Hensarling Ryan M

21Total Forward Citations
38Indexed Patents
3Patent H-Index
WO 2019/191574 A1#18533747 Most Cited · 6 citations0.9/yr · PR 1.39PendingWO · Application
Cerium-stabilized polyamides and processes for making same

A heat-stabilized polyamide composition comprising from 25 wt% to 90 wt%% of an amide polymer from 0.01 wt% to 10 wt% of a cerium-based heat stabilizer, a second heat stabilizer, a halide additive, and less than 0.3 wt% of a stearate additive. A weight ratio of halide additive…

US 2020247994 A1#22090409 Most Cited · 5 citations0.8/yr · PR 1.26PendingUS · Application
Polyamides having high levels of amine end groups

A heat-stabilized polyamide composition comprising from 25 wt % to 99 wt % of an amide polymer having an amine end group level greater than 50 μeq/gram; a first stabilizer comprising a lanthanoid-based compound; a second stabilizer; and from 0 wt % to 65 wt % filler; wherein,…

US 2019300709 A1#23364029 Most Cited · 4 citations0.6/yr · PR 1.71PendingUS · Application
Cerium-stabilized polyamides and processes for making same

A heat-stabilized polyamide composition comprising from 25 wt % to 90 wt %% of an amide polymer from 0.01 wt % to 10 wt % of a cerium-based heat stabilizer, a second heat stabilizer, a halide additive, and less than 0.3 wt % of a stearate additive. A weight ratio of halide…

US 2020247993 A1#43373474 Most Cited · 2 citations0.3/yr · PR 0.93PendingUS · Application
Impact-modified injection-molded polyamide

An impact-modified polyamide composition comprising from 5 wt % to 85 wt % of polyamide polymer; from 10 wt % to 60 wt % glass fiber; from 3 wt % to 30 wt % of an impact modifier; and a melt stabilizer at a concentration less than 5 wt %; wherein the weight ratio of the impact…

WO 2020/163571 A1#39799789 Most Cited · 2 citations0.3/yr · PR 1.02PendingWO · Application
Polyamides having high levels of amine end groups

A heat-stabilized polyamide composition comprising from 25 wt% to 99 wt% of an amide polymer having an amine end group level greater than 50 µeq/gram; a first stabilizer comprising a lanthanoid-based compound; a second stabilizer; and from 0 wt% to 65 wt% filler; wherein, when…

CN 113,396,186 A#56425814 Most Cited · 1 citations0.2/yr · PR 0.80ActiveCN · Utility
Polyamide with high amine end group content

A thermally stable polyamide composition comprising 25 to 99 wt.% of an amide polymer having an amine end group content of greater than 50 μ eq/gram; a first stabilizer comprising a lanthanide-based compound; a second stabilizer; and 0 to 65 wt% of a filler; wherein the…

US 2020255662 A1#58387162 Most Cited · 1 citations0.2/yr · PR 0.78PendingUS · Application
Hydrolysis resistant polyamides

A hydrolysis resistant polyamide composition comprising from 50 wt % to 80 wt % polyamide polymer having a theoretical amine end group content of at least 55 μeq/gram; and from 25 wt % to 60 wt % glass fibers. The weight ratio of polyamide polymer to glass fibers ranges from…

CA 3,095,329 A1#123001969 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Cerium-stabilized polyamides and processes for making same

A heat-stabilized polyamide composition comprising from 25 wt% to 90 wt%% of an amide polymer from 0.01 wt% to 10 wt% of a cerium-based heat stabilizer, a second heat stabilizer, a halide additive, and less than 0.3 wt% of a stearate additive. A weight ratio of halide additive…

CA 3,095,329 C#113539104 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCA · Utility
Cerium-stabilized polyamides and processes for making same
Inventors: Sparks Bradley J, Hensarling Ryan M, Somasiri Nanayakkara LAssignee: Ascend Performance Mat Operations LlcFiled 2019-03-29 · Granted 2024-05-21

