High gas barrier, delamination-resistant polyamide compositions suitable for extended shelf-life packaging applications are provided. Also provided are polyamide compositions exhibiting high oxygen scavenging capability. The polyamide compositions comprise mXDA-IPA containing…
Facinelli John V
The invention relates to epoxy-terminated polymers and copolymers derived from hydrosilyl-terminated hydrogenated polydienes and polyvinyl aromatics, and a process for preparing these polymers and copolymers. The epoxy-terminated polymers and copolymers are reactive with a…
A polyamide having a viscosity of between about 20 and about 40 FAV and a number average molecular weight of between about 9,000 and about 16,000 grams per mole is provided. The polyamide also includes un-terminated endgroups, where a difference between a concentration of…
High gas barrier, delamination-resistant polyamide compositions suitable for extended shelf-life packaging applications are provided. Also provided are polyamide compositions exhibiting high oxygen scavenging capability. The polyamide compositions comprise mXDA-IPA containing…
A polyamide composition is formed by combining a phosphorous containing catalyst with monomer starting materials under conditions suitable to cause polymerization of the monomer starting material into a low molecular weight polyamide material. The polyamide material, which may…
The present invention relates to the epoxy-terminated homopolymer and the multipolymer that obtain by hydrogenation silicomethane end group hydrogenation polydiene and polyvinyl aromatics and the method for preparing these homopolymer and multipolymer.These epoxy-terminated…
Methods for mixing nylon compounds and compositions useful in mixing nylon compounds are provided. The methods and compositions disclosed are useful in producing nylon for wire and cable jacketing. The disclosed methods provide nylon having a reduced heat history compared to…
Polyamide compositions for use in forming wire or cable jacket compositions. The polyamide compositions include a component of polyamide 6/66 copolymer formed from substantially randomly distributed caprolactam monomers and hexamethylene diamine monomers. The polyamide 6/66…
Polyamide compositions for use in forming wire or cable jacket compositions. The polyamide compositions include a component of polyamide 6/66 copolymer formed from substantially randomly distributed caprolactam monomers and hexamethylene diamine monomers. The polyamide 6/66…
High gas barrier, delamination-resistant polyamide compositions suitable for extended shelf-life packaging applications are provided. Also provided are polyamide compositions exhibiting high oxygen scavenging capability. The polyamide compositions comprise mXDA-IPA containing…
Amorphous polyamide terpolymers with a high level of transparency, transition glass temperature, flexibility, and chemical resistance. In one embodiment, the polyamide terpolymers are polymerized from caprolactam, at least one diamine, and at least one diacid.
Amorphous polyamide terpolymers with a high level of transparency, transition glass temperature, flexibility, and chemical resistance. In one embodiment, the polyamide terpolymers are polymerized from caprolactam, at least one diamine, and at least one diacid.
Methods for mixing nylon compounds and compositions useful in mixing nylon compounds are provided. The methods and compositions disclosed are useful in producing nylon for wire and cable jacketing. The disclosed methods provide nylon having a reduced heat history compared to…
High gas barrier, delamination-resistant polyamide compositions suitable for extended shelf-life packaging applications are provided. Also provided are polyamide compositions exhibiting high oxygen scavenging capability. The polyamide compositions comprise mXDA-IPA containing…
A polyamide having a viscosity between about 20 and about 40FAV and a number average molecular weight between about 9000 and about 16000 grams per mole is provided. The polyamide also includes endcapped end groups, wherein the difference between the concentration of carboxylic…
A polyamide having a viscosity of between about 20 and about 40 FAV and a number average molecular weight of between about 9,000 and about 16,000 grams per mole is provided. The polyamide also includes un-terminated endgroups, where a difference between a concentration of…
Methods for mixing nylon compounds and compositions useful in mixing nylon compounds are provided. The methods and compositions disclosed are useful in producing nylon for wire and cable jacketing. The disclosed methods provide nylon having a reduced heat history compared to…
High gas barrier, delamination-resistant polyamide compositions suitable for extended shelf-life packaging applications are provided. Also provided are polyamide compositions exhibiting high oxygen scavenging capability. The polyamide compositions comprise mXD A-IPA containing…
Polyamide base resins with improved crystallization dynamics for the production of reinforced polyamide compositions having improved surface, shrink, warpage and mechanical properties such as toughness. The polyamide base resins are copolymers of polyamide 6 and polyamide 66,…
Polyamide base resins with improved crystallization dynamics for the production of reinforced polyamide compositions having improved surface, shrink, warpage and mechanical properties such as toughness. The polyamide base resins are copolymers of polyamide 6 and polyamide 66,…
A polyamide having a viscosity of between about 20 and about 40 FAV and a number average molecular weight of between about 9,000 and about 16,000 grams per mole is provided. The polyamide also includes un-terminated endgroups, where a difference between a concentration of…
A polyamide having a viscosity of between about 20 and about 40 FAV and a number average molecular weight of between about 9,000 and about 16,000 grams per mole is provided. The polyamide also includes un-terminated endgroups, where a difference between a concentration of…
A polyamide having a viscosity of between about 20 and about 40 FAV and a number average molecular weight of between about 9,000 and about 16,000 grams per mole is provided. The polyamide also includes un-terminated endgroups, where a difference between a concentration of…
Polyamides terminated at the amine end group, the carboxyl end group, or both the amine and carboxyl end groups. Specifically, the present disclosure relates to terminated polyamide polymers having a weight average molecular weight (Mw) from 22,000 Da to 56,000 Da and a formic…
The invention relates to epoxy-terminated polymers and copolymers derived from hydrosilyl-terminated hydrogenated polydienes and polyvinyl aromatics, and a process for preparing these polymers and copolymers. The epoxy-terminated polymers and copolymers are reactive with a…