A method of producing low-viscosity water-based water-soluble polymer dispersions having a high concentration of the principal substance is achieved by polymerizing the following monomer components, (a1) 50-99.999 wt. % of at least one water-soluble monomer; (a2) 0.001-1 wt. %…
Desch Wolfram
Prepn. of a low viscosity, water-soluble polymer dispersion (PD) with a high actives content and an aq. basis and with the polymer having average mol.wt. Mw at least 500000 is by polymerisation of the following monomers (a1)-(a4) (100 wt.% total) in an aq. soln. in presence of a…
The invention relates to a method for coating a surface. According to said method, a coating substance having a viscosity of <100 Pa.s, measured at 25° C., is applied to a surface to be coated and left to harden. The inventive method is characterised in that, during the…
Prepn. of low viscosity water-soluble polymer dispersion comprises mixing a monomer component in aq. soln. with at least one polymeric dispersing agent. The monomer component comprises: (a1) 50-99.99 wt.% of at least one water-soluble monomer; (a2) 0.01-5 wt.% of a…
Prepn. of a low viscosity, water-soluble polymer dispersion (PD) with a high actives content and an aq. basis and with the polymer having average mol.wt. Mw at least 500000 is by polymerisation of the following monomers (a1)-(a4) (100 wt.% total) in an aq. soln. in presence of a…
The prodn. of low-viscosity aq. dispersions (PD') of water-soluble polymer with a mean mol. wt. of at least 500000 (A) and with a high concn. of active substance, comprises the polymerisation of (a1) 80-100 wt.% water-soluble monomer(s) and opt. (a2) 0-20 wt.% amphiphilic…
Low-viscosity, water-soluble polymeric aqueous dispersions with high active substance concentrations containing a polymer (A), made up of water-soluble monomers (a1) and, optionally, amphoteric monomers (a2), as well as a polymeric dispersion agent (D) may be prepared by…
A method of producing low-viscosity water-based water-soluble polymer dispersions having a high concentration of the principal substance is achieved by polymerizing the following monomer components, (a1) 50-99.999 wt.% of at least one water-soluble monomer; (a2) 0.001-1 wt.% of…
The invention relates to a method for coating a surface. According to said method, a coating substance having a viscosity of < 100 Pa.s, measured at 25 DEG C, is applied to a surface to be coated and left to harden. The inventive method is characterised in that, during the…
The prodn. of low-viscosity aq. dispersions (PD') of water-soluble polymer with a mean mol. wt. of at least 500000 (A) and with a high concn. of active substance, comprises the polymerisation of (a1) 80-100 wt.% water-soluble monomer(s) and opt. (a2) 0-20 wt.% amphiphilic…
Low-viscosity, water-soluble polymeric aqueous dispersions with high active substance concentrations containing a polymer (A), made up of water-soluble monomers (a1) and, optionally, amphoteric monomers (a2), as well as a polymeric dispersion agent (D) may be prepared by…
The prodn. of low-viscosity aq. dispersions (PD') of water-soluble polymer with a mean mol. wt. of at least 500000 (A) and with a high concn. of active substance, comprises the polymerisation of (a1) 80-100 wt.% water-soluble monomer(s) and opt. (a2) 0-20 wt.% amphiphilic…
Prepn. of low viscosity water-soluble polymer dispersion comprises mixing a monomer component in aq. soln. with at least one polymeric dispersing agent. The monomer component comprises: (a1) 50-99.99 wt.% of at least one water-soluble monomer; (a2) 0.01-5 wt.% of a…
The invention relates to a method for coating a surface. According to said method, a coating substance having a viscosity of < 100 Pa.s, measured at 25 DEG C, is applied to a surface to be coated and left to harden. The inventive method is characterised in that, during the…
Prepn. of a low viscosity, water-soluble polymer dispersion (PD) with a high actives content and an aq. basis and with the polymer having average mol.wt. Mw at least 500000 is by polymerisation of the following monomers (a1)-(a4) (100 wt.% total) in an aq. soln. in presence of a…
Prepn. of low viscosity water-soluble polymer dispersion comprises mixing a monomer component in aq. soln. with at least one polymeric dispersing agent. The monomer component comprises: (a1) 50-99.99 wt.% of at least one water-soluble monomer; (a2) 0.01-5 wt.% of a…
The invention relates to a method for coating a surface. According to said method, a coating substance having a viscosity of <100 Pa.s, measured at 25° C., is applied to a surface to be coated and left to harden. The inventive method is characterised in that, during the…
The invention relates to a method for coating a surface. According to said method, a coating substance having a viscosity of <100 Pa.s, measured at 25° C., is applied to a surface to be coated and left to harden. The inventive method is characterised in that, during the…
The invention relates to a method for coating a surface. According to said method, a coating substance having a viscosity of < 100 Pa.s, measured at 25 ~C, is applied to a surface to be coated and left to harden. The inventive method is characterised in that, during the…
The invention relates to a method for coating a surface. According to said method, a coating substance having a viscosity of <100 Pa.s, measured at 25° C., is applied to a surface to be coated and left to harden. The inventive method is characterised in that, during the…
The prodn. of low-viscosity aq. dispersions (PD') of water-soluble polymer with a mean mol. wt. of at least 500000 (A) and with a high concn. of active substance, comprises the polymerisation of (a1) 80-100 wt.% water-soluble monomer(s) and opt. (a2) 0-20 wt.% amphiphilic…
Prepn. of a low viscosity, water-soluble polymer dispersion (PD) with a high actives content and an aq. basis and with the polymer having average mol.wt. Mw at least 500000 is by polymerisation of the following monomers (a1)-(a4) (100 wt.% total) in an aq. soln. in presence of a…
Prepn. of low viscosity water-soluble polymer dispersion comprises mixing a monomer component in aq. soln. with at least one polymeric dispersing agent. The monomer component comprises: (a1) 50-99.99 wt.% of at least one water-soluble monomer; (a2) 0.01-5 wt.% of a…
The prodn. of low-viscosity aq. dispersions (PD') of water-soluble polymer with a mean mol. wt. of at least 500000 (A) and with a high concn. of active substance, comprises the polymerisation of (a1) 80-100 wt.% water-soluble monomer(s) and opt. (a2) 0-20 wt.% amphiphilic…
Prepn. of low viscosity water-soluble polymer dispersion comprises mixing a monomer component in aq. soln. with at least one polymeric dispersing agent. The monomer component comprises: (a1) 50-99.99 wt.% of at least one water-soluble monomer; (a2) 0.01-5 wt.% of a…