WO 2008/155271 A1#1481707 Most Cited · 39 citations2.2/yr · PR 3.92PendingWO · Application
Method for the production of polyamides in extruders

The invention relates to a method for the production of a polyamide based on dicarboxylic acids and diamines, wherein a solid mixture is heated in an extruder, the mixture containing a monomer mixture of 50 mol-% of a dicarboxylic acid mixture of 60 to 88 wt.-% of terephthalic…

DE 102004049342 A1#1969608 Most Cited · 33 citations1.6/yr · PR 3.56PendingDE · Application
Fließfähige Thermoplaste mit halogenfreiem Flammschutz

Thermoplastic molding compositions, comprising A) from 10 to 98% by weight of at least one thermoplastic polymer, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate having an OH number of from 1 to 600 mg KOH/g of polycarbonate (to…

WO 2013/139827 A1#1977220 Most Cited · 33 citations2.5/yr · PR 3.10PendingWO · Application
Pale-coloured flame-retardant polyamides

The invention relates to thermoplastic moulding compounds which contain A) 10 to 98 wt.% of a thermoplastic polyamide, B) 0.1 to 60 wt.% of red phosphorus, C) 0.5 to 20 wt.% of a melamine compound, D) 1 to 30 wt.% of rutile-type titanium dioxide, E) 0 to 40 wt.% of an impact…

US 2004192812 A1#2145570 Most Cited · 31 citations1.4/yr · PR 5.04PendingUS · Application
Halogen-free flameproof polyester
Inventors: Engelmann Jochen, Wartig DetlevAssignee: Jochen Engelmann, Detlev WartigFiled 2002-07-26

The invention relates to thermoplastic moulding materials containing A) between 20 and 97 wt. % of a thermoplastic polyester; B) between 1 and 40 wt. % of a phosphinic acid salt and/or a diphosphinic acid salt and/or the polymers thereof, constituent B) having an average…

DE 102004050025 A1#3088172 Most Cited · 25 citations1.2/yr · PR 2.78PendingDE · Application
Fließfähige Thermoplaste mit Halogenflammschutz

Thermoplastische Formmassen, enthaltend DOLLAR A A) 10 bis 98 Gew.-% mindestens eines thermoplastischen Polymeren, DOLLAR A B) 0,01 bis 50 Gew.-% DOLLAR A B1) mindestens eines hoch- oder hyperverzweigten Polycarbonates mit einer OH-Zahl von 1 bis 600 mg KOH/g Polycarbonat (gemäß…

US 2008262133 A1#3154532 Most Cited · 24 citations1.3/yr · PR 5.98PendingUS · Application
Thermal Aging-Resistant Polyamides

Thermoplastic molding compositions comprising A) from 10 to 99% by weight of at least one thermoplastic polyamide, B) from 0.1 to 5% by weight of at least one polyethyleneimine homo- or copolymer, C) from 0.05 to 3% by weight of a lubricant, D) from 0.05 to 3% by weight of a…

US 2008015303 A1#3604607 Most Cited · 22 citations1.2/yr · PR 5.01PendingUS · Application
Flowable Polyamides With Hyperbranched Polyesters/Polycarbonates

Thermoplastic molding compositions, comprising A) from 10 to 99% by weight of at least one thermoplastic polyamide, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate with an OH number of from 1 to 600 mg KOH/g of polycarbonate (to…

US 2008194741 A1#4286055 Most Cited · 20 citations1.1/yr · PR 2.81PendingUS · Application
Flowable Thermoplastic Materials With Halogen-Free Flame Protection

Thermoplastic molding compositions, comprising A) from 10 to 98% by weight of at least one thermoplastic polymer, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate having an OH number of from 1 to 600 mg KOH/g of polycarbonate (to…

WO 2004/069912 A1#5370196 Most Cited · 17 citations0.8/yr · PR 2.71PendingWO · Application
Hydrolysis-resistant polyesters

The invention relates to the use of epoxidised natural oils or fatty acid esters or the mixtures thereof (constituents B) for producing hydrolysis-resistant thermoplastic polyester moulding materials (A).

