The marking of absorbent material, in particular of ceramic piece goods, should be readable immediately and also after a thermal treatment at temperatures above 400 DEG C. The marking of absorbent material is carried out by applying a cobalt salt solution which can additionally…
Duismann Werner
2.1 The labelling of absorbent material, in particular individual pieces made from ceramic, should be immediately readily legible and should still be legible after thermal treatment at temperatures above 400 DEG C. <??>2.2 Absorbent material is labelled by applying a…
A process is provided for applying a thermostable identification mark to an absorbent material such as piece goods or ceramics. A cobalt salt solution containing hydrogen peroxide is applied in the form of a mark to the surface of an absorbent material, followed by a thermal…
Cpds. of formula: (where R1, R2 and R3 are 1-12C aliphatic, cycloaliphatic or araliphatic residues; R1 and R2 together with the C atom can constitute a cycloaliphatic ring) are prepd. in high yield by reacting cpds. for formula (I; R3 = Cl) with Al(R3)3.
Cpds. of formula (I) = R1R2R3C-N=N-CR3R2R1 (where R1, R2 and R3 are 1-12C aliphatic, cycloaliphatic or araliphatic gps.; R3 can also be an aromatic gp., and CR1R2 can also be a cycloaliphatic gp.) are prepd. by reacting R1R2C(Cl)-N=N-(Cl)CR1R2 with Al(R3)3. Cpds. (I) are useful…
Die Kennzeichnung von saugfähigem Material, insbesondere von Stückgütern aus Keramik, soll sofort und auch noch nach einer thermischen Behandlung bei Temperaturen oberhalb von 400 °C lesbar sein. Die Kennzeichnung von saugfähigem Material erfolgt durch Aufbrin gen einer…