Hydrophilic flexible polyurethane foam which foam is in a compressed state above its glass transition temperature and at ambient pressure in the absence of force suitable to create the compressed state.
Gerber Dirk
Process for preparing a flexible foam by reacting a prepolymer having an NCO value of 3-15% by weight, which is the reaction product obtained by reacting an excessive amount of a polyisocyanate with a polyether polyol or a mixture of such polyols, said polyol or mixture having…
Process for preparing a flexible foam by reacting a prepolymer having an NCO value of 3-15 % by weight, which is the reaction product obtained by reacting an excessive amount of a polyisocyanate with a polyether polyol or a mixture of such polyols, said polyol or mixture having…
Process for preparing a flexible foam by reacting a prepolymer having an NCO value of 3-15% by weight, which is the reaction product obtained by reacting an excessive amount of a polyisocyanate with a polyether polyol or a mixture of such polyols, said polyol or mixture having…
Process for preparing a flexible foam by reacting a prepolymer having an NCO value of 3-15% by weight, which is the reaction product obtained by reacting an excessive amount of a polyisocyanate with a polyether polyol or a mixture of such polyols, said polyol or mixture having…
Process for preparing a flexible foam by reacting a prepolymer having an NCO value of 3-15% by weight, which is the reaction product obtained by reacting an excessive amount of a polyisocyanate with a polyether polyol or a mixture of such polyols, said polyol or mixture having…
Process for making a flexible foam by reacting a polyisocyanate composition having an NCO value of 10-25% by weight and 30-150 parts by weight, per 100 parts by weight of polyisocyanate composition, of a polyol composition comprising water at an isocyanate-index of 40-100.
Hydrophilic flexible polyurethane foam which foam is in a compressed state above its glass transition temperature and at ambient pressure in the absence of force suitable to create the compressed state.
Process for making a flexible foam by reacting a polyisocyanate composition having an NCO value of 10-25% by weight and 30-150 parts by weight, per 100 parts by weight of polyisocyanate composition, of a polyol composition comprising water at an isocyanate-index of 40-100.
Process for removing unwanted material from wanted material containing water by bringing an isocyanate-containing prepolymer into contact with the materials, allowing the prepolymer to react with the water to form a flexible foam and removing the foam obtained from the wanted…
Process for preparing a flexible foam by reacting a prepolymer having an NCO value of 3-15 % by weight, which is the reaction product obtained by reacting an excessive amount of a polyisocyanate with a polyether polyol or a mixture of such polyols, said polyol or mixture having…
Process for making a flexible foam by reacting a polyisocyanate composition having an NCO value of 10-25 % by weight and 30-150 parts by weight, per 100 parts by weight of polyisocyanate composition, of a polyol composition comprising water at an isocyanate-index of 40-100.
Prepn. of a flexible foam comprises reacting water with a prepolymer (NCO value of 3-15 wt.%) which is the result of the reaction of excess polyisocyanate and at least one polyether polyol characterised by an average hydroxyl functionality of 2-6, an average hydroxyl equivalent…
<P>PROBLEM TO BE SOLVED: To provide a process for manufacturing a novel polymer flexible foam. <P>SOLUTION: The method for the preparation of a flexible foam comprises reacting a prepolymer, having an NCO value of 3-15% by weight which is the reaction product…
Process for preparing a flexible foam by reacting a prepolymer having an NCO value of 3-15% by weight, which is the reaction product obtained by reacting an excessive amount of a polyisocyanate with a polyether polyol or a mixture of such polyols, said polyol or mixture having…
Process for making a flexible foam by reacting a polyisocyanate composition having an NCO value of 10-25% by weight and 30-150 parts by weight, per 100 parts by weight of polyisocyanate composition, of a polyol composition comprising water at an isocyanate-index of 40-100.
The use of a polyurethane foam for absorbing/adsorbing hydrophobic liquid.
The use of a polyurethane foam for absorbing/adsorbing hydrophobic liquid.
Process for removing unwanted material from wanted material containing water by bringing an isocyanate-containing prepolymer into contact with the materials, allowing the prepolymer to react with the water to form a flexible foam and removing the foam obtained from the wanted…