheets in a protective gas atmosphere by fusion of a weld bead characterised in that particles of silica are introduced into the weld bead fusion region, in direct contact with the metal.
The invention relates to a method of making steel bars and tubes with good mechanical characteristics. The process consists of manufacturing a low alloy steel containing 0.06 to 0.12% carbon as well as additions with well-determined contents of Si, Mn, Nb, Al, B and optionally…
The invention relates to a method of making steel bars and tubes with good mechanical characteristics. The process consists of manufacturing a low alloy steel containing 0.06 to 0.12% carbon as well as additions with well-determined contents of Si, Mn, Nb, Al, B and optionally…
1. Screws, bolts, nuts and other components of steel with high mechanical characteristics which are produced by cold or warm die forging from rolled bar or wire characterised in that they are of the following composition in percent by weight : 0.060 to 0120 ; Si 0.30 to 0.70 ;…
1. Screws, bolts, nuts and other components of steel with high mechanical characteristics which are produced by cold or warm die forging from rolled bar or wire characterised in that they are of the following composition in percent by weight : 0.060 to 0120 ; Si 0.30 to 0.70 ;…
A grade of ferritic stainless steel sheet making it possible to avoid or very greatly limit the polishing work after deep-drawing of a receptacle such as a saucepan. The sheet of the invention, 0.4 to 1.5 mm in thickness, has a crystalline orientation texture of cubic type on…
Method for producing bars or rod wire having in the raw hot transformation state specially high mechanical characteristics. The method for producing steel bars or rod wire having after hot bonding and cooling a bainitic structure and characteristics: R >= 1000 Mpa, E >=…
Method for producing bars or rod wire having in the raw hot transformation state specially high mechanical characteristics. The method for producing steel bars or rod wire having after hot bonding and cooling a bainitic structure and characteristics: R >= 1000 Mpa, E >=…
The invention concerns a strip or sheet of ferritic stainless steel of the following composition (% by weight): (C+N)<.060; Si<0.9; Mn<1; Cr=15 to 19; Mo<1; Ni<0.5; Ti<0.1; Cu<0.4; S<0.02; P<0.045; Zr=0.10 to 0.40, and 7(C+N)</=Zr</=7(C+N)+0.15;…
The invention concerns a strip or sheet of ferritic stainless steel of the following composition (% by weight): (C+N)<.060; Si<0.9; Mn<1; Cr=15 to 19; Mo<1; Ni<0.5; Ti<0.1; Cu<0.4; S<0.02; P<0.045; Zr=0.10 to 0.40, and 7(C+N)</=Zr</=7(C+N)+0.15;…
The invention relates to a method of making steel bars and tubes with good mechanical characteristics. The process consists of manufacturing a low alloy steel containing 0.06 to 0.12% carbon as well as additions with well-determined contents of Si, Mn, Nb, Al, B and optionally…
1. Screws, bolts, nuts and other components of steel with high mechanical characteristics which are produced by cold or warm die forging from rolled bar or wire characterised in that they are of the following composition in percent by weight : 0.060 to 0120 ; Si 0.30 to 0.70 ;…
The invention concerns a strip or sheet of ferritic stainless steel of the following composition (% by weight): (C+N)<.060; Si<0.9; Mn<1; Cr=15 to 19; Mo<1; Ni<0.5; Ti<0.1; Cu<0.4; S<0.02; P<0.045; Zr=0.10 to 0.40, and 7(C+N)</=Zr</=7(C+N)+0.15;…
The invention relates to a method of making steel bars and tubes with good mechanical characteristics. The process consists of manufacturing a low alloy steel containing 0.06 to 0.12% carbon as well as additions with well-determined contents of Si, Mn, Nb, Al, B and optionally…
1. Screws, bolts, nuts and other components of steel with high mechanical characteristics which are produced by cold or warm die forging from rolled bar or wire characterised in that they are of the following composition in percent by weight : 0.060 to 0120 ; Si 0.30 to 0.70 ;…
The invention concerns a strip or sheet of ferritic stainless steel of the following composition (% by weight): (C+N)<.060; Si<0.9; Mn<1; Cr=15 to 19; Mo<1; Ni<0.5; Ti<0.1; Cu<0.4; S<0.02; P<0.045; Zr=0.10 to 0.40, and 7(C+N)</=Zr</=7(C+N)+0.15;…
The invention concerns a strip or sheet of ferritic stainless steel of the following composition (% by weight): (C+N)<.060; Si<0.9; Mn<1; Cr=15 to 19; Mo<1; Ni<0.5; Ti<0.1; Cu<0.4; S<0.02; P<0.045; Zr=0.10 to 0.40, and 7(C+N)</=Zr</=7(C+N)+0.15;…
The invention relates to a method of making steel bars and tubes with good mechanical characteristics. The process consists of manufacturing a low alloy steel containing 0.06 to 0.12% carbon as well as additions with well-determined contents of Si, Mn, Nb, Al, B and optionally…
Le procédé de la présente invention concerne une méthode de fabrication de barres ou de fil machine ayant dans l'état brut de transformation à chaud des caractéristiques mécaniques spécialement élevées. Le procédé, fournissant des barres ou fil machine en acier ayant après…
The invention concerns a strip or sheet of ferritic stainless steel of the following composition (% by weight): (C+N)<.060; Si<0.9; Mn<1; Cr=15 to 19; Mo<1; Ni<0.5; Ti<0.1; Cu<0.4; S<0.02; P<0.045; Zr=0.10 to 0.40, and 7(C+N)</=Zr</=7(C+N)+0.15;…