US 12,537,142 B2#3332645 Most Cited · 0 citations0.0/yr · PR 0.00ActiveUS · Utility
Fabrication of capacitors and recovery of capacitor fabrication materials
Inventors: Ralph Jason Hemphill, Henry Buser, III, Shelley M. Smith, Brian Smith, Debbie UselmanAssignee: PACESETTER, INC.Filed 2021-11-30 · Granted 2026-01-27

Fabricating a capacitor include using a first etching solution to etch a first sheet of material so as to generate a spent etchant. At least one chemical component is recovered from the spent etchant. A second etching solution is used to etch a second sheet of material. The…

US 12,537,143 B2#3332644 Most Cited · 0 citations0.0/yr · PR 0.00ActiveUS · Utility
Aluminum oxide layer on anode foil for aluminum electrolytic capacitor
Inventors: Ralph Jason Hemphill, Henry Buser, Brian Smith, Corina Geiculescu, David BowenAssignee: Pacesetter, Inc.Filed 2023-08-11 · Granted 2026-01-27

A method of producing a capacitor electrode includes forming an oxide layer on a foil. The method also includes heating the foil to a target temperature so as to induce defects in the oxide layer. The target temperature is about 450 ° C. to 560 ° C. and the duration of heating…

US 2026/0128233 A1#2586229 Most Cited · 0 citations0.0/yr · PR 0.00PendingUS · Application
FABRICATION OF CAPACITORS AND RECOVERY OF CAPACITOR FABRICATION MATERIALS

Fabricating a capacitor includes using a first etching solution to etch a first sheet of material so as to generate a spent etchant. At least one chemical component is recovered from the spent etchant. A second etching solution is used to etch a second sheet of material. The…

US 2026/0128234 A1#2586228 Most Cited · 0 citations0.0/yr · PR 0.00PendingUS · Application
ALUMINUM OXIDE LAYER ON ANODE FOIL FOR ALUMINUM ELECTROLYTIC CAPACITOR

A method of producing a capacitor electrode includes forming an oxide layer on a foil. The method also includes heating the foil to a target temperature so as to induce defects in the oxide layer. The target temperature is about 350 ° C. to 560 ° C. and the duration of heating…