A magnetic element is disclosed wherein first and second interfaces of a free layer with a Hk enhancing layer and tunnel barrier, respectively, produce enhanced surface perpendicular anisotropy to lower switching current or increase thermal stability in a magnetic tunnel…
Kula Witold
We describe the structure and method of forming a STT-MTJ MRAM cell that utilizes transfer of spin angular momentum as a mechanism for changing the magnetic moment direction of a free layer. The device includes an IrMn pinning layer, a SyAP pinned layer, a naturally oxidized,…
A STT-RAM MTJ is disclosed with a MgO tunnel barrier formed by natural oxidation and containing an oxygen surfactant layer to form a more uniform MgO layer and lower breakdown distribution percent. A CoFeB/NCC/CoFeB composite free layer with a middle nanocurrent channel layer…
A composite hard mask is disclosed that prevents build up of metal etch residue in a MRAM device during etch processes that define an MTJ shape. As a result, MTJ shape integrity is substantially improved. The hard mask has a lower non-magnetic spacer, a middle conductive layer,…
A STT-RAM MTJ that minimizes spin-transfer magnetization switching current (Jc) is disclosed. The MTJ has a MgO tunnel barrier layer formed with a natural oxidation process to achieve a low RA (10 ohm-um 2 ) and a Fe or Fe/CoFeB/Fe free layer which provides a lower intrinsic…
A magnetic element is disclosed that has a composite free layer with a FM1/moment diluting/FM2 configuration wherein FM1 and FM2 are magnetic layers made of one or more of Co, Fe, Ni, and B and the moment diluting layer is used to reduce the perpendicular demagnetizing field. As…
An MTJ cell without footings and free from electrical short-circuits across a tunneling barrier layer is formed by using a Ta hard mask layer and a combination of etches. A first etch patterns the Ta hard mask, while a second etch uses O 2 applied in a single high power process…
A composite hard mask is disclosed that enables sub-100 nm sized MTJ cells to be formed for advanced devices such as spin torque MRAMs. The hard mask has a lower non-magnetic metallic layer such as Ru to magnetically isolate an overlying middle metallic spacer such as MnPt from…
A method for forming a MTJ in a STT-MRAM is disclosed in which the easy-axis CD is determined independently of the hard-axis CD. One approach involves two photolithography steps each followed by two plasma etch steps to form a post in a hard mask which is transferred through a…
A STT-MTJ MRAM cell that utilizes transfer of spin angular momentum as a mechanism for changing the magnetic moment direction of a free layer includes an IrMn pinning layer, a SyAP pinned layer, a naturally oxidized, crystalline MgO tunneling barrier layer that is formed on an…
A STT-RAM MTJ is disclosed with a MgO tunnel barrier formed by a NOX process, a CoFeB/FeSiO/CoFeB composite free layer with a middle nanocurrent channel layer to minimize Jc 0 , and a Ru capping layer to enhance the spin scattering effect and increase dR/R. Good write margin is…
A boron or boron containing dusting layer such as CoB or FeB is formed along one or both of top and bottom surfaces of a free layer at interfaces with a tunnel barrier layer and capping layer to improve thermal stability while maintaining other magnetic properties of a MTJ…
A magnetic element is disclosed wherein first and second interfaces of a free layer with a Hk enhancing layer and tunnel barrier, respectively, produce enhanced surface perpendicular anisotropy to lower switching current or increase thermal stability in a magnetic tunnel…
A MTJ for a spintronic device is disclosed and includes a thin seed layer that enhances perpendicular magnetic anisotropy (PMA) in an overlying laminated layer with a (Co/Ni) n composition or the like where n is from 2 to 30. The seed layer is preferably NiCr, NiFeCr, Hf, or a…
An MTJ cell without footings and free from electrical short-circuits across a tunneling barrier layer is formed by using a Ta hard mask layer and a combination of etches. A first etch patterns the Ta hard mask, while a second etch uses O 2 applied in a single high power process…
A CoFeB or CoFeNiB magnetic layer wherein the boron content is 25 to 40 atomic % and with a thickness <20 Angstroms is used to achieve high perpendicular magnetic anisotropy and enhanced thermal stability in magnetic devices. A dusting layer made of Co, Ni, Fe or alloy…
A magnetic element is disclosed that has a composite free layer with a FM1/moment diluting/FM2 configuration wherein FM1 and FM2 are magnetic layers made of one or more of Co, Fe, Ni, and B and the moment diluting layer is used to reduce the perpendicular demagnetizing field. As…
A CoFeB or CoFeNiB magnetic layer wherein the boron content is 25 to 40 atomic % and with a thickness <20 Angstroms is used to achieve high perpendicular magnetic anisotropy and enhanced thermal stability in magnetic devices. A dusting layer made of Co, Ni, Fe or alloy…
A composite hard mask is disclosed that enables sub-100 nm sized MTJ cells to be formed for advanced devices such as spin torque MRAMs. The hard mask has a lower non-magnetic metallic layer such as Ru to magnetically isolate an overlying middle metallic spacer such as MnPt from…
A composite hard mask is disclosed that prevents build up of metal etch residue in a MRAM device during etch processes that define an MTJ shape. As a result, MTJ shape integrity is substantially improved. The hard mask has a lower non-magnetic spacer, a middle conductive layer,…
A MTJ for a spintronic device is disclosed and includes a thin seed layer that enhances perpendicular magnetic anisotropy (PMA) in an overlying laminated layer with a (Co/Ni) n composition or the like where n is from 2 to 30. The seed layer is preferably NiCr, NiFeCr, Hf, or a…
A method for forming a MTJ in a STT-MRAM is disclosed in which the easy-axis CD is determined independently of the hard-axis CD. One approach involves two photolithography steps each followed by two plasma etch steps to form a post in a hard mask which is transferred through a…
Enhanced Hc and Hk in addition to higher thermal stability to 400° C. are achieved in magnetic devices by adding dusting layers on top and bottom surfaces of a spacer in a synthetic antiferromagnetic (SAF) structure to give a RL1/DL1/spacer/DL2/RL2 reference layer configuration…
Methods for patterning a magnetic cell junction and a topography used for and/or resulting from such methods are provided. In particular, a method is provided which includes etching portions of a topography adjacent to a patterned photoresist layer to a level within a cap film…
Enhanced Hc and Hk in addition to higher thermal stability to 400° C. are achieved in magnetic devices by adding dusting layers on top and bottom surfaces of a spacer in a synthetic antiferromagnetic (SAF) structure to give a RL1/DL1/spacer/DL2/RL2 reference layer configuration…