WO 2008/022910 A1#5234967 Most Cited · 17 citations0.9/yr · PR 3.58PendingWO · Application
Polyamide molding materials with improved thermal aging and hydrolysis stability

Thermoplastic molding materials comprising: (A) 20 - 85% by weight of at least one polyamide having a number of amino end groups of 50 mmol/kg, (B) 14.9 - 60% by weight of glass fibers, (C) 0.01 - 2% by weight of at least one heat stabilizer, (D) 0 - 1.5% by weight of at least…

US 2011224346 A1#5603986 Most Cited · 16 citations1.1/yr · PR 4.20PendingUS · Application
Polyamide molding materials with improved thermal aging and hydrolysis stability
Inventors: Eibeck Peter, Engelmann Jochen, Neuhaus Ralf, Bernnat AnkaAssignee: Basf SeFiled 2007-08-07

Thermoplastic molding compositions, comprising: (A) from 20 to 85% by weight of at least one polyamide whose number of amino end groups is ≧50 mmol/kg, (B) from 14.9 to 60% by weight of glass fibers. (C) from 0.01 to 2% by weight of at least one heat stabilizer, (D) from 0 to…

US 2010190952 A1#6105724 Most Cited · 15 citations0.9/yr · PR 3.93PendingUS · Application
Method for the production of polyamides in extruders

In a process for preparing a polyamide based on dicarboxylic acids and diamines in an extruder, a solid mixture comprising a monomer mixture composed of 50 mol % of dicarboxylic acid mixture composed of from 60 to 88 % by weight of terephthalic acid and from 12 to 40% by weight…

US 2013023613 A1#6821508 Most Cited · 14 citations1.1/yr · PR 2.88PendingUS · Application
Use of polyamides that are resistant to corrosion and stress cracking

The use of thermoplastic molding materials comprising A) 10 to 98.8% by weight of a mixture formed from a1) 40 to 70% by weight of nylon-6,6 or nylon-4,6 or nylon-6 or mixtures thereof, a2) 30 to 60% by weight of a polyamide having a ratio of methylene to amide groups of 7 to…

WO 2006/042705 A1#7560419 Most Cited · 13 citations0.7/yr · PR 2.56PendingWO · Application
Flowable polyamides comprising hyperbranched polyesters/polycarbonates

Disclosed are thermoplastic molding materials containing A) 10 to 99 percent by weight of at least one thermoplastic polyamide, B) 0.01 to 50 percent by weight of B1) at least one highly branched or hyperbranched polycarbonate having a hydroxyl number ranging between 1 and 600…

US 2010311882 A1#8476491 Most Cited · 12 citations0.8/yr · PR 2.19PendingUS · Application
Thermally conductive polyamides
Inventors: Eibeck Peter, Engelmann Jochen, Neuhaus Ralf, Klaus UskeAssignee: Basf SeFiled 2007-03-22

Thermoplastic molding compisitions, comprising A) from 19.9% to 59.9% by weight of thermoplastic polyamide B) from 40 to 80% by weight of an aluminum oxide or magnesium oxide or a mixture of these C) from 0.1 to 2% by weight of nigrosin D) from 0 to 20% by weight of other…

DE 10,137,930 A1#9109774 Most Cited · 11 citations0.5/yr · PR 2.62PendingDE · Application
Thermoplastic molding composition e.g. for fibers and films, comprises thermoplastic polyester, a (di)phosphinic acid salt, fire retardant and ester or amide
Inventors: Engelmann Jochen, Wartig DetlevAssignee: Basf AgFiled 2001-08-07

Thermoplastic molding composition comprises (wt.%): (A) thermoplastic polyester (20-97); (B) phosphinic acid and/or diphosphinic acid salt (1-40), with mean particle size (d50-value) of less than 10 micro m; (C) nitrogen containing fire protection agent (1-30); (D) at least one…

