US 8,142,752 B2#16159254 Most Cited · 7 citations0.5/yr · PR 1.26ActiveUS · Utility
Method of preparation of talcum product with high purity degree
Inventors: Kovanda Ivan, Benkovsky Leo, Pobis Karol, Nemec Jiri, Ondrasikova JanaAssignee: Kovanda Ivan, Benkovsky LeoFiled 2008-02-26 · Granted 2012-03-27

The method which is the subject of protection is characteristic by the fact that firstly is made the suspension consisting of 10 to 20 mass % of mineral talc and 80 to 90 mass % of water; resulting suspension is homogenized and thereafter is heated to the temperature 50° to 70°…

WO 9,520,542 A1#28015561 Most Cited · 3 citations0.1/yr · PR 1.71PendingWO · Application
Method of treatment of talc

The way of talc treatment consists in the mixing-up 74 up to 89 weight % of water, 10 up to 20 weight % of talc and 1 up to 6 weight % of hydrochloric acid and the resulting substance is heated at constant stirring in 0.5 up to 6 hours to the temperature 40 °C up to 60 °C and it…

SK 278,312 B6#54517233 Most Cited · 1 citations0.0/yr · PR 0.81ExpiredSK · Utility
Method of talc treatment

Talc treatment is based on the principle, that water (74 up to 89 weight percent), talc (10 up to 20 weight percent) and hydrochloric acid with the density of 1,18 g.cm-3 (1 up to 6 weight percent) is mixed together. A created substance shall be mixed continuously and heated…

US 2010034720 A1#49586537 Most Cited · 1 citations0.1/yr · PR 0.88PendingUS · Application
Method of preparation of talcum product with high purity degree

The method which is the subject of protection is characteristic by the fact that firstly is made the suspension consisting of 10 to 20 mass % of mineral talc and 80 to 90 mass % of water; resulting suspension is homogenized and thereafter is heated to the temperature 50° to 70°…

CH 698,774 B1#77569038 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCH · Utility
A process for the manufacture of a talc product having a high degree of purity.

Das Verfahren, das der Gegenstand des Schutzes ist, ist durch die Tatsache gekennzeichnet, dass zunächst die Suspension hergestellt wird, die aus 10 bis 20 Massen-% Mineraltalk und 80 bis 90 Massen-% Wasser besteht; die resultierende Suspension homogenisiert und danach auf die…

CZ 281,195 A3#128627043 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCZ · Utility
Process of treating talc

The way of talc treatment consists in the mixing-up 74 up to 89 weight % of water, 10 up to 20 weight % of talc and 1 up to 6 weight % of hydrochloric acid and the resulting substance is heated at constant stirring in 0.5 up to 6 hours to the temperature 40 DEG C up to 60 DEG C…

CZ 284,979 B6#80477025 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCZ · Utility
Process of treating talc

Způsob spočívá v tom, že se smíchá 74 až 89 hmotnostních % vody, 10 až 20 hmotnostních % mastku a 1 až 6 hmotnostních % kyseliny chlorovodíkové a vzniklý roztok se za neustálého míchání zahřeje za 0,5 až 6 hodin na teplotu 40 .sup.o.n. C až 60.sup.o.n. C a udržuje se na této…

EP 2,137,109 A1#118954648 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Method of preparation of talcum product with high purity degree

The method which is the subject of protection is characteristic by the fact that firstly is made the suspension consisting of 10 to 20 mass % of mineral talc and 80 to 90 mass % of water; resulting suspension is homogenized and thereafter is heated to the temperature 50° to 70°…

WO 2008/105747 A1#150538902 Most Cited · 0 citations0.0/yr · PR 0.56PendingWO · Application
Method of preparation of talcum product with high purity degree

The method which is the subject of protection is characteristic by the fact that firstly is made the suspension consisting of 10 to 20 mass % of mineral talc and 80 to 90 mass % of water; resulting suspension is homogenized and thereafter is heated to the temperature 50° to 70°…