Patents
Inventor / Author Profile

Keown Eugene

37Total Forward Citations
24Indexed Patents
3Patent H-Index
EP 2,638,992 A1#4563110 Most Cited · 19 citations1.5/yr · PR 3.15PendingEP · Application
Method of surface hardening

The present invention relates to a method of surface hardening a plurality of sintered bodies comprising a hard phase and a binder phase. The method comprises the steps of placing the bodies in a container, and thereby forming a system comprising the container and the bodies…

US 2015098855 A1#18393959 Most Cited · 6 citations0.6/yr · PR 1.44PendingUS · Application
Method of surface hardening sintered bodies by using vibrations

The present invention relates to a method of surface hardening a plurality of sintered bodies having a hard phase and a binder phase. The method includes the steps of placing the bodies in a container, and forming a system including the container and the bodies therein, and…

WO 2013/135555 A1#22087437 Most Cited · 5 citations0.4/yr · PR 1.26PendingWO · Application
Method of surface hardening sintered bodies by using vibrations

The present invention relates to a method of surface hardening a plurality of sintered bodies comprising a hard phase such as WC and a binder phase such as cobalt or nickel. The method comprises the steps of placing the bodies in a container, and thereby forming a system…

CN 104,203,458 A#33346421 Most Cited · 3 citations0.2/yr · PR 1.04ActiveCN · Utility
Method for surface hardening sintered body by using vibration

The present invention relates to a method of case hardening a plurality of sintered bodies comprising a hard phase such as WC and a binder phase such as cobalt or nickel. The method comprises the following steps: placing the blanks in a container, thereby forming a system…

EP 2,825,338 A1#39668162 Most Cited · 2 citations0.2/yr · PR 1.02PendingEP · Application
Method of surface hardening sintered bodies by using vibrations

The present invention relates to a method of surface hardening a plurality of sintered bodies comprising a hard phase such as WC and a binder phase such as cobalt or nickel. The method comprises the steps of placing the bodies in a container, and thereby forming a system…

US 2018002783 A1#54685495 Most Cited · 1 citations0.1/yr · PR 0.81PendingUS · Application
Light weight cemented carbide for flow erosion components

A cemented carbide for a flow component for controlling the pressure and flow of well products includes in wt %: about 7 to about 9 Co; about 5 to about 7 Ni; about 19 to about 24 Ti C; about 1.5 to about 2.5 Cr 3 C 2 ; about 0.1 to about 0.3 Mo and balance of WC. A cemented…

WO 2016/107843 A1#57330192 Most Cited · 1 citations0.1/yr · PR 0.79PendingWO · Application
Light weight cemented carbide for flow erosion components

A cemented carbide for a flow component for controlling the pressure and flow of well products includes in wt%: about 7 to about 9 Co; about 5 to about 7 Ni; about 19 to about 24 Ti C; about 1.5 to about 2.5 Cr 3 C 2 ; about 0.1 to about 0.3 Mo and balance of WC. A cemented…

AU 2013231455 A1#82000709 Most Cited · 0 citations0.0/yr · PR 0.56PendingAU · Application
Method of surface hardening sintered bodies by using vibrations

The present invention relates to a method of surface hardening a plurality of sintered bodies comprising a hard phase such as WC and a binder phase such as cobalt or nickel. The method comprises the steps of placing the bodies in a container, and thereby forming a system…

AU 2013231455 B2#139861067 Most Cited · 0 citations0.0/yr · PR 0.56ActiveAU · Utility
Method of surface hardening sintered bodies by using vibrations
Inventors: Carpenter Michael, Geoghegan Sarah, Keown Eugene, Smith JaneAssignee: Hyperion Materials & Tech Sweden AbFiled 2013-03-07 · Granted 2017-01-05

The present invention relates to a method of surface hardening a plurality of sintered bodies comprising a hard phase such as WC and a binder phase such as cobalt or nickel. The method comprises the steps of placing the bodies in a container, and thereby forming a system…

AU 2015373452 A1#68777164 Most Cited · 0 citations0.0/yr · PR 0.56PendingAU · Application
Light weight cemented carbide for flow erosion components

A cemented carbide for a flow component for controlling the pressure and flow of well products includes in wt%: about 7 to about 9 Co; about 5 to about 7 Ni; about 19 to about 24 Ti C; about 1.5 to about 2.5 Cr

