Inventors: Kehal NarinderAssignee: Raychem LtdFiled 1996-11-08 · Granted 2000-03-28

A hot-melt adhesive composition based on ethylene/vinyl actetate copolymer comprising not more than 35% (preferably not more than 30%, more preferably not more than 25%) by weight, based on the whole composition, of halogen-free char-forming flame-retardant additive(s) in an…

WO 9,717,410 A1#14648896 Most Cited · 7 citations0.2/yr · PR 2.14PendingWO · Application
Flame-retarded adhesive composition
Inventors: Kehal NarinderAssignee: Raychem Ltd, Kehal NarinderFiled 1996-11-08

A hot-melt adhesive composition based on ethylene/vinyl acetate copolymer comprising not more than 35 % (preferably not more than 30 %, more preferably not more than 25 %) by weight, based on the whole composition, of halogen-free char-forming flame-retardant additive(s) in an…

WO 9,840,436 A1#18200148 Most Cited · 6 citations0.2/yr · PR 1.49PendingWO · Application
Gels

Flame-retarded gels of oil-extended triblock copolymers are made with less than 40 % (pref. 35 %, 30 %) flame retardant additive while achieving at least 25 % (pref. 45 %, 65 %) reduction in burn rate under UL-94 Horizontal Burn Test. Preferred additives, e.g. char-forming and…

WO 9,214,128 A1#26629898 Most Cited · 4 citations0.1/yr · PR 1.18PendingWO · Application
Temperature sensor

A sensor for detecting a change in temperature comprises an element at least part of which expands in response to a change in temperature causing a change primarily in the surface electrical resistance of the element. In a preferred embodiment a component of the element expands…

DE 69,620,624 D1#96643088 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDE · Utility
Flammwidrige klebstoffmasse
Inventors: Kehal NarinderAssignee: Tyco Electronics Ltd UkFiled 1996-11-08 · Granted 2002-05-16

PCT No. PCT/GB96/02735 Sec. 371 Date Apr. 23, 1998 Sec. 102(e) Date Apr. 23, 1998 PCT Filed Nov. 8, 1996 PCT Pub. No. WO97/17410 PCT Pub. Date May 15, 1997A hot-melt adhesive composition based on ethylene/vinyl actetate copolymer comprising not more than 35% (preferably not more…

EP 0,859,818 A1#138357508 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Flame-retarded adhesive composition
Inventors: Kehal NarinderAssignee: Raychem LtdFiled 1996-11-08

PCT No. PCT/GB96/02735 Sec. 371 Date Apr. 23, 1998 Sec. 102(e) Date Apr. 23, 1998 PCT Filed Nov. 8, 1996 PCT Pub. No. WO97/17410 PCT Pub. Date May 15, 1997A hot-melt adhesive composition based on ethylene/vinyl actetate copolymer comprising not more than 35% (preferably not more…

EP 0,859,818 B1#142148579 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredEP · Utility
Flame-retarded adhesive composition
Inventors: Kehal NarinderAssignee: Tyco Electronics Ltd UkFiled 1996-11-08 · Granted 2002-04-10

PCT No. PCT/GB96/02735 Sec. 371 Date Apr. 23, 1998 Sec. 102(e) Date Apr. 23, 1998 PCT Filed Nov. 8, 1996 PCT Pub. No. WO97/17410 PCT Pub. Date May 15, 1997A hot-melt adhesive composition based on ethylene/vinyl actetate copolymer comprising not more than 35% (preferably not more…