US 2017158789 A1#2873151 Most Cited · 26 citations2.9/yr · PR 3.60PendingUS · Application
High density rotomolding resin

The present disclosure provides high density polyethylene resins having good low temperature impact resistance. The resins are suitable for use in rotomolding application for large parts. The resin is a bi- or trimodal resin produced using solution phase polymerization in the…

US 2013310532 A1#6362214 Most Cited · 15 citations1.1/yr · PR 2.51PendingUS · Application
Rotomolding Resin

Resins suitable for rotomolded articles comprise a bimodal polyethylene copolymer comprising from 0.1 to 5 weight % of one or more C 6-8 alpha olefins and the balance ethylene, comprising from 20 to 50 weight % of a higher molecular weight polymer component having an Mw greater…

US 8,907,018 B2#11721397 Most Cited · 9 citations0.8/yr · PR 2.01ActiveUS · Utility
Rotomolding resin
Inventors: Bellehumeur Celine, Lacombe Yves, Hoidas MarkAssignee: Bellehumeur Celine, Lacombe YvesFiled 2013-05-09 · Granted 2014-12-09

Resins suitable for rotomolded articles comprise a bimodal polyethylene copolymer comprising from 0.1 to 5 weight % of one or more C 6-8 alpha olefins and the balance ethylene, comprising from 20 to 50 weight % of a higher molecular weight polymer component having an Mw greater…

CN 105,705,572 A#12673751 Most Cited · 8 citations0.8/yr · PR 2.56ActiveCN · Utility
Enhanced ESCR bimodal rotomolding resins

The present invention provides a resin suitable for rotational moulding having an environmental stress crack resistance of more than 1000 hours. The resin has a density of 0.937 to 0.942g/cm 3 According to ASTM D1238 (2.16kg 190 ℃ -I) 2 ) Measured melt index I 2 From 4.0 to…

US 9,181,422 B2#22127921 Most Cited · 5 citations0.5/yr · PR 1.25ActiveUS · Utility
Enhanced ESCR bimodal rotomolding resin
Inventors: Bellehumeur Marie Therese Celine, Hoidas MarkAssignee: Nova Chem Int SaFiled 2014-11-07 · Granted 2015-11-10

The present disclosure provides a resin suitable for use in rotational molding having an environmental stress crack resistance of greater than 1000 hours. The resin has a density from 0.937 to 0.942 g/cm 3 , a melt index I 2 determined according to ASTM D 1238 (2.16 kg/190° C.−I…

WO 2017/098359 A1#21819223 Most Cited · 5 citations0.6/yr · PR 1.32PendingWO · Application
High density rotomolding resin

The present invention provides high density polyethylene resins having good low temperature impact resistance. The resins are suitable for use in rotomolding application for large parts. The resin is a bi- or trimodal resin produced using solution phase polymerization in the…

CA 2,777,386 A1#23545245 Most Cited · 4 citations0.3/yr · PR 1.64PendingCA · Application
Rotomolding resin
Inventors: Bellehumeur Celine, Lacombe Yves, Hoidas MarkAssignee: Nova Chemicals CorpFiled 2012-05-17

Resins suitable for rotomolded articles comprise a bimodal polyethylene copolymer comprising from 0.1 to 5 weight % of one or more C6-8 alpha olefins and the balance ethylene, comprising from 20 to 50 weight % of a higher molecular weight polymer component having an Mw greater…

US 2015141579 A1#26693329 Most Cited · 4 citations0.4/yr · PR 1.17PendingUS · Application
Enhanced escr bimodal rotomolding resin

The present disclosure provides a resin suitable for use in rotational molding having an environmental stress crack resistance of greater than 1000 hours. The resin has a density from 0.937 to 0.942 g/cm 3 , a melt index I 2 determined according to ASTM D 1238 (2.16 kg/190° C.−I…

WO 2015/071807 A1#27253995 Most Cited · 4 citations0.4/yr · PR 1.06PendingWO · Application
Enhanced escr bimodal rotomolding resin
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chem Int SaFiled 2014-11-06

