hottub.patents
US 4,741,747 A#506942 Most Cited · 69 citations1.8/yr · PR 7.98ExpiredUS · Utility
Method of fabricating optical fibers
Inventors: Geittner Peter E E, Weling Alfred L MAssignee: Philips CorpFiled 1985-12-06 · Granted 1988-05-03

In the PCVD method glass layers are deposited on the inner wall of a glass tube by heating the tube to a temperature between 1100° and 1300° C., passing a reactive gas mixture at a pressure between 1 and 30 hPa through the glass tube, and moving back and forth inside the glass…

US 5,106,402 A#503160 Most Cited · 69 citations2.0/yr · PR 11.11ExpiredUS · Utility
Method of manufacturing a monomode optical fiber
Inventors: Geittner Peter E E, Hagemann Hans-juergen E, Lydtin Hans-juergenAssignee: Philips CorpFiled 1990-09-27 · Granted 1992-04-21

In the manufacture of preforms for optical fibres, the materials of the core (α) and of the light-conducting cladding layer (β 1 ) are previously deposited from the gaseous phase. Deposition time is here considerably reduced in that only the materials of the core (α) and a part…

US 4,714,589 A#723898 Most Cited · 57 citations1.5/yr · PR 13.55ExpiredUS · Utility
Method of and device for coating the inside of tubes
Inventors: Auwerda Cornelis P, Geittner Peter E E, Lydtin Hans-juergenAssignee: Philips CorpFiled 1986-06-30 · Granted 1987-12-22

The inside of a tube of an electrically insulating material is coated with a layer of electrically insulating material by reactive deposition of the coating material from a gas mixture which is passed through the tube. The tube is heated and the deposition is activated by a…

US 5,188,648 A#1135041 Most Cited · 45 citations1.4/yr · PR 6.29ExpiredUS · Utility
Method of manufacturing optical fibres
Inventors: Geittner Peter E E, Hagemann Hans-juergen, Warnier Jacques P MAssignee: Philips CorpFiled 1991-10-16 · Granted 1993-02-23

In the PCVD method glass is deposited in layers on the inner wall of a glass tube by heating the tube to a temperature between 1100° and 1300° C., by passing a reactive gas mixture through the glass tube from a gas inlet side at a pressure between 1 and 30 hPa, by forming a…

US 4,802,733 A#1457392 Most Cited · 39 citations1.1/yr · PR 6.10ExpiredUS · Utility
Fluorine-doped optical fibre and method of manufacturing such fibre
Inventors: Bachmann Peter K, Geittner Peter E E, Leers Dieter, Wilson Howard J CAssignee: Philips CorpFiled 1985-12-30 · Granted 1989-02-07

In an optical fiber based on silicon dioxide with fluorine doping which determines its refractive index profile, at least in the light transmitting core a substance is added that increases the thermal expansion coefficient. The added substance is uniformly distributed at least…

US 4,857,091 A#1946287 Most Cited · 33 citations0.9/yr · PR 4.71ExpiredUS · Utility
Method of manufacturing optical fibers
Inventors: Geittner Peter E E, Lydtin Hans-juergen, Wilson Howard J CAssignee: Philips CorpFiled 1987-10-08 · Granted 1989-08-15

Optical fibres whose refractive index profiles show specific peripheral and/or radial and/or axial optical modulation structures are manufactured according to the PCVD method, in which such method parameters are varied which influence: (a) the uniformity of the material…

US 5,049,406 A#5092879 Most Cited · 17 citations0.5/yr · PR 8.64ExpiredUS · Utility
Method of manufacturing solid bodies
Inventors: Geittner Peter E E, Lydtin Hans-juergenAssignee: Philips CorpFiled 1989-07-11 · Granted 1991-09-17

A substrate (35) is coated by using starting materials which are supplied in the form of clusters (28). The clusters are disintegrated into their molecular or atomic constituents, and the constituents are deposited on the substrate in the form of compact layers (34). In this…

CA 1,242,889 A#139338166 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Method of manufacturing optical fibres
Inventors: Geittner Peter E E, Lydtin Hans, Wilson Howard J CAssignee: Philips NvFiled 1984-07-11 · Granted 1988-10-11

ABSTRACT: In the PCVD method, glass layers are deposited on the inner wall of a glass tube heated at a temperature between 1100 and 1300°C by passing a reactive gas mixture through the glass tube at a pressure between 1 and 30 mbar, while a plasma is reciprocated strokewise in…

CA 1,258,993 A#100583363 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Method of and device for coating the inside of tubes
Inventors: Auwerda Cornelis P, Geittner Peter E E, Lydtin Hans-juergenAssignee: Philips NvFiled 1986-07-31 · Granted 1989-09-05

ABSTRACT: Method of and device for coating the inside of tubes. For coating the inside of a tube of an electrically insulating material with a second electrically insulating material by reactive deposition of the second electrically insulating material from a gas mixture which…

CA 1,266,978 A#82848988 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Method of manufacturing optical waveguides
Inventors: Bachmann Peter K, Geittner Peter E E, Lydtin Hans-juergen, Wilson Howard J CAssignee: Philips NvFiled 1984-05-17 · Granted 1990-03-27

Abstract: Method of manufacturing optical waveguides. In a method in which compact glass layers are directly produced on the inside of a substrate tube from a reactive gas mixture without sintering, a volatile hydrogen-free fluorine compound is added to the mixture of the…

CA 1,293,126 C#91827859 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Method of manufacturing optical fibres
Inventors: Geittner Peter E E, Hagemann Hans-juergen, Warnier JacquesAssignee: Geittner Peter E EFiled 1986-07-17 · Granted 1991-12-17

PHD.85-105 13 2.5.86 ABSTRACT: Method of manufacturing optical fibres. In the PCVD method glass is deposited in layers on the inner wall of a glass tube heated at a temperature between 1100 and 1300°C by passing a reactive gas mixture through the glass tube from a gas inlet side…