In the prodn. of linear polyesters (I) by discontinuous direct esterification of HOCH2CH2OH (II) and terephthalic acid (III) in 1.1-2.0:1 molar ratio, in which (III) is added to preheated (II), the reactor contains 0.1-1.4, pref. 0.3-0.8 mole (II)/mole (III) and is heated above…
Inventor / Author Profile
Haeckel Eberhard
3Total Forward Citations
6Indexed Patents
1Patent H-Index
Prepn. of polyamide fibres heat-stabilised with Cu cpds., in which an amt. corresp. to 10-40 p.p.m. Cu is added before spinning, and the remainder as a Cu salt is added with the spinning prepn. to the fibres. Used esp. for polyamide tyre cords. Harmful effects of Cu deposits in…
1,147,286. Oxidation of cyclohexane. VICKERS-ZIMMER A.G. PLANUNG UND BAU VON INDUSTRIEANLAGEN. 14 June, 1967 [14 June, 1966], No. 27477/67. Heading C2C. The invention relates to a process for the controlled oxidation of cyclohexane to convert from 4 to 15% of the latter to…