A POLYBUTYLENE TEREPHTHALATE MELT AT A TEMPERATURE IN THE RANGE OF THE MELT TEMPERATURE OF POLYBUTYLENE TEREPTHALATE AND 495*F., AND HAVING AM INTRINSIC VISOCITY OF AT LEAST 1.05 DECILITERSPER GRAM IS BLOW MOLDED INAN EXTRUSION BLOW MOLDING APPARATUS THE MOLD OF WHICH IS…
Inventor / Author Profile
Halek G
14Total Forward Citations
7Indexed Patents
1Patent H-Index
Frequent Co-Inventors: Berardinelli F Carrington R Freed W Gall J Hendry C Pauls S Roberts W Rupp R Schaul J
Non-digestible food additives are prepared by heating starch with an edible di- or tri-basic carboxylic acid and anhydrides thereof acid at 140 DEG to 220 DEG C. under reduced pressure and in the presence of less than 5% water for sufficient time to form a non-digestible product.