This substantially water-free method for preparing high density igniter granules involves uniformly coating fuel and oxidizer particulates dispersed in a non-solvent with a thermoplastic elastomer solution to produce coated igniter granules exhibiting substantially uniform size…
Lee Kenneth E
A closure assembly for a furnace wall in which a plug member is secured to a shell member which, in turn, is pivotally mounted to the furnace wall. The plug member is formed from a cast ceramic fiber tamping mix of bulk fiber and high temperature inorganic binders and has a…
A water slurry method of making high performance explosive compositions and ordnances using the explosive compositions as an explosive ingredient for high performance, low sensitivity explosive applications is disclosed. The method involves combining an aqueous dispersion…
High performance explosive compositions and ordnances using the explosive compositions as an explosive ingredient for high performance, low sensitivity explosive applications are disclosed. The explosive formulation includes CL-20 as an explosive ingredient, and a binder system…
High performance explosive compositions and ordnances using the explosive compositions as an explosive ingredient for high performance, low sensitivity explosive applications are disclosed. The explosive formulation includes CL-20 as an explosive ingredient, and a binder system…
This substantially water-free method for preparing high density igniter granules involves uniformly coating fuel and oxidizer particulates dispersed in a non-solvent with a thermoplastic elastomer solution to produce coated igniter granules exhibiting substantially uniform size…
Digital metamorphic alloy (DMA) buffer structures for transitioning from a bottom crystalline layer to a lattice mismatched top crystalline layer, and methods for manufacturing such layers are described. In some embodiments, a layered crystalline structure includes a first layer…
An explosive composition is provided that includes 85 to about 96 weight percent nitramine, based on the total composition weight, and about 4 to 15 weight percent plasticized binder. At least 80 weight percent of the total composition weight, and more preferably 85 to 96 weight…
A composition C-4 substitute is provided, the substitute include 2,4,6,8,10,12-hexanitro-2,4,6,8,10,12-hexaazatetracyclo[5.5.0.0 5,9 0 3,11 ]-dodecane (CL-20), optionally one or more nitramines other than CL-20, and silicone fluid. Also provided is an additive composition…
An explosive composition is provided that includes 85 to about 96 weight percent nitramine based on the total composition weight, and about 4 to 15 weight percent plasticized binder. At least 80 weight percent of the total composition weight, and more preferably 85 to 96 weight…
An explosive composition is provided that includes 85 to about 96 weight percent nitramine, based on the total composition weight, and about 4 to 15 weight percent plasticized binder. At least 80 weight percent of the total composition weight, and more preferably 85 to 96 weight…
An explosive composition is provided that includes 85 to about 96 weight percent nitramine based on the total composition weight, and about 4 to 15 weight percent plasticiyed binder. At least 80 weight percent of the total composition weight, and more preferably 85 to 96 weight…
A composition C-4 substitute is provided, the substitute include 2,4,6,8,10, 12-hexanitro-2,4,6,8,10, 12-hexaazatetracyclo(5.5.0.05,9,3,11)-dodecane (CL- 20), optionally one or more nitramines other than CL-20, and silicone fluid. Also provided is an additive composition…
High performance explosive compositions and ordnances using the explosive compositions as an explosive ingredient for high performance, low sensitivity explosive applications are disclosed. The explosive formulation includes CL-20 as an explosive ingredient, and a binder system…
A composition C-4 substitute is provided, the substitute include 2,4,6,8,10, 12-hexanitro-2,4,6,8,10, 12-hexaazatetracyclo(5.5.0.0?5,9,3,11¿)-dodecane (CL-20), optionally one or more nitramines other than CL-20, and silicone fluid. Also provided is an additive composition…
An explosive composition is provided that includes 85 to about 96 weight percent nitramine based on the total composition weight, and about 4 to 15 weight percent plasticiyed binder. At least 80 weight percent of the total composition weight, and more preferably 85 to 96 weight…
A composition C4 substitute is provided, the substitute including 2,4,6,8,10,12-hexanitro-2,4,6,8,10,12-hexaazatetracyclo[5.5.0.0 5,9 0 3,11 ]-dodecane (CL-20), optionally one or more nitramines other than CL-20, and silicone fluid. Also provided is an additive composition…
This substantially water-free method for preparing high density igniter granules involves uniformly coating fuel and oxidizer particulates dispersed in a non-solvent with a thermoplastic elastomer solution to produce coated igniter granules exhibiting substantially uniform size…