The present invention provides a resin suitable for use in rotational molding having an environmental stress crack resistance of greater than 1000 hours. The resin has a density from 0.937 to 0.942 g/cm³, a melt index I2 determined according to ASTM D 1238 (2.16 kg 190°C – I2)…

CN 108,290,980 A#34068235 Most Cited · 3 citations0.4/yr · PR 0.95ActiveCN · Utility
High density rotational moulding resin
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chem Int SaFiled 2016-11-15

The present invention provides the high-density polyethylene resin with good low-temperature impact resistance.The resin is suitable for the rotational moulding application of large component.The resin be in the presence of single site catalysts using solution phase symphysis at…

KR 20160088876 A#31531171 Most Cited · 3 citations0.3/yr · PR 1.15ActiveKR · Utility
Enhanced escr bimodal rotomolding resin
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chem Int SaFiled 2014-11-06

본 발명은 내환경응력균열성이 1000시간 초과인 회전성형에 사용하기에 적합한 수지를 제공한다. 이 수지는 밀도가 0.937 내지 0.942 g/㎤이고, ASTM D1238(2.16kg 190℃ - I 2 )에 따라 측정된 용융지수 I 2 가 4.0 내지 7.0g/10min이며, ASTM D1238(21.6kg 190℃-I 21 )에 따라 측정된 I 21 은 160 내지 200g/10min이며, I 21 /I 2 는 30 내지 40이고, 말단 비닐 불포화도가 1000개 탄소원자당 0.06…

US 9,540,505 B2#34083527 Most Cited · 3 citations0.3/yr · PR 0.95ActiveUS · Utility
Enhanced ESCR bimodal rotomolding resin
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chemicals International SaFiled 2015-09-17 · Granted 2017-01-10

The present disclosure provides a resin suitable for use in rotational molding having an environmental stress crack resistance of greater than 1000 hours. The resin has a density from 0.937 to 0.942 g/cm 3 , a melt index I 2 determined according to ASTM D 1238 (2.16 kg/190° C.—I…

US 9,321,865 B2#45337314 Most Cited · 2 citations0.2/yr · PR 0.86ActiveUS · Utility
Rotomolding resin
Inventors: Bellehumeur Celine, Lacombe Yves, Hoidas MarkAssignee: Nova Chem Int SaFiled 2015-09-04 · Granted 2016-04-26

Resins suitable for rotomolded articles comprise a bimodal polyethylene copolymer comprising from 0.1 to 5 weight % of one or more C 6-8 alpha olefins and the balance ethylene, comprising from 20 to 50 weight % of a higher molecular weight polymer component having an Mw greater…

KR 20180090800 A#51486798 Most Cited · 1 citations0.1/yr · PR 0.85ActiveKR · Utility
고밀도 회전성형 수지
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chem Int SaFiled 2016-11-15

본 발명은 양호한 저온 충격저항성을 가진 고밀도 폴리에틸렌 수지를 제공한다. 이 수지는 큰 부품들의 회전성형 용도에 사용하기에 적합하다. 이 수지는 단일 부위 촉매의 존재하에 용액상 중합을 사용하여 생산한 이봉성(bimodal) 또는 삼봉성(trimodal) 수지이다.

US 2015065657 A1#58570949 Most Cited · 1 citations0.1/yr · PR 0.78PendingUS · Application
Rotomolding resin
Inventors: Bellehumeur Celine, Lacombe Yves, Hoidas MarkAssignee: Nova Chem Int SaFiled 2014-11-07

Resins suitable for rotomolded articles comprise a bimodal polyethylene copolymer comprising from 0.1 to 5 weight % of one or more C 6-8 alpha olefins and the balance ethylene, comprising from 20 to 50 weight % of a higher molecular weight polymer component having an Mw greater…

US 2015376313 A1#57911330 Most Cited · 1 citations0.1/yr · PR 0.79PendingUS · Application
Rotomolding resin
Inventors: Bellehumeur Celine, Lacombe Yves, Hoidas MarkAssignee: Nova Chem Int SaFiled 2015-09-04

