The use of a chromium-containing martensitic alloy for plastic molds is described. The use properties of a thermally treated plastic mold of a hardness of at least 45 Rockwell C are improved by an iron-based alloy including, in weight-%, ______________________________________ C…
Hackl Gerhard
Iron-based alloy contains (in wt.%): 0.25-1, pref. 0.4-0.8, C; max. 1 Si; max. 1.6, pref. 0.3-0.8, Mn; 0.1-0.35, pref. 0.12-0.29, N; max. 1, pref. 0.002-0.8, Al; max. 2.8 Co, 14-25, pref. 16-19, Cr; 0.5-3, pref. 0.8-1.5, Mo; max. 3.9, pref. max 1.5 Ni; 0.04-0.4, pref. 0.05-0.2,…
A process for making and using machine parts which in their function are exposed to severe stress from sliding superficial friction and machine parts produced thereby are described. The parts are made from an iron-based alloy which includes the following elements, in weight %:…
Corrosion-resistant alloy having a hardness of more than 54 HRC consists of (in wt.%):0.40-0.85 C, up to 1.0 Si,, up to 1.4Mn, 16.0-19.0 G, 0.8-1.5 Mo, 0.05-0.2 V, up to 0.18 Ti, 0.12-0.29 N, with the proviso that Ni max is 0.25, Co max. is 0.20, Cu max is 0.25, and Ni + Co +…
Process for the powder-metallurgical production of work pieces, particularly tools, containing high-melting point carbides and/or carbonitrides homogeneously distributed in a matrix, in which an amount of elements of the IVa and Va groups, or secondary groups, of the periodic…
The invention relates to a process for the production of preformed material for workpieces, preferably tools, in particular of high-speed steel, having a high proportion of metal compounds. To achieve good hot workability in conjunction with a high proportion of metal compounds…
The present invention relates to use of a chromium-containing martensitic alloy for plastic molds. The use properties of a thermally treated plastic mold of a hardness of at least 45 HRC are improved by an iron-based alloy including, in weight%, C 0.25 to 1.0, preferably 0.4 to…
The use of a ferrous alloy for the mfr. of machine parts subject to high wear by sliding surface rubbing. The ferrous alloy contains in wt.%: 0.35-1 pref. 0.4-0.8 C; max. 1 Si; max. 1.6, pref. 0.3-1.4 N; max. 1 pref. max. 0.8 Al; max. 2.0 Co; 14-25, pref. 16-19 Cr; 0.5-03, pref.…
Turbine blade has a tensile strength Rm of at least 700 N/mm<2>, a creep limit Rp0.2, an expansion A of at least 15% and a constriction Z of at least 10%. The blade is produced from a powder metallurgical feed material formed by pulverizing a melt by atomizing with…
PROBLEM TO BE SOLVED: To provide a mold economically preparable with a little size change and having improved use performance. SOLUTION: This alloy is an iron-based alloy including, by wt.% 0.25-1.0C, max. 1.0 Si, max. 1.6 Mn, 0.10-0.35 N, max. 1.0 Al, max. 2.8 Co, 14.0-25.0 Cr,…
Die Erfindung betrifft ein Verfahren und eine Anordnung zur Recyclierung von Kunststoffen umfassend die folgenden Bearbeitungsschritte: a) Aufbereitung des Rohmaterials, wobei das Material, falls erforderlich zerkleinert und, in eine fluidartige Form gebracht wird und unter…
In a process for making workpieces, in particular tools, with refractory carbides and/or carbonitrides homogeneously distributed in a matrix by powder metallurgy, a content of the elements of group or subgroup IV and V of the periodic table of at least 3 % by weight and a low…
Corrosion-resistant alloy having a hardness of more than 54 HRC consists of (in wt.%):0.40-0.85 C, up to 1.0 Si,, up to 1.4Mn, 16.0-19.0 G, 0.8-1.5 Mo, 0.05-0.2 V, up to 0.18 Ti, 0.12-0.29 N, with the proviso that Ni max is 0.25, Co max. is 0.20, Cu max is 0.25, and Ni + Co +…
El invento se refiere a una composición de una aleación martensítica que contiene cromo para moldes para materiales sintéticos. Para mejorar laspropiedades de uso de un molde templado para material sintético, con una dureza de al menos 45 HRC, seprevee una aleación a base de…
Corrosion-resistant alloy having a hardness of more than 54 HRC consists of (in wt.%):0.40-0.85 C, up to 1.0 Si,, up to 1.4Mn, 16.0-19.0 G, 0.8-1.5 Mo, 0.05-0.2 V, up to 0.18 Ti, 0.12-0.29 N, with the proviso that Ni max is 0.25, Co max. is 0.20, Cu max is 0.25, and Ni + Co +…
The use of a chromium-containing martensitic alloy for plastic molds is described. The use properties of a thermally-treated plastic mold of a hardness of at least 45 Rockwell C are improved by an iron-based alloy including, in weight-%: C 0.25 to 1.0, preferably 0.4 to 0.8; N…
The use of a chromium-containing martensitic alloy for plastic molds is described. The use properties of a thermally-treated plastic mold of a hardness of at least 45 Rockwell C are improved by an iron-based alloy including, in weight-%: C 0.25 to 1.0, preferably 0.4 to 0.8; N…
The present invention relates to use of a chromium-containing martensitic alloy for plastic molds. The use properties of a thermally treated plastic mold of a hardness of at least 45 HRC are improved by an iron-based alloy including, in weight%, C 0.25 to 1.0, preferably 0.4 to…
LA PRESENTE INVENCION SE REFIERE A UN MOLDE PARA PLASTICOS EL CUAL TIENE UNA ALTA RESISTENCIA A LA CORROSION Y/O ABRILLANTABILIDAD Y ESTA HECHO DE UNA ALEACION MARTENSITICA QUE CONTIENE CROMO PRA EL MEJORAMIENTO DE LAS PROPIEDADES DE USO SE HA PREVISTO UNA DUREZA DE MATERIAL DE…