A process for producing an MAS glass is described wherein 10 to 40 mol % of MgO, 5 to 30 mol % of Al 2 O 3 and 40 to 70 mol % of SiO 2 or precursors of these raw materials are mixed, the mixture is melted, the melt is cooled and comminuted to afford particles of less than 10 mm,…
Inventor / Author Profile
Lars ORTMANN
0Total Forward Citations
1Indexed Patents
0Patent H-Index