Method of producing peroxide bleached pulp from fibrous lignocellulose materials which are subjected to a defibration step in a grinding space defined between a pair of discs which rotate relative to one another within a steam pressurized grinding housing. The pulp material is…
Falk Bo
An absorbent, chemithermomechanical pulp produced from lignocellulosic material with a wood yield above 88 %, a low resin content < 0.15 %, a long fibre content above 70 %, a short fibre content below 10 % and a shive content below 3 %. A method for producing the pulp. The…
An absorbent, chemithermomechanical pulp produced from lignocellulosic material with a wood yield above 88%, a low resin content <0.15%, a long fiber content above 70%, a short fiber content below 10% and a shive content below 3%. The method for producing the pulp comprises…
Methods for producing mechanical pulp are disclosed including impregnating softwood chips with water and a complexing agent, refining the impregnated chips in a first refining step including a double-disk refiner, fractionating the refined softwood pulp to produce a reject…
An absorbent, chemithermomechanical pulp produced from lignocellulosic material with a wood yield above 88%, a low resin content <0.15%, a long fibre content above 70%, a short fibre content below 10% and a shive content below 3. The method for producing the pulp comprises…
Processes are disclosed for processing low consistency newsprint pulp including refining the pulp in a first refiner to a consistency of greater than 2%, screening the processed pulp with a slotted screen basket with a slot width of from 0.05 to 0.15 mm, with the withdrawal of…
A method of producing mechanical and chemi-mechanical pulp with a yield above 85 % from lignocellulose-containing material for the manufacture of paper or board products. The material is subjected to mechanical processing in at least two steps. The material at its feed into the…
The present invention relates to a process for production of upgraded TMP to SC/LWC qualities. The newsprint pulp is pumped to an LC-refiner (1) in which the average fibre length is reduced, and is then transferred to a primary screen (2) in which the pulp is divided into a…
The processing comprises screening for dividing the pulp into an accept and a reject fraction, of which the reject fraction constitutes 10-40%. The reject fraction is dewatered, impregnated with sodium sulphite and preheated with steam. Thereafter refining is carried out under…
A method for producing chemithermomechanical pulp from lignocellulosic material, by preheating and refining the material at an elevated temperature of 160-180 °C, subsequent to pre-impregnating the chips with an impregnating liquid that contains borohydride, at least one…
A method of producing mechanical and chemi-mechanical pulp with a yield above 85 % from lignocellulose-containing material for the manufacture of paper or board products. The material is subjected to mechanical processing in at least two steps. The material at its feed into the…
Mechanical pulp intended for coated light weight paper (LWC), magazine paper or the like made as follows. Impregnation and preheating of the material, refining in a double-disc refiner, bleaching, refining in a single-disc refiner and screening of the pulp.
A method of producing mechanical and chemi-mechanical pulp with a yield above 85 % from lignocellulose-containing material for the manufacture of paper or board products. The material is subjected to mechanical processing in at least two steps. The material at its feed into the…
A method for producing mechanical pulps which are useful for producing coated light weight paper, magazine paper and the like, is disclosed, which includes preheating lignocellulose-containing material in the presence of impregnation chemicals, refining the preheated…
Manufacture of chemi-mechanical pulp from hardwood intended for wood-containing printing paper, especially wood-containing fine paper. The wood material in the form of chips is impregnated in one or two steps at a temperature below 80°C with 15-40 kg NaOH and 0-30 kg Na2SO3 per…
Processes are disclosed for processing low consistency newsprint pulp including refining the pulp in a first refiner to a consistency of greater than 2%, screening the processed pulp with a slotted screen basket with a slot width of from 0.05 to 0.15 mm, with the withdrawal of…
The making of mechanical pulp from softwood intended for coated light-weight paper (LWC), for uncoated calendered magazine paper (FSC) or the like is carried out in several steps as follows: a) impregnation (2) of chips with water in combination with complex-forming agent; b)…
A method of producing mechanical and chemi-mechanical pulp with a yield above 85 % from lignocellulose-containing material for the manufacture of paper or board products. The material is subjected to mechanical processing in at least two steps. The material at its feed into the…
An absorbent, chemithermomechanical pulp produced from lignocellulosic material with a wood yield above 88%, a low resin content <0.15%, a long fibre content above 70%, a short fibre content below 10% and a shive content below 3. The method for producing the pulp comprises…
A process for regulating the prepn. of mechanical pulp for lignocellulosic material fed into a defibrator (15) contg. two grinding discs rotating in different directions for grinding down material and then passing it out at 50-200 CSF selected freeness and with a chosen reduced…
Processes are disclosed for processing low consistency newsprint pulp including refining the pulp in a first refiner to a consistency of greater than 2%, screening the processed pulp with a slotted screen basket with a slot width of from 0.05 to 0.15 mm, with the withdrawal of…
A method of producing mechanical and chemi-mechanical pulp with a yield above 85 % from lignocellulose-containing material for the manufacture of paper or board products. The material is subjected to mechanical processing in at least two steps. The material at its feed into the…