According to this method for producing an electrode, a fibrous binder is produced by fibrillating a particulate binder, which has a volume-based median diameter of from 5 to 100 μm, by means of the application of a shear force, and an electrode mixture is produced by mixing the…
Jin takuya
This electrode for secondary batteries is provided with a core material and an electrode mixture sheet that is bonded to the surface of the core material. The electrode mixture sheet contains an active material, a fibrous first binder and a particulate second binder; and the…
This secondary battery electrode is provided with a core material configured from a metal foil that softens at less than or equal to 200°C, and an electrode mixture sheet which is bonded on the surface of the core material. The electrode mixture sheet includes an active material…
Provided is a PTFE powder that is in a dry state, wherein the percentage of fibrous particles which have an aspect ratio of 1.5 or higher with respect to all particles is 20-60%, and the average major axis size of the fibrous particles is 1-20 μm. A PTFE powder according to…
This lithium-containing complex oxide production method comprises: a first step for preparing lithium hydroxide; a second step for heating, to 300-800°C, a hydroxide including nickel and a metal M1 other than lithium and nickel to obtain a complex oxide including nickel and…
This electrode is obtained by superposing an electrode mixture material on the surface of a core material, said electrode mixture material containing a coated active material, wherein a conductive material adheres to the surface of an active material, and a PTFE powder. With…
The electrode is an electrode in which an electrode composite material is laminated on the surface of a core material, the electrode composite material including: the coating active material having a conductive material attached to the surface of the active material, and the…
This electrode for secondary batteries is provided with a core material and an electrode mixture sheet that is bonded to the surface of the core material. The electrode mixture sheet contains an active material, a fibrous first binder and a particulate second binder; and the…
Provided is a PTFE powder that is in a dry state, wherein the percentage of fibrous particles which have an aspect ratio of 1.5 or higher with respect to all particles is 20-60 %, and the average major axis size of the fibrous particles is 1-20 µm. A PTFE powder according to…
To enable an opening/closing sliding force of a sliding door to be adjusted to a user's preference.SOLUTION: A door side hinge 12 attached to a slide door and a rail side hinge 14 attached to a slide rail of a vehicle body are pivotally supported by a hinge pin 16. A…
A method for producing a lithium-containing composite oxide, the method including: a first step of preparing a lithium hydroxide; a second step of heating a hydroxide containing nickel and a metal M1 other than lithium and nickel to 300° C. or higher and 800° C. or lower, to…
According to this method for producing an electrode, a fibrous binder is produced by fibrillating a particulate binder, which has a volume-based median diameter of from 5 to 100 µm, by means of the application of a shear force, and an electrode mixture is produced by mixing the…
This electrode for secondary batteries is provided with a core material and an electrode mixture sheet that is bonded to the surface of the core material. The electrode mixture sheet contains an active material, a fibrous first binder and a particulate second binder; and the…
A negative electrode active material for a non-aqueous electrolyte secondary battery according to one example of an embodiment comprises composite particles (30) that include a lithium aluminate phase (31) and a silicon phase (32) dispersed in the lithium aluminate phase (31).…
The PTFE powder is in a dry state, the ratio of the fibrous particles having an aspect ratio of 1.5 or more to the total particles is 20 to 60%, and the average major axis dimension of the fibrous particles is 1 to 20 [ mu ] m. In another embodiment of the present invention, the…
According to this method for producing an electrode, a fibrous binder is produced by fibrillating a particulate binder, which has a volume-based median diameter of from 5 to 100 µm, by means of the application of a shear force, and an electrode mixture is produced by mixing the…
This electrode is obtained by superposing an electrode mixture material on the surface of a core material, said electrode mixture material containing a coated active material, wherein a conductive material adheres to the surface of an active material, and a PTFE powder. With…
With respect to this electrode, the coverage of the surface of a coated active material by a conductive material is from 10% to 60%; the mixture resistance of a electrode mixture material is 20 Ωcm or less in cases where the electrode mixture material is divided into three equal…
Provided is a PTFE powder that is in a dry state, wherein the percentage of fibrous particles which have an aspect ratio of 1.5 or higher with respect to all particles is 20-60%, and the average major axis size of the fibrous particles is 1-20 μm. A PTFE powder according to…
A negative electrode active material for a non-aqueous electrolyte secondary battery according to one example of an embodiment comprises composite particles ( 30 ) that include a lithium aluminate phase ( 31 ) and a silicon phase ( 32 ) dispersed in the lithium aluminate phase (…
A negative electrode active material for nonaqueous electrolyte secondary batteries according to the present invention is characterized by containing composite particles that contain SiC and at least one of Si and an Si alloy, and is also characterized in that the composite…
The method for producing a lithium-containing composite oxide comprises the following steps: a first step of preparing lithium hydroxide; a second step of heating a hydroxide containing nickel and containing a metal M1 other than lithium and nickel to 300 ℃ or higher and 800 ℃…
The method for producing a lithium nickel composite oxide includes the steps of: a molded body comprising a mixture of a lithium-containing compound and a nickel-containing compound is fired in a container to obtain a fired body. The space ratio occupied by the clearance of the…
The method for producing a lithium transition metal composite oxide includes: preparing a1 st mixture containing a lithium-containing compound and a transition metal compound; a step of compressing the first mixture 1 at least 1 time to obtain a compressed body; a step of…
The method for producing a lithium transition metal composite oxide comprises the steps of: preparing a mixture containing a lithium-containing compound and a transition metal compound; a step of obtaining a molded product of the mixture; and a step of firing the molded body in…