The invention relates to a method for producing low-molecular, highly reactive polyisobutylene having an average molecular weight Mn ranging from 500 to 5000 dalton and having a content of terminal double bonds of over 80 mol %. To this end, isobutane or hydrocarbon streams…
Kanne U
The invention relates to a method for producing highly reactive polyisobutenes consisting of a polymer isobutene in the presence of a complex boron trifluoride and at least one cocatalyst at a reaction temperature of 60 to -4 DEG C in a liquid organic phase which is mixed with…
The invention relates to a process, which uses boron trifluoride coordination catalyst at-40-20 ℃ and 1 x 10 5 -2×10 6 The average molecular weight M is prepared from isobutene or isobutene-containing hydrocarbon materials by polymerization in liquid phase under the pressure of…
A process for the production of highly reactive polyisobutenes is disclosed, in which isobutene is polymerized in a liquid organic phase at from-60 to-4 ℃ in the presence of a complex of boron trifluoride and at least one cocatalyst, and water is added to the organic phase in…