CA 2,864,636 A1#147841886 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Method of surface hardening sintered bodies by using vibrations

The present invention relates to a method of surface hardening a plurality of sintered bodies comprising a hard phase such as WC and a binder phase such as cobalt or nickel. The method comprises the steps of placing the bodies in a container, and thereby forming a system…

CA 2,864,636 C#90135602 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCA · Utility
Method of surface hardening sintered bodies by using vibrations
Inventors: Carpenter Michael, Geoghegan Sarah, Keown Eugene, Smith JaneAssignee: Sandvik Intellectual PropertyFiled 2013-03-07 · Granted 2020-03-24

The present invention relates to a method of surface hardening a plurality of sintered bodies comprising a hard phase such as WC and a binder phase such as cobalt or nickel. The method comprises the steps of placing the bodies in a container, and thereby forming a system…

CA 2,970,584 A1#154568382 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Light weight cemented carbide for flow erosion components

A cemented carbide for a flow component for controlling the pressure and flow of well products includes in wt%: about 7 to about 9 Co; about 5 to about 7 Ni; about 19 to about 24 Ti C; about 1.5 to about 2.5 Cr3C2; about 0.1 to about 0.3 Mo and balance of WC. A cemented carbide…

EP 3,240,916 A1#147407001 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Light weight cemented carbide for flow erosion components

A cemented carbide for a flow component for controlling the pressure and flow of well products includes in wt%: about 7 to about 9 Co; about 5 to about 7 Ni; about 19 to about 24 Ti C; about 1.5 to about 2.5 Cr 3 C 2 ; about 0.1 to about 0.3 Mo and balance of WC. A cemented…

ES 2,759,537 T3#136081977 Most Cited · 0 citations0.0/yr · PR 0.56ActiveES · Utility
Procedimiento de endurecimiento de superficies
Inventors: Carpenter Michael, Keown Eugene, Smith Jane, Geoghegan SarahAssignee: Hyperion Materials & Tech Sweden AbFiled 2012-03-13 · Granted 2020-05-11

Procedimiento de endurecimiento de superficies de una pluralidad de cuerpos sinterizados que comprenden una fase dura y una fase de aglutinante, en el que dicho procedimiento comprende las etapas de: colocar los cuerpos en un recipiente formando, de este modo, un sistema que…

ES 2,759,730 T3#72919666 Most Cited · 0 citations0.0/yr · PR 0.56ActiveES · Utility
Carburo cementado de peso ligero para componentes con erosión por flujo

Un carburo cementado para componentes de manipulación de fluidos y anillos de sellado, teniendo el carburo cementado una composición que comprende: 15 a 30% en peso de TiC; 5 a 20% en peso de Ni; 0,5 a 2,5% en peso Cr3C2; 0,7 a 1,6% en peso de Mo; y el resto WC.

MY 179,165 A#117617669 Most Cited · 0 citations0.0/yr · PR 0.56ActiveMY · Utility
Light weight cemented carbide for flow erosion components

A cemented carbide for a flow component for controlling the pressure and flow of well products includes in wt%: about 7 to about 9 Co; about 5 to about 7 Ni; about 19 to about 24 TiC; about 1.5 to about 2.5 Cr3C2; about 0.1 to about 0.3 Mo and balance of WC. A cemented carbide…

RU 2,675,432 C1#84944545 Most Cited · 0 citations0.0/yr · PR 0.56ActiveRU · Utility
Facilitated cemented carbide for contact with components flow
Inventors: Carpenter Michael, Mech Milena, Smith Jane, Keown Eugene, Dorvlo SelassieAssignee: Sandvik Intellectual PropertyFiled 2015-12-28 · Granted 2018-12-19

FIELD: construction materials. SUBSTANCE: group of inventions relates to cemented carbide for a component subjected to the pressure of a fluid. According to option 1, cemented carbide contains Co, Ni, TiC, Mo, WC and Cr 3 C 2 . According to option 2, cemented carbide contains…

US 10,226,819 B2#106016306 Most Cited · 0 citations0.0/yr · PR 0.56ActiveUS · Utility
Method of surface hardening sintered bodies by using vibrations

The present invention relates to a method of surface hardening a plurality of sintered bodies having a hard phase and a binder phase. The method includes the steps of placing the bodies in a container, and forming a system including the container and the bodies therein, and…