A process for the heat treatment of a steel rail which is at a temperature which is in the austenite range which comprises quenching at least the head portion of said rail in water maintained at a temperature of at least 80° C until the temperature of said rail is such that said…
Heller Wilhelm
The invention relates to a rail having high resistance to wear in its head and high resistance to rupture in its foot. It is the characteristic feature of the invention that after rolling followed by heat treatment the rail has a fine pearlitic structure in the head and a…
The present invention relates to a method for thermal treatment of pearlitic rail steel. For increasing strength and wear resistance steels with the claimed composition are produced with a fine lamellar pearlite structure by heat treatment. During the first cycle the rail head…
An oscillation dampening system composed of masses, in which a spring and dampeners are clamped together and coupled to a railroad track to prevent the formation of ripples on the track. The system is tuned to the characteristic frequency of the railroad track and is coupled…
A low-carbon rail steel having a tensile strength of at least 900 N/mm2 and a yield point of at least 650 N/mm2 conmprising:
Abrasion resistant rails or rail wheels formed from a steel alloy having between 0.02 to 0.35 percent by weight of lead or bismuth, and a process for the production of the same comprising alloying 0.02 to 0.35 percent by weight of lead or bismuth with a rail or rail wheel steel.
The invention relates to a process for the production of steel rails with low residual stresses by means of roller straightening. Before entering the roller straightening machine, the rails, which have been cooled to below 100 DEG C following hot rolling, are heated in the rail…
The present invention relates to a method for thermal treatment of pearlitic rail steel. For increasing strength and wear resistance steels with the claimed composition are produced with a fine lamellar pearlite structure by heat treatment. During the first cycle the rail head…
The present invention relates to a process for reducing internal stresses of roller straightened rails. After the straightening operation the rail web portion is heated for a short time to temperatures ranging between 200°-700° C., preferably between 350°-500° C., and after…
The hot rail coming from the rolling mill is cooled at an accelerated rate to temperatures below 100@C at the head and foot only, whereas the web is held at temperatures of 150 to 500@C, and is then passed immediately through a roller straightening machine. With the method…
The present invention relates to a method for thermal treatment of pearlitic rail steel. For increasing strength and wear resistance steels with the claimed composition are produced with a fine lamellar pearlite structure by heat treatment. During the first cycle the rail head…
To align and straighten rails (S) to be used in a railway permanent way, after cooling at the end of hot rolling, each rail is passed through an alignment machine (R). A group of alignment rollers (1-7) act on the rail foot (F) and a group of rollers align the rail head (K). The…
A rail wheel comprising a wheel rim, wheel disc and a wheel hub wherein at least the wheel rim consists essentially of a steel having the following composition: 0.04 to 0.12 weight percent carbon 0.20 to 0.70 weight percent silicon 3.5 to 5.0 weight percent mangangese 0.005 to…
A railway-track element is disclosed not only for normal track but also for rail points. The track element is formed of vacuum-treated steel containing at least 0.53 to 0.62% C, 0.65 to 1.1% Mn, 0.8 to 1.3% Cr, 0.05 to 0.11% Mo, 0.05 to 0.11% V and </=0.02% P, the balance…
The properties of conventional steels for rails, check rails and railroad rolling components can be improved by small amounts of tellurium. This applies particularly to the wear resistance and the mechanical properties in the transverse direction and at oxygen contents of less…
In order to be able to use a railway-track element (10) not only for normal track but also for points, the invention proposes the use of a vacuum-treated steel containing at least 0.53 to 0.62 % C, 0.65 to 1.1 % Mn, 0.8 to 1.3 % Cr, 0.05 to 0.11 % Mo, 0.05 to 0.11 % V and « 0.02…
To prevent wear of the rail head in a UIC railway rail, the starting profile of the rail head (2) at the running edges (4) has in each case a radius of curvature (r3) whose length is 1/13 to 1/17 of the length of the radius of curvature (r1) of the running surface in the centre…
The present invention relates to a method for thermal treatment of pearlitic rail steel. For increasing strength and wear resistance steels with the claimed composition are produced with a fine lamellar pearlite structure by heat treatment. During the first cycle the rail head…