Surfaces of unrecrystallized alloys are sanded and polished. This is followed by a two-step welding process wherein the strength of the parent metal is retained at the weld joint. The first step forces the surfaces into intimate contact at a temperature where the metal still has…
Holko K
Using magnetic force upset welding to form T-joints between dissimilar thickness parts. This type of resistance welding is used to join compressor and turbine parts thereby reducing the weight and cost of a jet engine.
Solid state welding a butt joint by fusion welding the peripheral surfaces to form a seal, autogenetically cleaning the faying or mating surfaces of the joint by heating the abutting surfaces to 1,200*C., and heating to the diffusion welding temperature in air.
Dispersion-strengthened nickel alloys are sanded on one side and chemically polished. This is followed by a single-step welding process wherein the polished surfaces are forced into intimate contact at 1,400* F for one hour in a vacuum. Diffusion, recrystallization, and grain…
USING MAGNETIC FORCE UPSET WELDING TO FORM T-JOINTS BETWEEN DISSIMILAR THICKNESS PARTS. THIS TYPE OF RESISTANCE WELDING IS USED TO JOIN COMPRESSOR AND TURBINE PARTS THEREBY REDUCING THE WEIGHT AND COST OF A JET ENGINE.