Resins suitable for rotomolded articles comprise a bimodal polyethylene copolymer comprising from 0.1 to 5 weight % of one or more C 6-8 alpha olefins and the balance ethylene, comprising from 20 to 50 weight % of a higher molecular weight polymer component having an Mw greater…

US 2016002448 A1#61026404 Most Cited · 1 citations0.1/yr · PR 0.75PendingUS · Application
Enhanced escr bimodal rotomolding resin
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chem Int SaFiled 2015-09-17

The present disclosure provides a resin suitable for use in rotational molding having an environmental stress crack resistance of greater than 1000 hours. The resin has a density from 0.937 to 0.942 g/cm 3 , a melt index I 2 determined according to ASTM D 1238 (2.16 kg/190° C.—I…

AU 2016366721 A1#137101254 Most Cited · 0 citations0.0/yr · PR 0.56PendingAU · Application
High density rotomolding resin
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chem Int SaFiled 2016-11-15

The present invention provides high density polyethylene resins having good low temperature impact resistance. The resins are suitable for use in rotomolding application for large parts. The resin is a bi- or trimodal resin produced using solution phase polymerization in the…

BR 112016011268 B1#140210341 Most Cited · 0 citations0.0/yr · PR 0.56ActiveBR · Utility
Composição de polietileno bimodal, processo para produzir uma composição de polietileno bimodal e parte rotomoldada
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chem Int SaFiled 2014-11-06

resina de rotomoldagem bimodal com escr aprimorada. a presente invenção proporciona uma resina adequada para o uso em moldagem rotacional tendo uma resistência a quebras sob tensão ambiental superior a 1000 horas. a resina possui uma densidade de 0,937 a 0,942 g/cm³, um índice…

BR 112018011675 B1#147581114 Most Cited · 0 citations0.0/yr · PR 0.56ActiveBR · Utility
Resinas de polietileno de densidade alta tendo boa resistência a impacto em baixa temperatura
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chem Int SaFiled 2016-11-15

RESINA DE ROTOMOLDAGEM DE ALTA DENSIDADE A presente invenção fornece resinas de polietileno de densidade alta tendo boa resistência a impacto em baixa temperatura. As resinas são adequadas para uso em aplicação de rotomoldagem para partes grandes. A resina é uma resina bi- ou…

CA 2,777,386 C#94329863 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCA · Utility
Rotomolding resin
Inventors: Bellehumeur Celine, Lacombe Yves, Hoidas MarkAssignee: Nova Chemicals CorpFiled 2012-05-17 · Granted 2020-06-30

Resins suitable for rotomolded articles comprise a bimodal polyethylene copolymer comprising from 0.1 to 5 weight % of one or more C6-8 alpha olefins and the balance ethylene, comprising from 20 to 50 weight % of a higher molecular weight polymer component having an Mw greater…

CA 2,834,068 A1#87851710 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Enhanced escr bimodal rotomolding resin

The present invention provides a resin suitable for use in rotational molding having an environmental stress crack resistance of greater than 1000 hours. The resin has a density from 0.937 to 0.942 g/cm3, a melt index12 determined according to ASTM D 1238 (2.16 kg 190°C ¨I2)…

CA 2,834,068 C#94554723 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCA · Utility
Enhanced escr bimodal rotomolding resin
Inventors: Bellehumeur Marie Therese Celine, Hoidas MarkAssignee: Nova Chemicals CorpFiled 2013-11-18 · Granted 2020-07-28

The present invention provides a resin suitable for use in rotational molding having an environmental stress crack resistance of greater than 1000 hours. The resin has a density from 0.937 to 0.942 g/cm3, a melt index12 determined according to ASTM D 1238 (2.16 kg 190°C ¨I2)…

CA 2,914,166 A1#95273864 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
High density rotomolding resin
Inventors: Bellehumeur Celine, Hoidas MarkAssignee: Nova Chemicals CorpFiled 2015-12-08

The present invention provides high density polyethylene resins having good low temperature impact resistance. The resins are suitable for use in rotomolding application for large parts. The resin is a bi- or trimodal resin produced using solution phase polymerization in the…