Patents
CH 505,902 A#68239093 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCH · Utility
Ledeburite tool steel articles

(Semi)finished articles of high quality with increased working-life and absence of defects are produced by process in which ledeburite tool steel, esp. high speed tool steel, blanks are made for continuous re-casting, continuously melted and melt led to water-cooled ingot mould…

CH 532,124 A#102046421 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCH · Utility
Waste reducing manufacture of high alloy - steel products

High-alloy steel containing at least 20% total of nickel and chromium is cast by passing it through a water-cooled zone, particularly in a continuous casting process, and is then annealed above 1150 degrees C until the degree of segregation of nickel or chromium measured by…

CH 533,681 A#115369599 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCH · Utility
Cast steel ingot finishing - by re-melting blanks chill-casting, annealing and hot-working

Cast steel ingots contg. >0.5% minute steel impurities or alloying elements and which can be brought to a one-phase zone by heating to a temp. between 1150 degrees C up to solidus temp., are (semi-)finished to a fine-grained structure by (a) prepg. a blank, suitable for a…