The present invention relates to a process for producing a water-absorbing polymer, comprising the process steps of (i) mixing (α1) 0.1 to 99.999% by weight of polymerizable, ethylenically unsaturated monomers containing acid groups, or salts thereof, (α2) 0 to 70% by weight of…
Henn Markus
본 발명은 (i) 하기 성분들을 혼합시키는 단계, (α1) 0.1 내지 99.999중량%, 바람직하게는 20 내지 98.99중량% 및 좀더 바람직하게는 30 내지 98.95중량%의 산성 기를 함유하는 중합가능한, 에틸렌계 불포화 단량체, 또는 이의 염, 또는 양성자화 또는 사급화된 질소를 포함하는 중합가능한, 에틸렌계 불포화 단량체, 또는 이의 혼합물, 특히 선호하게는 산성 기, 바람직하게는 아크릴산을 함유하는 적어도 에틸렌계 불포화 단량체를 포함하는 혼합물, (α2) 0 내지 70중량%,…
The present invention relates to a water-absorbing composition comprising water-absorbing polymer structures, on the surface of which is at least one tannin fraction which has a number-average molecular weight, determined in accordance with the test method described herein, of…
The present invention relates to a process for producing a water-absorbing polymer, comprising the steps of (i) mixing ([alpha]1) from 0.1 to 99.999% by weight, preferably from 20 to 98.99% by weight and particularly preferably from 30 to 98.95% by weight, of polymerizable,…
The present invention relates to a process for producing a water-absorbing polymer, comprising the steps of (i) mixing (α1) from 0.1 to 99.999% by weight, preferably from 20 to 98.99% by weight and particularly preferably from 30 to 98.95% by weight, of polymerizable,…
The present invention relates to a water-absorbing polymer comprising the process steps of (i) mixing (α1) 0.1 to 99.999% by weight of polymerizable, ethylenically unsaturated monomers containing acid groups, or salts thereof, (α2) 0 to 70% by weight of polymerized,…
The present invention relates to a process for producing a water-absorbing polymer, comprising the steps of (i) mixing (α1) from 0.1 to 99.999% by weight, preferably from 20 to 98.99% by weight and particularly preferably from 30 to 98.95% by weight, of polymerizable,…
The present invention relates to a water-absorbing composition comprising water-absorbing polymer structures, on the surface of which is at least one tannin fraction which has a number-average molecular weight, determined in accordance with the test method described herein, of…
Verfahren zur Herstellung wasserabsorbierender Polymerer, umfassend Verfahrenschritte (i) Mischen von (1) 0,1 bis 99,99 Gew.-% polymerisierbaren, ethylenisch ungesättigten, säuregruppenhaltigen Monomeren oder deren Salze oder polymerisierbaren, ethylenisch ungesättigten, einen…
The present invention relates to a water-absorbent composition, comprising water-absorbent polymer structures having at least one tannin fraction on the surfaces thereof, said fraction having a specific average molecular weight of at least 1,000 g/mol determined according to the…
본 발명은 (i) 하기 성분들을 혼합시키는 단계, (α1) 0.1 내지 99.999중량%, 바람직하게는 20 내지 98.99중량% 및 좀더 바람직하게는 30 내지 98.95중량%의 산성 기를 함유하는 중합가능한, 에틸렌계 불포화 단량체, 또는 이의 염, 또는 양성자화 또는 사급화된 질소를 포함하는 중합가능한, 에틸렌계 불포화 단량체, 또는 이의 혼합물, 특히 선호하게는 산성 기, 바람직하게는 아크릴산을 함유하는 적어도 에틸렌계 불포화 단량체를 포함하는 혼합물, (α2) 0 내지 70중량%,…
The present invention relates to a process for producing a water-absorbing polymer, comprising the process steps of (i) mixing ([alpha]1) 0.1 to 99.999% by weight, preferably 20 to 98.99% by weight and more preferably 30 to 98.95% by weight of polymerizable, ethylenically…
The present invention relates to a particulate absorbent polymer material having: i) a maximum APC i×10 sec value ≥1.6) for at least one number i selected from the group of integers from 2 to 12 (=APC max ); or ii) a value ≥12 for the sum total of all APC i×10 sec values for all…
The present invention relates to a particulate absorbent polymer material having: i) a maximum APC i×10 sec value ≧1.6) for at least one number i selected from the group of integers from 2 to 12 (=APC max ); or ii) a value ≧12 for the sum total of all APC i×10 sec values for all…
Die vorliegende Erfindung betrifft ein Verfahren zur Herstellung eines wasserabsorbierenden Polymers, umfassend die Verfahrenschritte (i) Mischen von (α1)0,1 bis 99,999 Gew.-% bevorzugt 20 bis 98,99 Gew.-% und besonders bevorzugt 30 bis 98,95 Gew.-% polymerisierbaren,…
The present invention relates to a water-absorbent composition, comprising water-absorbent polymer structures having at least one tannin fraction on the surfaces thereof, said fraction having a specific average molecular weight of at least 1,000 g/mol determined according to the…
The present invention relates to a water-absorbent composition, comprising water-absorbent polymer structures having at least one tannin fraction on the surfaces thereof, said fraction having a specific average molecular weight of at least 1,000 g/mol determined according to the…
The present invention relates to a particulate absorbent polymer material having at least one of the following properties: i) maximum APC for at least one number i selected from integers from 2 to 12 i x 10 seconds Value ≥ 1.6(═ APC) Most preferably Big (a) ) (ii) a ii) for all…
The invention relates to a method (100) for producing a defect-free boundary surface between a GaN semiconductor substrate and a gate dielectric of a GaN power transistor, comprising the following steps: -placing (120) at least one GaN semiconductor substrate into a device,…
Die vorliegende Erfindung betrifft ein teilchenförmiges, absorbierendes Polymermaterial, welches mindestens eine der folgenden Eigenschaften aufweist: i) einen maximalen APCi×10sec-Wert ≥ 1,6 für mindestens eine Zahl i ausgewählt aus der Gruppe der ganzen Zahlen von 2 bis 12 (=…
The present invention relates to a water-absorbent composition, comprising water-absorbent polymer structures having at least one tannin fraction on the surfaces thereof, said fraction having a specific average molecular weight of at least 1,000 g/mol determined according to the…
The invention relates to a particulate, absorbent polymer material comprising at least one of the following properties: i) a maximum APCi x 10 sec-value of >=1.6 for at least one number i selected from the group of the whole numbers from 2 to 12 (=APCmax); ii) a value for the…
The present invention relates to a process for producing a water-absorbing polymer, comprising the steps of (i) mixing (α1) from 0.1 to 99.999% by weight, preferably from 20 to 98.99% by weight and particularly preferably from 30 to 98.95% by weight, of polymerizable,…