Silicon wafers are first subjected to an oxidative treatment and subsequey to exposure to organosilicon compounds which contain at least one radical in the molecule which is hydrolyzably bound to the silicon and at least one radical in the molecule having hydrophilic properties.…
Fabry Laszlo
PROBLEM TO BE SOLVED: To provide chunk polycrystalline silicon having a surface carbon concentration of 0.5-35 ppbw.SOLUTION: In a method for cleaning a polycrystalline silicon chunk having carbon contamination on the surface, a heat treatment of the polycrystalline silicon…
The invention relates to a method for producing polycrystalline silicon rods by deposition of silicon on at least one thin rod in a reactor, wherein, before the silicon deposition, hydrogen halide at a temperature of 400-1000° C. is introduced into the reactor containing at…
The invention provides chunk polycrystalline silicon having a concentration of carbon at the surface of 0.5-35 ppbw. A process for cleaning polycrystalline silicon chunks having carbon contaminations at the surface, includes a thermal treatment of the polycrystalline silicon…
The subject of the invention is a cosmetic preparation for teeth which is composed of one or more film-forming polymers--at least one of which is water soluble, partly soluble, emulsifiable or dispersible--and coloring agents. The composition ensures the aesthetic appearance of…
The ability of aq. cleaning compsns. to remove metal-contg. residues from semiconductor surfaces, esp. Si wafers, is improved by treating the compsn. with CO2 and/or oxalic acid. The cleaning compsn. is pref. water or an aq. nonionic surfactant soln. CO2 is added in an amt.…
Bei der Behandlung von Halbleiter-, insbesondere Siliciumscheiben mit wäßrigen flußsäurehaltigen Lösungen wird in der Regel eine Kontamination der Scheibenoberfläche mit die nachfolgenden Prozesse störenden Partikeln beobachtet. Diese Partikelzunahme kann dadurch deutlich…
PROBLEM TO BE SOLVED: To provide a polycrystalline silicon chunk which is a cube having a metal content of below 200 pptw and a dopant content of below 50 ppta.SOLUTION: The provided method for manufacturing a polycrystalline silicon chunk includes the steps of: feeding a…
The invention relates to a process for preparing trichlorosilane by reacting metallurgic silicon and HCl in a fluid-bed reactor at a temperature of 290°C to 400°C, the process being characterized in that a high-boiling compound is fed to the fluid-bed reactor.
Gegenstand der Erfindung ist ein Verfahren zur Herstellung einer Halbleiterscheibe mit einer Vorderseite und einer Rückseite, bei dem die Halbleiterscheibe einer beidseitigen Politur unterzogen wird. Das Verfahren beinhaltet folgende zeitliche Reihenfolge von Schritten: DOLLAR A…
Cubic polycrystalline silicon chunks comprise less than 200 parts per trillion by weight (pptw) of metal and less than 50 parts per trillion atoms (ppta) of dopant on their surfaces. An independent claim is included for producing polycrystalline silicon chunks comprising…
The present invention relates to polycrystalline silicon chunks which are cubic and have a metal content of less than 200 pptw and a dopant content of less than 50 ppta. Methods for producing polycrystalline silicon chunks, include the steps of providing a polycrystalline…
A method is provided to remove crystal regions from silicon wafers which are damaged as a consequence of mechanical machining of the silicon wafers. The silicon wafers are pretreated with an aqueous solution containing hydrogen fluoride. Then the wafers are etched in an aqueous…
A process for producing silicon wafers which have a storage-stable surface and which can be thermally oxidized directly, that is to say, without a prior HF immersion bath, and without the addition of halogen-containing gases, it being possible to achieve an equal or better…
A process is for producing a semiconductor wafer with a front surface and a back surface, in which the semiconductor wafer is subjected to two-sided polishing. The process includes the following: (a) producing a hydrophobic surface on the semiconductor wafer by treating the…
The invention relates to a polycrystalline silicon portion having at least one fracture surface or cut surface, which comprises metal contamination of from 0.07 ng/cm2 to 1 ng/cm2. The invention also relates to a method for breaking a silicon body, preferably a rod of…
The unit tests filters used for air cleaning. It passes a flow of ambient air (3) containing impurities through a test filter, taking a sample before and after so doing. An instrument measures and records physical data from the air stream. A novel feature is a trolley (1)…
Gegenstand der Erfindung ist ein polykristallines Siliciumbruchstück mit einer Konzentration von Kohlenstoff an der Oberfläche von 0,5–35 ppbw. Verfahren zur Reinigung von polykristallinen Siliciumbruchstücken mit Kohlenstoff-Kontaminationen an der Oberfläche, umfassend eine…
The invention provides chunk polycrystalline silicon having a concentration of carbon at the surface of 0.5-35 ppbw. A process for cleaning polycrystalline silicon chunks having carbon contaminations at the surface, includes a thermal treatment of the polycrystalline silicon…
The method involves pretreating the silicon plates with a water sol. contg. hydrofluoric acid and then etching it in a water sol. contg. alkali metal hydroxide at a temp. of 55 to 95 deg. C. The plates are immersed for preliminary treatment in the water sol. contg. 1 to 5 wt.%…
Polycrystalline silicon fracture-piece with 0.5-35 ppbw carbon concentration on the surface, is claimed. An independent claim is also included for cleaning the polycrystalline silicon fracture-piece having carbon contamination on the surface, comprising carrying out thermal…
A process is for producing a semiconductor wafer with a front surface and a back surface, in which the semiconductor wafer is subjected to two-sided polishing. The process includes the following: (a) producing a hydrophobic surface on the semiconductor wafer by treating the…
The disclosure relates to an apparatus and a method for producing a single crystal of semiconductor material. The apparatus comprises a chamber and a crucible which is arranged in the chamber and is enclosed by a crucible heater, a radiation shield for shielding a growing single…
Use of a compound of general formula RnZpSiX(4-n-p) for the treatment of steel surfaces, wherein X is selected from a group consisting of H, OH, halogen, alkoxy (C1-C3), acyloxy (C1-C3) and NR1R2; wherein each of R1 and R2 is selected from a group consisting of H, methyl and…
Polycrystalline silicon pieces having at least one break or cut surface and a metal contamination of 0.07-1 ng/cm 2>, is claimed. An independent claim is included for breaking silicon body, preferably a rod made of polycrystalline silicon, comprising (a) determining a lowest…