An untwisted hollow blade with internal reinforcing ribs is formed by diffusion bonding two halves. A predominate portion of the blade twist is accomplished by gravity creep deforming against a supporting die, aided by applying twisting moments at the ends. The blade is free to…
Leibfried Peter E
A process is described for producing hollow articles from high strength, high temperature metals such as titanium alloys. A finite element analysis is used to determine a preform configuration in which the external surface of the finished article is translated into a flat plane.…
An untwisted hollow blade (66) with internal reinforcing ribs is formed by diffusion bonding two halves. A predominate portion of the blade twist is accomplished by gravity creep deforming against a supporting die (90), aided by applying twisting moments at the ends. The blade…
A hollow element such as a turbine blade is manufactured by cutting a metallic member into first and second pieces so that each has a cut side and an opposite uncut side. The cut sides are machined to form interior features of the element. The uncut sides are machined to form…
A method of repairing a defect in a component includes forming a slot in the component, thereby removing at least a substantial part of the defect from the component, where the slot has a predetermined geometry.
A titanium gas injection tube 18 is located within a counterbore (16) in the blade (10) halves which are to be bonded and formed. An internal stainless steel sleeve (24) is placed in the counterbore inside the titanium tube to resist bonding forces. An external stainless steel…
A method for repairing a component having first and second major surfaces, a thickness between the major surfaces, and an edge, is characterized by utilizing a template to determine if the component is suitable for repair, and forming a slot cut entirely through the thickness of…
<P>PROBLEM TO BE SOLVED: To provide method and system for repairing a defective part of a component. <P>SOLUTION: In this method, a slot 30 is formed in the component to eliminate at least a substantial part of the defective part. The slot 30 includes shapes of an…
A method for repairing a defect in a component having a first major surface and a second major surface, a thickness defined between the major surfaces, and an edge adjoining both the major surfaces is characterized by forming a slot cut entirely through the thickness of the…
A method of repairing a defect (18) in a component (10) includes forming a slot (30; 78) in the component (10), thereby removing at least a substantial part of the defect (18) from the component (10), where the slot (30; 78) has a predetermined geometry.
A titanium gas injection tube (18) is located within a counterbore (16) in the blade (10) halves which are to be bonded and formed. An internal stainless steel sleeve (24) is placed in the counterbore inside the titanium tube to resist bonding forces. An external stainless steel…
A method of forming a component (100) having an airfoil (102) includes the steps of a) molding an airfoil preform (112) such that it has an airfoil (102) extending radially, and between a leading edge (103) and a trailing edge (105), with at least one of the leading and trailing…
<P>PROBLEM TO BE SOLVED: To provide a method for easily manufacturing a hollow member such as a turbine blade. <P>SOLUTION: A hollow member such as a turbine blade is manufactured by cutting a metal member into a first part and a second part in a manner to have an…
A method of repairing a defect in a component includes forming a slot in the component, thereby removing at least a substantial part of the defect from the component, where the slot has a predetermined geometry.
A method of forming a component having an airfoil includes the steps of a) molding an airfoil preform such that it has an airfoil extending radially, and between a leading edge and a trailing edge, with at least one of the leading and trailing edges being formed with a mold…
A titanium gas injection tube (18) is located within a counterbore (16) in the blade (10) halves which are to be bonded and formed. An internal stainless steel sleeve (24) is placed in the counterbore inside the titanium tube to resist bonding forces. An external stainless steel…