Uranium and vanadium are recovered from carnotite ores by leaching the roasted ores with alkali metal carbonate solution, for example 5-10% sodium carbonate solution, and absorbing the dissolved uranium and vanadium values on an anion exchange resin from which the uranium and…
Long Ray Smith
Molybdenum values are recovered from oxidic ores and minerals by treatment at 200-800 DEG C. with substantially enhydrous HCl or mixtures containing 0.5 to 4 parts HCl and 0.1 to 2 parts Cl2, removing the oxychloride formed while maintaining the temperature in the same range and…
Pigment grade titanium dioxide is prepared by treating a titaniferous material with sulphuric acid at 40-80 DEG C., leaching with water, selectively extracting titanium values with a liquid mono- or di-alkyl orthophosphoric acid, or contaminants with an alkyl phosphate or alkyl…
A pigment grade, crystalline, acicular titanium dioxide having a cross-sectional diameter of 0.05-0.2 m , a length of 0.3-1.5 m , with a length: diameter ratio of 3-15, is prepared by mixing an aqueous colloidal suspension of TiO2, nucleating seed particles, prepared by heating…
Uranium values are recovered from an impure source material by leaching with hydrochloric acid and an oxidizing agent increasing the chloride ion concentration to above 5M to convert the uranium to an uranyl chloride complex anion which is then adsorbed on an anion exchange…
1,182,457. Hydrogen peroxide. DOW CHEMICAL CORP. 21 March, 1967, No. 13135/67. Heading C1A. An amalgam containing up to 0À2 wt. per cent of sodium, or potassium, metal is oxidized with dry air and/or oxygen at below 80‹ C. for not more than 5 minutes and then contacted with a…