Patents
DD 144,655 A1#35331348 Most Cited · 2 citations0.0/yr · PR 1.35PendingDD · Application
Schweissdraht fuer das elektrische lichtbogenschweissen unter schutzgas

Die Erfindung bezieht sich auf einen Schweißdraht, vorzugsweise für das Metall-Aktivgas-Schweißen (MAG), insbesondere in senkrechter Schweißposition. Ziel ist, einen titanhaltigen Schweißdraht zu schaffen, der unter Beibehaltung seines positiven Einflusses auf die Gütewerte das…

DE 4,017,899 C1#37287843 Most Cited · 2 citations0.1/yr · PR 1.11ExpiredDE · Utility
Extn. of silver and gold from ores - by contacting ore with aq. leaching soln. contg. cyanide in presence of peroxo:borate, and sepg. cyano complexes formed

Au and Ag are leached from particulate cuts and cut concentrates contg. at least one of these metals by intimate contact with an aq. leaching soln. contg. 0.005-2.5 wt.% cyanide and having a pH of 8-13, in the presence of at least one peroxoborate cpd. liberating O. The amt. of…

CA 2,043,654 A1#46491995 Most Cited · 1 citations0.0/yr · PR 1.17PendingCA · Application
Process for leaching of precious metals

A process is disclosed for the leaching of gold and silver from ores and ore concentrates through intimate contact of the ore or ore concentrate with an aqueous leach solution containing cyanide. The leach solution has a pH of 8 to 13. The leaching process takes place in the…

CA 2,043,654 C#92620404 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Process for leaching of precious metals
Inventors: Diehl Manfred, Konig Karl-heinz, Krone Eckhard, Lorosch Jurgen, Steinar NorbertAssignee: Manfred Diehl, Karl-Heinz KonigFiled 1991-05-31 · Granted 2003-01-14

A process is disclosed for the leaching of gold and silver from ores and ore concentrates through intimate contact of the ore or ore concentrate with an aqueous leach solution containing cyanide. The leach solution has a pH of 8 to 13. The leaching process takes place in the…

CA 2,050,529 A1#112386642 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Process for the removal of oxygen from cyanide leaching solutions containing noble metals before cementation of the noble metals with zinc

Abstract In the Merrill-Crowe process for the removal of noble metals from cyanide leaching solutions by cementation with zinc, the dissolved oxygen has to be removed. According to the invention, oxygen scavengers are used to reduce the oxygen instead of the degassing technique…

CA 2,050,531 A1#145344143 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Use of formamidine sulfuric acid as an oxygen scavenger

Abstract The invention relates to the use of formamidine sulfinic acid as an oxygen scavenger, preferably in aqueous systems in the alkaline pH range. Formamidine sulrinic acid is effective at low temperatures and does not require the presence of catalytically active metals.…

DD 147,552 A1#85928781 Most Cited · 0 citations0.0/yr · PR 0.56PendingDD · Application
Kaltstauchstahl fuer normteile

Die Erfindung betrifft einen Kaltstauchstahl fuer komplizierte Normteile, insbesondere Kreuzschlitzschrauben, die durch mehrstufiges Kaltverformen hergestellt werden. Die Erfindung bezweckt, eine Stahlzusammensetzung zu finden, bei der auf das Rekristallisationsgluehen…

DE 4,028,239 A1#71391152 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Formamidine sulphinic acid used as oxygen@ binder - pref. in aq. alkaline soln. esp. cyanide soln. contg. noble metal cyano complex for cementation with zinc@

The use of formamidinesulphinic acid (I) as O2 binder is claimed. USE/ADVANTAGE - (I) is claimed for use as O2 binder in aq. alkaline soln., esp. in a cyanide lixiviation soln. contg. noble metal cyano complex, before pptn. of the noble metal by cementation with Zn. It is very…

DE 4,028,240 A1#72172738 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Oxygen@ removal from alkaline cyanide soln. contg. noble metal - using oxygen binder and opt. heavy metal catalyst, reducing zinc@ consumption in cementation

Removal of O2 from cyanide lixiviation soln. contg. noble metal before noble metal cementation with Zn involves reducing dissolved O2 at pH 9-14 by adding 1-5 times the stoichiometric amt. of O2 binder (I) for quantitative redn. of O2 and, if necessary, an effective amt. of…