A powder of tantalum, niobium, or an alloy thereof, having an oxygen content less than about 300 ppm, and the production thereof without exposure to a temperature greater than about 0.7 T H . A powder metallurgy formed product of tantalum, niobium, or an alloy thereof, having an…
Kumar Prabhat
Tantalum electrode material is produced which has extremely low tortuosity, exceptionally low ESL and ESR, potentially extended high frequency performance, very high volumetric efficiency, and reduced tantalum consumption per electrode. The electrode material is characterized by…
A wrought metal alloy product having a tantalum or niobium base metal, 10 to 1000 ppm silicon, and 10 to 10000 ppm yttrium nitride. Fine uniform grain size contributes to improved ductility.
The invention relates to a sputtering target which has a fine uniform equiaxed grain structure of less than 44 microns, no preferred texture orientation as measured by electron back scattered diffraction (“EBSD”) and that displays no grain size banding or texture banding…
A method of making sheet bar and other precursors of formed products to be made by extensive working. The method includes providing a powder metal, preferably under 100 PPM oxygen content of non-spherical particles, compacting the powder into a coherent precursor form of at…
One step process for producing formed Ta/Nb powder metallurgy products using Ta and/or Nb hydride powders with an oxygen content greater than a target level, e.g., 300 ppm, heating the metal hydride in the presence of another metal having a higher affinity for oxygen, removing…
A method ( 10 ) of forming sputtering target ( 11 ) from ingots of tantalum or niobium of requisite purity by the process of cutting the ingot to short lengths ( 12 ) and pressure working ( 14, 22, 30, 34 ) the ingot along alternating essentially orthogonal work axes.…
A method and system of hybrid dicing using a blade and laser are described. In one embodiment, a method involves focusing a laser beam inside the substrate in regions between the integrated circuits, inducing defects inside the substrate in the regions. The method also involves…
A method of making sheet bar and other precursors of formed products to be made by extensive working. The method includes providing a powder metal, preferably under 100 PPM oxygen content of non-spherical particles, compacting the powder into a coherent precursor form of at…
A process to chemically refine and consolidate tantalum, niobium and their alloys to a fabricated product of net shape or near-net shape with higher throughput, more consistency, and lower manufacturing costs compared to prior art routes or rejuvenate damaged and deteriorated…
Molybdenum, sputtering targets and sintering characterized as having no or minimal texture banding or through thickness gradient. The molybdenum sputtering targets having a fine, uniform grain size as well as uniform texture, are high purity and can be micro-alloyed to improved…
A powder of tantalum, niobium, or an alloy thereof, having an oxygen content less than about 300 ppm, and the production thereof without exposure to a temperature greater than about 0.7 T H . A powder metallurgy formed product of tantalum, niobium, or an alloy thereof, having an…
Molybdenum titanium sputter targets are provided. In one aspect, the targets are substantially free of the β(Ti, Mo) alloy phase. In another aspect, the targets are substantially comprised of single phase β(Ti, Mo) alloy. In both aspects, particulate emission during sputtering…
Embodiments of the present invention are directed to processes for making solar cells by simultaneously co-firing metal layers disposed both on a first and a second surface of a bifacial solar cell substrate. Embodiments of the invention may also provide a method forming a solar…
The invention relates to high purity MoO 2 powder by reduction of ammonium molybdate or molybdenum trioxide using hydrogen as the reducing agent in a rotary or boat furnace. Consolidation of the powder by press/sintering, hot pressing, and/or HIP is used to make discs, slabs, or…
Molybdenum sputtering targets and sintering characterized as having no or minimal texture banding or through thickness gradient. The molybdenum sputtering targets having a fine, uniform grain size as well as uniform texture, are high purity and can be micro-alloyed to improved…
A process for producing a wrought product of improved ductility from substantially noncompactible prealloyed metal powder. The process comprises the steps of: comminuting substantially noncompactible prealloyed metal powder so as to flatten the particles thereof; heating the…
Refractory metal products, such as tantalum on non-refractory conductive metal backings, e.g. copper, can be rejuvenated after metal consumption in selected zones by powder filling the zones and high energy heating at high scan speed to sinter the added powder, without complete…
The present invention relates to novel fused pyridazine compounds, their pharmaceutically acceptable salts, and their isomers, stereoisomers, conformers, tautomers, polymorphs, hydrates and solvates. The present invention also encompasses pharmaceutically acceptable compositions…
The present invention is directed to a composition consisting essentially of: a) from about 0.1 to about 60 mole % of MoO 2 , b) from 0 to about 99.9 mole % of In 2 O 3 , c) from 0 to about 99.9 mole % of SnO 2 , d) from 0 to about 99.9 mole % of ZnO, e) from 0 to about 99.9…
Disclosed is a process for the reprocessing or production of a sputter target or an X-ray anode wherein a gas flow forms a gas/powder mixture with a powder of a material chosen from the group consisting of niobium, tantalum, tungsten, molybdenum, titanium, zirconium, mixtures of…
A wrought metal alloy product having a tantalum or niobium base metal, 25 to 1000 ppm silicon, and 25 to 1000 ppm molybdenum. Fine uniform grain size contributes to improved tensile strength, processability, and high temperature stability.
Improved wafer coating processes, apparatuses, and systems are described. In one embodiment, an improved spin-coating process and system is used to form a mask for dicing a semiconductor wafer with a laser plasma dicing process. In one embodiment, a spin-coating apparatus for…
Methods of dicing semiconductor wafers, each wafer having a plurality of integrated circuits, are described. In an example, a method of dicing a semiconductor wafer having a plurality of integrated circuits involves forming a mask above the semiconductor wafer, the mask…
Improved wafer coating processes, apparatuses, and systems are described. In one embodiment, an improved spin-coating process and system is used to form a mask for dicing a semiconductor wafer with a laser plasma dicing process. In one embodiment, a spin-coating apparatus for…