A photovoltaic cell is fabricated from an active medium comprising an organic semiconductor in a gel. When a film of such material is sandwiched between transparent conducting electrodes a solar cell is obtained. The electrical output is greatly in excess of that obtained from…
Kay Robert E
A process for producing ZSM-48 comprises crystallizing an aqueous reaction mixture comprising at least one source of silica, at least one source of alumina, at least one source of hydroxyl ions, at least one source of diquaternary alkylammonium, R 2+ , ions having the formula:…
A layer of HgCdTe (15) epitaxially grown on a crystalline support (10). A single crystal CdTe substrate (5) is first epitaxially grown to a thickness of between 1 micron and 5 microns onto the support (10). Then a HgTe source (3) is spaced from the CdTe substrated (5) a distance…
Systems and processes for disinfecting fluids, such as water, use a mercury-free source of ultraviolet radiation such as a flash-lamp. The systems and processes can be used, for example, to inactivate pathogens such as bacteria, spores, and viruses, and pyrogens such as…
A process for producing ZSM-48 comprises crystallizing an aqueous reaction mixture comprising at least one source of silica, at least one source of alumina, at least one source of hydroxyl ions, at least one source of diquaternary alkylammonium, R 2+ , ions having the formula:…
A layer of HgCdTe (15) is epitaxially grown onto a CdTe substrate (5). A HgTe source (3) is spaced from the CdTe substrate (5) a distance of between 0.1 mm and 10 mm. The substrate (5) and source (3) are heated within a temperature range of between 500° C. and 625° C. for a…
A process for producing ZSM-48 comprises crystallizing an aqueous reaction mixture comprising at least one source of silica, at least one source of alumina, at least one source of hydroxyl ions, at least one source of diquaternary alkylammonium, R2+, ions having the formula:…
This invention relates to hydrocracking catalysts utilizing stabilized aggregates of small primary crystallites of zeolite Y that are clustered into larger secondary particles. At least 80% of the secondary particles may comprise at least 5 primary crystallites. The size of the…
This invention relates to stabilized aggregates of small primary crystallites of zeolite Y that are clustered into larger secondary particles. At least 80% of the secondary particles may comprise at least 5 primary crystallites. The size of the primary crystallites may be at…
This invention relates to hydrocracking catalysts utilizing stabilized aggregates of small primary crystallites of zeolite Y that are clustered into larger secondary particles. At least 80% of the secondary particles may comprise at least 5 primary crystallites. The size of the…
The invention provides the method for a kind of ZSM-48 of manufacturing, described method comprises making and comprises at least a silica source, at least a alumina source, at least a hydroxyl ion source, at least a alkyl two quaternary ammonium sources, R 2+ , have a formula…
A process is described for synthesizing a porous, crystalline material having the framework structure of ZSM- 12 of the formula: (n)YO2: X2O3 wherein X is a trivalent element, Y is a tetravalent element and n is between about 80 and about 250. In the process, a mixture capable…
Methods for growing HgCdTe (15) upon a CdTe substrate (5) using a HgTe source (3) and close-spaced vapor phase epitaxy (CSVPE). A processing temperature T of between 520° C. and 625° C. is employed over a processing time t of between approximately 1/4 and 4 hours. The thickness…
A layer of HgCdTe (15) epitaxially grown onto a crystalline support (10), e.g., of sapphire of GaAs. A CdTe substrate (5) is epitaxially grown to a thickness of between 1 micron and 5 microns on the support (10). A HgTe source (3) is spaced from the CdTe substrate (5) a distance…
Method for growing HgCdTe (15) upon a CdTe substrate (5) using a HgTe source (3) and close-spaced vapor phase epitaxy (CSVPE). A processing temperature T of between 520° C. and 625° C. is employed over a processing time t of between approximately 1/4 and 4 hours. The thickness A…
A supported catalyst comprises a zeolite having a silica to alumina molar ratio of 500 or less, a first metal oxide binder having a crystallite size greater than 200 Å and a second metal oxide binder having a crystallite size less than 100 Å, wherein the second metal oxide…
A layer of HgCdTe (15) is epitaxially grown on a crystalline support (10). A single crystal CdTe substrate (5) is first epitaxially grown to a thickness of between 1 micron and 5 microns onto the support (10). Then a HgTe source (3) is spaced from the CdTe substrate (5) a…
In a process for producing a molecular sieve material, water, at least one source of an oxide of a tetravalent and/or a trivalent element and at least one structure directing agent is mixed in a reactor equipped with a mixer having a Froude number of at least 1, to produce a…