Aluminum plating according to which aluminum film formed has no cracks and pin-holes on its surface, a uniform thickness, excellent luster and is strongly bonded to the substrate can be attained by heat treating a substrate covered with aluminum at 400* C the melting point of…
Ichiki E
AN ALKYLALUMINUM COMPOUND IS PRODUCED CONTINOUSLY AND ECONOMICALLY WITH LESS ALUMINUM LOSS BY REACTING HYDROGEN AND AN ALKYLALUMINUM COMPOUND OR FURTHER AN OLEFIN IN ADDITION THERETO, WITH AN ALLOY CONTAINING ALUMINUM AND SILICON AND HAVING A SIZE LARGER THAN THAT OF A METAL…
A TRIALKOXYLAUMINUM IS PRODUCED FROM AN ALKYLALUMINUM COMPOUND, R1-AL(-R2)-R3 WHEREIN R1 AND R2 REPRESENT ALKYL GROUP HAVING 2 TO 30 CARBON ATOMS, AND R3 AN ALKYL OR ALKOXY GROUPS HAVING 2 TO 30 CARBON ATOMS THROUGH OXIDATION BY CONTACTING THE ALKYLALUMINUM COMPOUND WITH A…
WHEREIN R1 REPRESENTS AN ALKYL GROPU HAVING 2-30 CARBON ATOMS AND R2 AND R3 REPRESENT ALKYL GROUPS OR ALKOXY GROUPS HAVING 2-30 CARBON ATOMS THROUGH OXIDATION BY INTRODUCING THE ALKYLALUMINUM COMPOUND DILUTED WITH AT LEAST 600 G. OF A SOLVENT HAVING A BOILING POINT OF -50*150*C.…
ALUMINUM OR ITS ALLOY IS ACTIVATED BY HEATING ALUMINUM OR ITS ALLOY AT 70 -200*C. IN THE PRESENCE OF AN ACTIVATING AGENT COMPRISING (1) A COMPOUND REPRESENTED BY THE GENERAL FORMULA R2AIX, WHEREIN R REPRESENTS AN ALKYL, ARYL, ARALKYL OR ALKARYL GROUP AND X REPRESENTS A HYDROGEN…