A process for producing a grain-oriented electrical steel sheet by so-called low-temperature slab heating including nitriding (step S7), wherein the finish temperature of finish rolling in hot rolling (step S2) is set to 950 ℃ or lower, cooling is started within 2 seconds after…
Hama Chie
Disclosed is a method for producing a directional electromagnetic steel sheet, wherein: a decarburized nitrided steel sheet is obtained by heating and hot rolling specific steel that contains 0.0005-0.0050% by mass of Te at a temperature not more than 1,320˚C, and then…
A predetermined steel containing Te: 0.0005 mass% to 0.0050 mass% is heated to 1320°C or lower to be subjected to hot rolling, and is subjected to annealing, cold rolling, decarburization annealing, and nitridation annealing, and thereby a decarburized nitrided steel sheet is…
A predetermined steel containing Te: 0.0005 mass % to 0.0050 mass % is heated to 1320° C. or lower to be subjected to hot rolling, and is subjected to annealing, cold rolling, decarburization annealing, and nitridation annealing, and thereby a decarburized nitrided steel sheet…
Disclosed is a process for producing a unidirectional electromagnetic steel sheet, which employs so-called "low-temperature slab heating" that involves a nitriding treatment (step S7), wherein the temperature at which a finishing rolling procedure in hot rolling (step…
In a method of manufacturing a grain-oriented electrical steel sheet including a nitriding treatment (step S 7 ) and adopting so-called “low-temperature slab heating”, the finish temperature of finish rolling in hot rolling (step S 2 ) is set to 950° C. or below, the cooling is…
질화 처리(스텝 S7)를 포함하는 소위 저온 슬래브 가열을 채용한 일방향성 전자기 강판의 제조 방법에 있어서, 열간 압연(스텝 S2)의 마무리 압연의 종료 온도를 950℃ 이하로 하고, 마무리 압연의 종료부터 2초간 이내에 냉각을 개시하고, 700℃ 이하의 온도에서 권취를 행한다. 또한, 마무리 압연의 종료부터 권취를 행할 때까지 사이의 냉각 속도를 10℃/sec 이상으로 한다. 열간 압연 강대의 어닐링(스텝 S3)에서는, 800℃ 내지 1000℃의 온도 범위 내에서의 승온 속도를 5℃/sec…
In a method of manufacturing a grain-oriented electrical steel sheet including a nitriding treatment (step S 7 ) and adopting so-called “low-temperature slab heating”, the finish temperature of finish rolling in hot rolling (step S 2 ) is set to 950° C. or below, the cooling is…
In a method of manufacturing a grain-oriented electrical steel sheet including a nitriding treatment (step S7) and adopting so-called "low-temperature slab heating", the finish temperature of finish rolling in hot rolling (step S2) is set to 950°C or below, the cooling…
método de produção de chapa de aço elétrico com grão orientado. a presente invenão refere-se a um aço predeterminado contendo te: 0,0005% em massa a 0,0050% em massa que é aquecido a 1320<198>c ou menos para ser submetido á laminação a quente, e é submetido a recozimento,…
The invention provides a method for manufacturing a grain-oriented electrical steel sheet. Wherein the compound is prepared by mixing a compound containing Te: 0.0005 to 0.0050 mass% of a predetermined steel is heated to 1320 ℃ or lower, hot-rolled, annealed, cold-rolled,…
A predetermined steel containing Te: 0.0005 mass % to 0.0050 mass % is heated to 1320° C. or lower to be subjected to hot rolling, and is subjected to annealing, cold rolling, decarburization annealing, and nitridation annealing, and thereby a decarburized nitrided steel sheet…