A heat-stabilized polyamide composition comprising from 25 wt% to 90 wt%% of an amide polymer from 0.01 wt% to 10 wt% of a cerium-based heat stabilizer, a second heat stabilizer, a halide additive, and less than 0.3 wt% of a stearate additive. A weight ratio of halide additive…

CA 3,128,002 A1#79102086 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Impact-modified injection-molded polyamide

An impact-modified polyamide composition comprising from 5 wt% to 85 wt% of polyamide polymer; from 10 wt% to 60 wt% glass fiber; from 3 wt% to 30 wt% of an impact modifier; and a melt stabilizer at a concentration less than 5 wt%; wherein the weight ratio of the impact modifier…

CA 3,129,079 A1#128924114 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Polyamides having high levels of amine end groups

A heat-stabilized polyamide composition comprising from 25 wt% to 99 wt% of an amide polymer having an amine end group level greater than 50 µeq/gram; a first stabilizer comprising a lanthanoid-based compound; a second stabilizer; and from 0 wt% to 65 wt% filler; wherein, when…

CA 3,129,447 A1#145482723 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Hydrolysis resistant polyamides

A hydrolysis resistant polyamide composition comprising from 50 wt% to 80 wt% polyamide polymer having a theoretical amine end group content of at least 55 µeq/gram; and from 25 wt% to 60 wt% glass fibers. The weight ratio of polyamide polymer to glass fibers ranges from 0.5:1…

CA 3,129,447 C#137954056 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCA · Utility
Hydrolysis resistant polyamides
Inventors: Sparks Bradley J, Hensarling Ryan MAssignee: Ascend Performance Mat Operations LlcFiled 2020-02-12 · Granted 2023-10-17

A hydrolysis resistant polyamide composition comprising from 50 wt% to 80 wt% polyamide polymer having a theoretical amine end group content of at least 55 µeq/gram; and from 25 wt% to 60 wt% glass fibers. The weight ratio of polyamide polymer to glass fibers ranges from 0.5:1…

CN 111,918,912 A#148887547 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Cerium-stabilized polyamide and method for producing same

A heat stabilized polyamide composition comprising 25 to 90 weight percent amide polymer, 0.01 to 10 weight percent cerium based heat stabilizer, a second heat stabilizer, a halide additive, and less than 0.3 weight percent stearate additive. The weight ratio of halide additive…

CN 113,677,497 A#152681898 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Impact-modified injection-molded polyamides

An impact modified polyamide composition comprising 5 to 85 weight percent of a polyamide polymer; 10 to 60 weight percent glass fiber; 3 to 30 weight percent of an impact modifier; and a melt stabilizer at a concentration of less than 5 weight percent; wherein the weight ratio…

CN 113,677,754 A#152677859 Most Cited · 0 citations0.0/yr · PR 0.56ActiveCN · Utility
Hydrolysis resistant polyamides

A hydrolysis resistant polyamide composition comprising 50 to 80 wt% of a polyamide polymer having a theoretical amine end group content of at least 55 μ eq/gram; and 25 to 60 weight percent glass fiber. The weight ratio of polyamide polymer to glass fiber is 0.5:1 to 4.0: 1.…

EP 3,775,012 A1#68864757 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Cerium-stabilized polyamides and processes for making same

A heat-stabilized polyamide composition comprising from 25 wt% to 90 wt%% of an amide polymer from 0.01 wt% to 10 wt% of a cerium-based heat stabilizer, a second heat stabilizer, a halide additive, and less than 0.3 wt% of a stearate additive. A weight ratio of halide additive…

EP 3,917,748 A1#110764062 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Impact-modified injection-molded polyamide

An impact-modified polyamide composition comprising from 5 wt% to 85 wt% of polyamide polymer; from 10 wt% to 60 wt% glass fiber; from 3 wt% to 30 wt% of an impact modifier; and a melt stabilizer at a concentration less than 5 wt%; wherein the weight ratio of the impact modifier…

