A preparation method of a photonic crystal optical fiber preform comprises the following steps: preparing a capillary tube with two sealed ends, an outer sleeve glass tube with one sealed end and a core forming glass rod; placing the cored glass rod into the outer sleeve glass…
Da Ning
An electronic device structure and an ultra-thin glass sheet used therein. The electronic device structure includes a functional device and an ultra-thin glass above the functional device. The ultra-thin glass has a thickness of no more than 0.4 mm and also has a toughening…
The present disclosure relates to a protective cover including at least one transparent inorganic layer and at least one transparent adhesion layer. The transparent inorganic layer may include glass or glass ceramic. In a preferred embodiment, the inorganic layer is glass or…
A thin chemically toughenable or toughened lithium containing aluminosilicate glass with low expansion after chemical toughening. A method for producing as well as to uses of the glass. The glass is used in applications in the field of high precision equipment, electronic…
A method for producing an ultrathin chemically toughened glass article comprises providing an ultrathin glass sheet with a first surface and a second surface joined by at least one edge, having a thickness between the first and the second surface, chemically toughening the…
It relates to an ultrathin chemically toughened and subsequently etched glass article (1) having a thickness or less than or equal to 0.4mm. In order to improve the impact resistance the glass article (1) has a breakage height (given in mm) of more than 200 multiplied by the…
The invention provides a pair of human body kinetic energy power supply intelligent shoes based on piezoelectric material. The pair of human body kinetic energy power supply intelligent shoes based on the piezoelectric material comprises shoe bodies, and is characterized in that…
A shaped glass article is provided that is ultrathin, has two surfaces and one or more edges joining the two surfaces, and a thickness between the two surfaces. The shaped ultrathin glass article has at least one curved area with a non-vanishing surface curvature with a minimal…
It relates to a chemically toughened glass article (1) having a thickness (t) of equal to or less than 0.4 mm, a first surface (2), a second surface (3) and a compressive stress region being defined by a compressive stress (CS) of at least 100 MPa, and at least one edge (4)…
A method for producing an ultrathin chemically toughened glass article is provided that includes: providing an ultrathin glass sheet with a first surface and a second surface joined by at least one edge, having a thickness between the first and the second surface, chemically…
A shaped glass article and a method for producing it are provided. The article is ultrathin and has two surfaces and one or more edges joining the two surfaces, and a thickness between the two surfaces. The article has at least one curved area with a non-vanishing surface…
The invention relates to a lithium-containing aluminosilicate thin glass which can be chemically tempered or chemically tempered and which has a low expansion after chemical tempering. The invention also relates to a method for producing the glass according to the invention and…
The coal base hot-air bottom-rotating furnace melt-reduction iron-smelting method for producing bead iron includes the following steps: using iron ore powder, coal powder, flux and adhesive to pelletize, in the coal base hot-air bottom-rotating furnace make the above-mentioned…
The invention relates to a chemically tempered glass product (1) comprising: a thickness (t) equal to or less than 0.4 mm; a first surface (2) and a second surface (3); a compressive stress region defined by a Compressive Stress (CS) of at least 100 MPa; at least one edge (4)…
The invention relates to an ultra-thin chemically tempered and subsequently etched glass article (1) having a thickness of less than or equal to 0.4 mm. In order to improve the impact resistance, the glass article (1) has a fracture height (in mm) greater than 200 times the…
A glass ribbon in the form of a glass roll is provided that is optimized with respect to the requirements of a long service life and at the same time compact dimensions. A bending radius on the inner side of the thin glass roll is determined by performing breakage tests on…
A chemically toughenable or toughened glass has, before chemical toughening, a thickness t of at most 1100 μm. The glass comprises the following components: 45-75 mol-% SiO 2 ; 10-25 mol-% Al 2 O 3 ; >1-11 mol-% Li 2 O; 0-15 mol-% P 2 O 5 ; 0-8 mol-% B 2 O 3 ; and 0-5 mol-%…
A method for producing an ultrathin chemically toughened glass article, comprising providing an ultrathin glass sheet with a first surface and a second surface joined by at least one edge, having a thickness between the first and the second surface, chemically toughening the…
A kind of method for producing ultra-thin chemically toughened glass product, it includes providing with the first surface connected by least one edge and the ultra-thin glass piece of second surface, the ultra-thin chemically toughened glass product has the thickness between…
An ultrathin chemically toughened and subsequently etched glass article is provided. The article has a thickness of less than or equal to 0.4 mm and a breakage height (given in mm) of more than 200 multiplied by the thickness (t given in mm)). Further, the article has a breakage…
A chemically toughened glass article is provided that has a thickness (t) of equal to or less than 0.4 mm, a first surface, a second surface, and a compressive stress region that is defined by a compressive stress (CS) of at least 100 MPa and at least one edge connecting the…
PROBLEM TO BE SOLVED: To provide: an electronic device structure which improves the functionality of a device, reduces the thickness of the whole device, and improves the reliability of the device; and an ultra-thin glass sheet used therein.SOLUTION: An electronic device…
The invention relates to the technical field of software engineering, in particular relating to a requirement priority ordering method and system based on dependence reduction. The method comprises the following steps: analyzing an incidence relation among requirement items to…
An ultrathin glass-ceramic article is provided having an article thickness (t) of equal to or less than 0.3 mm and an outer surface followed towards the inside of the article by an outer layer and a central part. The glass-ceramic has a crystal phase and an amorphous phase and…
An active large-core-diameter single-mode double-clad photonic crystal fiber comprises a signal core, an inner cladding, an outer cladding and a protective layer, and is characterized in that the signal core is a fiber core part doped with active ions, the inner cladding…