FIELD: artificial diamonds. SUBSTANCE: in a method, in which graphite-fullerene-catalyst mixture is subjected to pressure and temperature in the diamond stability range, followed by ageing under synthesis conditions, novelty consists in using fullerene concentrations from 0.01…
Davidenko V M
FIELD: production of abrasive materials and tools. SUBSTANCE: method includes mixing of hexagonal boron nitride, magnesium and hydrazine chloride in the amount of 38-63 wt.% of the mixture; placement into high-pressure chamber; treatment with high pressure and temperature for…
FIELD: abrasives. SUBSTANCE: charge containing 1-4% diamond or cubic boron nitride, graphite or hexagonal boron nitride, and catalyst is placed into high-pressure "anvil-with-socket"-type apparatus and exposed to temperature and pressure with diamond or cubic boron…
Cubic boron nitride is produced by subjecting a charge of hexagonal boron nitride and an alkali(ne earth) metal and/or if boride as initiator to a pressure of 40-70 Kilobars and a temp. of 1100-2000 deg. C. The yield and crystal size of the prod. are increased if a crystalline…
Cubic BN is made from a mixture containing hexagonal BN, and, as initiators, one or more borides nitrides, silicides, or germanides of transition metals of Groups IV, V, VI, and VIII at pressure >55 kilobars at above 1500 degrees C. There may be 40-2% initiators and the…
FIELD: inorganic synthesis. SUBSTANCE: invention relates to manufacture of abrasive and blade tools. Hexagonal boron nitride is supplemented by cubic boron nitride and catalyst to form initial blend. In another embodiment, blend is prepared from hexagonal boron nitride, boron,…
Initiator consisting of alkali(ne earth) metal boride, pref. Mg- or Be boride, promotes conversion of hexagonal to cubic BN above 1000 degrees C and 40 kbar press. B content of initiator, calc. as elemental B, is such as to raise total B content of reaction mixt. by >=10%…