The invention concerns a new pre alloyed steel powder comprising in addition to iron and inevitable impurities, by wt %, 1.3-1.7% by weight of Cr, 0.15-0.3% by weight of Mo, 0.09-0.3% by weight of Mn, not larger than 0.01 by weight of C, not larger than 0.25% of O.
Engstrom Ulf
The present invention relates to a water-soluble cationic acrylamide-based polymer having one or more acetoacetate groups. The invention also relates to a method for producing the water-soluble polymer which comprises polymerizing ethylenically unsaturated monomers in an aqueous…
The invention concerns a new pre alloyed steel powder comprising in addition to iron and inevitable impurities, by wt %, 1.3-1.7% by weight of Cr, 0.15-0.3% by weight of Mo, 0.09-0.3% by weight of Mn, not larger than 0.01 by weight of C, not larger than 0.25% of O.
The present invention relates to a water-soluble cationic acrylamide-based polymer having one or more acetoacetate groups. The invention also relates to a method for producing the water-soluble polymer which comprises polymerizing ethylenically unsaturated monomers in an aqueous…
A novel carrier powder for electrophotographic develop- ens is provided. The carrier powder comprises spherical magnetite particles having a wustite (FeO) content of less than 10% by weight, a particle diameter of 30 - 200 µm and a surface porosity of less than 20%.
The present invention relates to an iron-base powder containing Ni, Mo and C for producing highly resistant sintered bodies under normal pressing and sintering conditions. The powder contains 7-12% by weight of Ni, 0.4-1.5% by weight of Mo, and 0.3-0.7% by weight of C.
The present invention relates to a water-soluble cationic acrylamide-based polymer having one or more acetoacetate groups. The invention also relates to a method for producing the water-soluble polymer which comprises polymerizing ethylenically unsaturated monomers in an aqueous…
A water-atomized iron-based powder is provided that is pre-alloyed with 0.75-1.1% by weight of Ni, 0.75-1.1% by weight of Mo and up to 0.45% by weight of Mn, and further including 0.5-3.0%, preferably 0.5-2.5% and most preferably 0.5-2.0% by weight of Cu, and inevitable…
Disclosed is a new diffusion-bonded powder consisting of an iron powder having 1-5%, preferably 1.5-4% and most preferabiy 1.5-3.5% by weight of copper particles diffusion bonded to the surfaces of the iron powder particles. The new diffusion bonded powder is suitable for…
Disclosed is a new diffusion-bonded powder consisting of an iron powder having 1-5%, preferably 1.5-4% and most preferably 1.5-3.5% by weight of copper particles diffusion bonded to the surfaces of the iron powder particles. The new diffusion bonded powder is suitable for…
A novel carrier material useful in conjunction with a toner for preparing a two-component developer for electrophotographic processes is provided. The carrier comprises a spherical magnetite particulate material having a reduced metallic iron outer layer which is coated with an…
An electrophotographic carrier material comprising a spherical core of hematite-containing magnetite and a resinous coating layer applied thereon is provided. The carrier material exhibits good copying characteristics, an improved durability and an enhanced stability to the…
A heat-insulating component consists of a porous body obtained by moulding and sintering an iron-base powder having an admixture of 2-10% by weight of silicon, preferably 4-8% by weight. A method of making the heat-insulating component includes the steps of preparing an…
Disclosed is a new diffusion-bonded powder consisting of an iron powder having 1-5%, preferably 1.5-4% and most preferably 1.5-3.5% by weight of copper particles diffusion bonded to the surfaces of the iron powder particles. The new diffusion bonded powder is suitable for…
A pre-alloyed brazing powder material consists of by weight about 3 to 15% iron, about 30 to 45% nickel, about 10 to 20% manganese, about 1 to 3% silicon, about 1 to 3% boron and the balance copper. The pre-alloyed brazing powder material can be mixed with up to 3% by weight of…
A kind of new difference bonded powder is disclosed, is made of iron powder, the iron powder has 1-5%, preferably 1.5-4%, most preferably the copper particle for being diffused and bonded to ferrous powder granules surface of 1.5-3.5% weight.The new difference bonded powder is…
Disclosed is a new diffusion-bonded powder consisting of an iron powder having 1-5%, preferably 1.5-4% and most preferably 1.5-3.5% by weight of copper particles diffusion bonded to the surfaces of the iron powder particles. The new diffusion bonded powder is suitable for…
The present invention concerns the preparation of a manganese sulphide by heating of particulate or agglomerate manganese sulphate to a temperature of at least 700 DEG C in the presence of at least one reduction agent.
The present invention concerns the preparation of a manganese sulphide by heating of particulate or agglomerate manganese sulphate to a temperature of at least 700 DEG C in the presence of at least one reduction agent.