A process for producing silicon wafers with low defect density is one wherein a) a silicon single crystal having an oxygen doping concentration of at least 4*10 17 /cm 3 is produced by molten material being solidified to form a single crystal and is then cooled, and the holding…
Lambert Ulrich
Production of silicon wafers comprises: (a) forming a silicon single crystal having an oxygen doping concentration of 4 x 10<17>/cm<3>, in which a molten material is solidified to a single crystal and cooling for 80 minutes at 850-1100 degrees C; (b) processing the…
PROBLEM TO BE SOLVED: To make a defect density smaller and to obtain a silicon semiconductor wafer having satisfactory gate oxidized film perfectivity by doping a silicon single crystal with oxygen and nitrogen of respective specific concns. while this single crystal is pulled…
A silica glass crucible is produced by a) providing a porous amorphous silica glass green body, which is infiltrated with at least one substance that promotes crystallization of a silica glass crucible, b) drying the infiltrated silica glass green body, c) filling the green body…
Silicon single crystal production involves doping the growing crystal with specified high nitrogen and low oxygen concentrations. Silicon single crystal production by the Czochralski method involves doping the growing crystal with less than 6.5 x 10<17> atoms/cm<3>…
<P>PROBLEM TO BE SOLVED: To provide a SOI wafer which includes an electric insulation layer having a high heat transfer coefficient and whose high yield is secured in the succeeding manufacturing of electric components. <P>SOLUTION: The SOI wafer includes a carrier…
Verfahren zur Herstellung eines Kieselglastiegels, dadurch gekennzeichnet, daß DOLLAR A a) ein poröser amorpher Kieselglasgrünkörper hergestellt wird, der mit mindestens einer Substanz infiltriert ist, die eine Kristallisation eines Kieselglastiegels fördert DOLLAR A b) der…
An SOI wafer, includes a substrate made from silicon, an electrically insulating layer with a thermal conductivity of at least 1.6 W/(Km) and a single-crystal silicon layer with a thickness of from 10 nm to 10 μm, a standard deviation of at most 5% from the mean layer thickness…
The method involves applying one or more voltage pulses of predefined pulse amplitude and duration to the capacitor. A map of the gate oxide defects is then produced using an imaging process, e.g. electron beam induced current imaging or optical beam induced current imaging.…
Monocrystalline semiconductor wafers have defect-reduced regions, the defect-reduced regions having a density of GOI-relevant defects within the range of 0/cm 2 to 0.1/cm 2 and occupy overall an areal proportion of 10% to 100% of the planar area of the semiconductor wafer,…
A silica glass crucible is produced by a) providing a porous amorphous silica glass green body, which is infiltrated with at least one substance that promotes crystallization of a silica glass crucible, b) drying the infiltrated silica glass green body, c) filling the green body…
In a process for producing silicon semiconductor wafers, a silicon single crystal is pulled using the Czochralski method and is processed to form semiconductor wafers, a ratio V/G of pulling rate V and axial temperature gradient G at a growth front during the pulling of the…
An SOI wafer, includes a substrate made from silicon, an electrically insulating layer with a thermal conductivity of at least 1.6 W/(Km) and a single-crystal silicon layer with a thickness of from 10 nm to 10 μm, a standard deviation of at most 5% from the mean layer thickness…
Manufacture of a crucible from fused quartz comprises: (a) fabricating a green compact from porous, amorphous, fused quartz permeated with a substance promoting crystallisation of the crucible; (b) drying the obtained compact, (c) filling the compact with metal or metalloid; and…
The invention relates to a process for producing silicon wafers with low defect density. The process is one wherein (a) a silicon single crystal having an oxygen doping concentration of at least 4x10<17>/cm<3> is produced by molten material being solidified to form a…
In a process for producing silicon semiconductor wafers, a silicon single crystal is pulled using the Czochralski method and is processed to form semiconductor wafers, a ratio V/G of pulling rate V and axial temperature gradient G at a growth front during the pulling of the…
Die Erfindung bezieht sich auf eine SOI-Scheibe, umfassend einen Träger aus Silicium, eine elektrisch isolierende Schicht mit einer thermischen Leitfähigkeit von wenigstens 1,6 W/(Km) und eine einkristalline Siliciumschicht mit einer Dicke von 10 nm bis 10 mum mit einer…
L'invention concerne une tranche SOI, comprenant un support en silicium, une couche isolante électrique présentant une conductibilité thermique d'au moins 1,6 W/(Km) et une couche de silicium monocristallin d'une épaisseur de 10 nm à 10 m avec un écart standard…
PROBLEM TO BE SOLVED: To provide a process that can produce silicon semiconductor wafers that can minimize the defect density as much as possible and includes a satisfactory amount of GOI. SOLUTION: In the production process of silicon single crystal that is pulled up through…
Die Erfindung bezieht sich auf eine monokristalline Halbleiterscheibe, die defektreduzierte Bereiche aufweist, wobei diese defektreduzierten Bereiche eine Dichte der GOI-relevanten Defekte im Bereich von 0/cm<SUP>2</SUP> bis 0,1/cm<SUP>2</SUP> aufweisen…
<P>PROBLEM TO BE SOLVED: To provide an optimized manufacturing method of a silicon wafer which can obtain the silicon wafer in which oxygen doping concentration having low defect density is at least 4 × 10<SP>17</SP>/cm<SP>3</SP>in especially near…
<P>PROBLEM TO BE SOLVED: To provide a semiconductor wafer that does not cause any problem in the case where further size miniaturization is performed. <P>SOLUTION: This invention is related to the single crystal semiconductor wafer having a region where defects are…