A device includes a substrate and a Ill-nitride structure grown on the substrate, the Ill-nitride structure comprising a light emitting layer disposed between an n-type region and a p-type region. The substrate is a RAO3(MO)n, where R is one of a trivalent cation, Sc, In, Y, and…
Epler John Edward
A device includes a substrate ( 10 ) and a III-nitride structure ( 15 ) grown on the substrate, the III-nitride structure comprising a light emitting layer ( 16 ) disposed between an n-type region ( 14 ) and a p-type region ( 18 ). The substrate is a RAO 3 (MO) n where R is one…
LED epitaxial layers (n-type, p-type, and active layers) are grown on a substrate. For each die, the n and p layers are electrically bonded to a package substrate that extends beyond the boundaries of the LED die such that the LED layers are between the package substrate and the…
A light emitting device includes a semiconductor structure having a light emitting region ( 102 ) disposed between an N-type region ( 103 ) and a P-type region ( 101 ). A porous region ( 103 A) is disposed between the light emitting region ( 102 ) and a contact (N-contact 131 )…
In embodiments of the invention, a semiconductor structure comprising a III-nitride light emitting layer disposed between an n-type region and a p-type region is grown on a substrate. The substrate is a non-III-nitride material. The substrate has an in-plane lattice constant…
In a method according to embodiments of the invention, a III-nitride layer is grown on a growth substrate. The III-nitride layer is connected to a host substrate. The growth substrate is removed. The growth substrate is a non-III-nitride material. The growth substrate has an…
A uLED and method for regrowth with thinner deposition on sidewall are disclosed. The uLED and method include a growth substrate including flat first and second regions, where the growth substrate is thicker in the first region as compared to the second region, and a third…
A uLED and method for regrowth with thinner deposition on sidewall are disclosed. The uLED and method include a growth substrate including flat first and second regions, where the growth substrate is thicker in the first region as compared to the second region, and a third…
Techniques, devices, and systems are disclosed and include LEDs with a first flat region, at a first height from an LED base and including a plurality of epitaxial layers including a first n-layer, a first active layer, and a first p-layer. A second flat region is provided, at a…
Techniques, devices, and systems are disclosed and include LEDs with a first flat region, at a first height from an LED base and including a plurality of epitaxial layers including a first n-layer, a first active layer, and a first p-layer. A second flat region is provided, at a…
A light emitting device includes a semiconductor structure having a light emitting region (102) disposed between an N-type region (103) and a P-type region (101). A porous region (103A) is disposed between the light emitting region (102) and a contact (N-contact 131)…
In a method according to embodiments of the invention, a III-nitride layer is grown on a growth substrate. The III-nitride layer is connected to a host substrate. The growth substrate is removed. The growth substrate is a non-III-nitride material. The growth substrate has an…
Techniques, devices, and systems are disclosed and include LEDs with a first flat region, at a first height, including a plurality of epitaxial layers such as a first n-layer, a first p-layer, and a first active layer. A second flat region at a second height and parallel to the…
Techniques, devices, and systems are disclosed and include LEDs with a first flat region, at a first height, including a plurality of epitaxial layers such as a first n-layer, a first p-layer, and a first active layer. A second flat region at a second height and parallel to the…
The current distribution across the p-layer ( 130 ) of a semiconductor device is modified by purposely inhibiting current flow through the p-layer ( 130 ) in regions ( 310 ) adjacent to the guardsheet ( 150 ), without reducing the optical reflectivity of any part of the device.…
The current distribution across the p-layer (130) of a semiconductor device is modified by purposely inhibiting current flow through the p- layer (130) in regions (310) adjacent to the guardsheet (150), without reducing the optical reflectivity of any part of the device. This…
In a method according to embodiments of the invention, a Ill-nitride layer is grown on a substrate. The substrate is RA03(MO)n, where R is selected from Sc, In, Y, and the lanthanides; A is selected from Fe (III), Ga, and A1; M is selected from Mg, Mn, Fe (II), Co, Cu, Zn and…
A light emitting device is produced by depositing a layer of wavelength converting material over the light emitting device, testing the device to determine the wavelength spectrum produced and correcting the wavelength converting member to produce the desired wavelength…
The structural characteristics of the light-exiting surface of a light emitting device ( 200 ) are controlled so as to increase the light extraction efficiency of that surface ( 225 ) when the surface is roughened. A light emitting surface ( 225 ) comprising layers of materials…
Methods and apparatus are described. An apparatus includes a hexagonal oxide substrate and a III-nitride semiconductor structure adjacent the hexagonal oxide substrate. The III-nitride semiconductor structure includes a light emitting layer between an n-type region and a p-type…
The current distribution across the p-layer ( 130 ) of a semiconductor device is modified by purposely inhibiting current flow through the p-layer ( 130 ) in regions ( 310 ) adjacent to the guardsheet ( 150 ), without reducing the optical reflectivity of any part of the device.…
In a method according to embodiments of the invention, a Ill-nitride layer is grown on a substrate. The substrate is RA0 3 (MO) n , where R is selected from Sc, In, Y, and the lanthanides; A is selected from Fe (III), Ga, and A1; M is selected from Mg, Mn, Fe (II), Co, Cu, Zn…
In a method according to embodiments of the invention, a III-nitride layer is grown on a growth substrate. The III-nitride layer is connected to a host substrate. The growth substrate is removed. The growth substrate is a non-III-nitride material. The growth substrate has an in-…
A device includes a substrate and a Ill-nitride structure grown on the substrate, the Ill-nitride structure comprising a light emitting layer disposed between an n-type region and a p-type region. The substrate is a RAO 3 (MO) n , where R is one of a trivalent cation, Sc, In, Y,…
The structural characteristics of the light-exiting surface of a light emitting device (200) are controlled so as to increase the light extraction efficiency of that surface (225) when the surface is roughened. A light emitting surface (225) comprising layers of materials with…