EP 3,921,371 A1#101551560 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Polyamides having high levels of amine end groups

A heat-stabilized polyamide composition comprising from 25 wt% to 99 wt% of an amide polymer having an amine end group level greater than 50 µeq/gram; a first stabilizer comprising a lanthanoid-based compound; a second stabilizer; and from 0 wt% to 65 wt% filler; wherein, when…

EP 3,924,415 A1#127660476 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Hydrolysis resistant polyamides

A hydrolysis resistant polyamide composition comprising from 50 wt% to 80 wt% polyamide polymer having a theoretical amine end group content of at least 55 µeq/gram; and from 25 wt% to 60 wt% glass fibers. The weight ratio of polyamide polymer to glass fibers ranges from 0.5:1…

KR 20200132956 A#142502482 Most Cited · 0 citations0.0/yr · PR 0.56ActiveKR · Utility
세륨-안정화된 폴리아미드 및 이를 제조하는 방법

본 개시는 25 중량% 내지 90 중량%의 아미드 폴리머, 0.01 중량% 내지 10 중량%의 세륨-기반 열 안정화제, 제2 열 안정화제, 할라이드 첨가제, 및 0.3 중량% 미만의 스테아레이트 첨가제를 포함하는 열-안정화된 폴리아미드 조성물에 관한 것이다. 스테아레이트 첨가제에 대한 할라이드 첨가제의 중량 비율이 45.0 미만이다.

KR 20210122822 A#147003405 Most Cited · 0 citations0.0/yr · PR 0.56ActiveKR · Utility
충격-개질된 사출 성형 폴리아미드

본 발명은 5 중량% 내지 85 중량%의 폴리아미드 중합체; 10 중량% 내지 60 중량%의 유리 섬유; 3 중량% 내지 30 중량%의 충격 개질제; 및 5 중량% 미만 농도의 용융 안정화제를 포함하는 충격-개질된 폴리아미드 조성물에 관한 것으로서, 이때 상기 충격 개질제 대 상기 용융 안정화제의 중량비는 1.0:1 내지 100:1 범위이고; 상기 폴리아미드 조성물은 80 kJ/m 2 초과인 23℃에서의 비-노치 샤르피 충격 에너지 손실 및 135 MPa 초과의 인장 강도를 나타낸다.

KR 20210124400 A#119201022 Most Cited · 0 citations0.0/yr · PR 0.56ActiveKR · Utility
높은 수준의 아민 말단기를 갖는 폴리아미드

본 발명은, 25 중량% 내지 99 중량%의, 50 μeq/g 초과의 아민 말단기 수준을 갖는 아미드 중합체; 란타노이드계 화합물을 포함하는 제1 안정화제; 제2 안정화제; 및 0 중량% 내지 65 중량%의 충전제를 포함하는 열-안정화된 폴리아미드 조성물에 관한 것으로서, 이때 190℃ 내지 220℃의 온도 범위에 걸쳐 3000시간 동안 열 에이징될 때, 상기 폴리아미드 조성물은 23℃에서 측정시 51% 초과의 인장 강도 유지율을 나타낸다.

KR 20210126672 A#70459338 Most Cited · 0 citations0.0/yr · PR 0.56ActiveKR · Utility
내가수분해성 폴리아미드

내가수분해성 폴리아미드 조성물은 55 μeq/g 이상의 이론적 아민 말단기 함량을 갖는 50 내지 80 중량%의 폴리아미드 중합체; 및 25 내지 60 중량%의 유리 섬유를 포함한다. 폴리아미드 중합체 대 유리 섬유의 중량비는 0.5:1 내지 4.0:1 범위이다. 폴리아미드 조성물은 0.06 중량% 미만의 구리; 및/또는 1 ppb 내지 0.24 중량%의 비-구리 금속 할라이드 화합물를 포함한다. 폴리아미드 조성물은, 500시간 동안 130℃에서 가수분해 에이징될 때, 23℃에서 측정시 40…