US 2007257240 A1#9679657 Most Cited · 11 citations0.6/yr · PR 1.57PendingUS · Application
Flowable Thermoplastics with Halogen Flame Retardancy System

Thermoplastic molding compositions, comprising A) from 10 to 98% by weight of at least one thermoplastic polymer, B) from 0.01 to 50% by weight of B1) at least one highly branched or hyperbranched polycarbonate with an OH number of from 1 to 600 mg KOH/g of polycarbonate (to DIN…

US 7,169,838 B2#9999205 Most Cited · 10 citations0.5/yr · PR 2.86ExpiredUS · Utility
Halogen-free flameproof polyester
Inventors: Engelmann Jochen, Wartig DetlevAssignee: Basf AgFiled 2002-07-26 · Granted 2007-01-30

The invention relates to thermoplastic moulding materials containing A) between 20 and 97 wt. % of a thermoplastic polyester; B) between 1 and 40 wt. % of a phosphinic acid salt and/or a diphosphinic acid salt and/or the polymers thereof, constituent B) having an average…

WO 2006/040066 A1#10001334 Most Cited · 10 citations0.5/yr · PR 2.86PendingWO · Application
Flowable thermoplastic materials with halogen-free flame protection

The invention relates to thermoplastic moulded masses containing A) between 10 and 98 wt. % of at least one thermoplastic polymer, B) between 0.01 and 50 wt. % of B1) at least one highly branched or hyperbranched polycarbonate with an OH-number of between 1 and 600 mg KOH/g of…

WO 03,014,212 A1#10989192 Most Cited · 9 citations0.4/yr · PR 4.26PendingWO · Application
Halogen-free flameproof polyester
Inventors: Engelmann Jochen, Wartig DetlevAssignee: Basf Ag, Engelmann JochenFiled 2002-07-26

The invention relates to thermoplastic moulding materials containing A) between 20 and 97 wt. % of a thermoplastic polyester; B) between 1 and 40 wt. % of a phosphinic acid salt and/or a diphosphinic acid salt and/or the polymers thereof, constituent B) having an average…

CN 102,834,463 A#13087012 Most Cited · 8 citations0.6/yr · PR 2.04ActiveCN · Utility
Use of polyamides that are resistant to corrosion and stress cracking

The invention relates to the use of thermoplastic molding compounds containing A) 10 to 98.8 wt.% of a mixture made of a1) 40 to 70 wt.% polyamide 6.6 or polyamide 4.6 or polyamide 6 or mixtures thereof, a2) 30 to 60 wt.% of a polyamide with a ratio of methyl groups to amide…

WO 2006/084862 A1#13954584 Most Cited · 8 citations0.4/yr · PR 1.42PendingWO · Application
Heat aging-resistant polyamides

Disclosed are thermoplastic molding materials containing: A) 10 to 99 percent by weight of at least one thermoplastic polyamide; B) 0.1 to 5 percent by weight of at least one polyethyleneimine homopolymer or copolymer; C) 0.05 to 3 percent by weight of a lubricant; D) 0.05 to 3…

WO 2007/113116 A1#12825099 Most Cited · 8 citations0.4/yr · PR 2.30PendingWO · Application
Thermally conductive polyamides

Thermoplastic moulding materials comprising A) from 19.9 to 59.9% by weight of a thermoplastic polyamide, B) from 40 to 80% by weight of an aluminium oxide or magnesium oxide or mixtures thereof, C) from 0.1 to 2% by weight of nigrosine, D) from 0 to 20% by weight of further…

WO 2011/120949 A1#12802059 Most Cited · 8 citations0.5/yr · PR 2.33PendingWO · Application
Use of polyamides that are resistant to corrosion and stress cracking

The invention relates to the use of thermoplastic molding compounds containing A) 10 to 98.8 wt.% of a mixture made of a1) 40 to 70 wt.% polyamide 6.6 or polyamide 4.6 or polyamide 6 or mixtures thereof, a2) 30 to 60 wt.% of a polyamide with a ratio of methyl groups to amide…