A method for welding a first powder metallurgical (PM) part to a second powder metallurgical (PM) part includes: working a first face of the first PM part; working a first face of the second PM part; and friction welding the first face of the first part to the first face of the…
Kaplan Max A
A joining method includes performing a first heat treatment step on a first superalloy workpiece and a second superalloy workpiece wherein at least one of the first and second superalloy workpieces include a gamma matrix phase and a gamma-prime precipitate phase. The first and…
A method for welding a first powder metallurgical (PM) part to a second powder metallurgical (PM) part includes: working a first face of the first PM part; working a first face of the second PM part; and friction welding the first face of the first part to the first face of the…
A joining method includes performing a first heat treatment step on a first superalloy workpiece and a second superalloy workpiece wherein at least one of the first and second superalloy workpieces include a gamma matrix phase and a gamma-prime precipitate phase. The first and…
A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second…
An embodiment of a superalloy composition includes 1.5 to 4.5 wt% Al; 0.005 to 0.06 wt% B; 0.02 to 0.07 wt% C; 21.0 to 26.0 wt% Co; 11.5 to 16.0 wt% Cr; 8.50 to 19.0 wt% Ta; 0.005-0.10 wt% Zr; and balance Ni and incidental impurities.
An embodiment of a superalloy composition includes 0 to 3.5 wt% Al; 0.005 to 0.05 wt% B; 0.005 to 0.25 wt% C; 10 to 27 wt% Co; 12 to 20 wt% Cr; 6 to 10 wt% Ti; 0.01 to 0.1 wt% Zr; and balance Ni and incidental impurities.
A method for welding a first powder metallurgical (PM) part to a second powder metallurgical (PM) part includes: working a first face of the first PM part; working a first face of the second PM part; and friction welding the first face of the first part to the first face of the…
A method for welding a first powder metallurgical (PM) part to a second powder metallurgical (PM) part includes: working a first face of the first PM part; working a first face of the second PM part; and friction welding the first face of the first part to the first face of the…
A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second…
An embodiment of a superalloy composition includes 1.5 to 4.5 wt % Al; 0.005 to 0.06 wt % B; 0.02 to 0.07 wt % C; 21.0 to 26.0 wt % Co; 11.5 to 16.0 wt % Cr; 8.50 to 19.0 wt % Ta; 0.005-0.10 wt % Zr; and balance Ni and incidental impurities.
A joining method includes performing a first heat treatment step on a first superalloy workpiece and a second superalloy workpiece wherein at least one of the first and second superalloy workpieces include a gamma matrix phase and a gamma-prime precipitate phase. The first and…
A joining method includes performing a first heat treatment step on a first superalloy workpiece and a second superalloy workpiece wherein at least one of the first and second superalloy workpieces include a gamma matrix phase and a gamma-prime precipitate phase. The first and…
A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second…
An embodiment of a superalloy composition includes 1.5 to 4.5 wt % Al; 0.005 to 0.06 wt % B; 0.02 to 0.07 wt % C; 21.0 to 26.0 wt % Co; 11.5 to 16.0 wt % Cr; 8.50 to 19.0 wt % Ta; 0.005-0.10 wt % Zr; and balance Ni and incidental impurities.
A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second…
An embodiment of a superalloy composition includes 0 to 3.5 wt % Al; 0.005 to 0.05 wt % B; 0.005 to 0.25 wt % C; 10 to 27 wt % Co; 12 to 20 wt % Cr; 6 to 10 wt % Ti; 0.01 to 0.1 wt % Zr; and balance Ni and incidental impurities.
A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second…
A joining method includes performing a first heat treatment step on a first superalloy workpiece and a second superalloy workpiece wherein at least one of the first and second superalloy workpieces include a gamma matrix phase and a gamma-prime precipitate phase. The first and…
A method for heat treating a superalloy component includes heating a superalloy component to a first temperature, cooling the superalloy from the first temperature to a second temperature at a first cooling rate in a furnace, and cooling the superalloy component from the second…