Patents
Inventor / Author Profile

Classen Bruno

76Total Forward Citations
17Indexed Patents
4Patent H-Index
Frequent Co-Inventors: Colombet Pierre Le Rolland Bruno
US 6,695,910 B2#3136688 Most Cited · 24 citations1.1/yr · PR 7.61ExpiredUS · Utility
Sulfoaluminous clinker without iron and without free lime, its process of preparation and its use in white binders
Inventors: Classen Bruno, Colombet PierreAssignee: Francais CimentsFiled 2002-10-24 · Granted 2004-02-24

The lightly colored sulfoaluminous clinker contains: more than 55% by weight of calcium sulfoaluminate phase (C4A3S), more than 10% by weight of belite phase (C2S), less than 10% by weight of anhydrite (C{overscore (S), and contains practically no ferrite phase, nor a gehlenite…

EP 1,306,356 A1#4218481 Most Cited · 20 citations0.9/yr · PR 3.47PendingEP · Application
Ironless sulfoaluminous clinker containing no free lime, method for its production and its use in white binders
Inventors: Classen Bruno, Colombet PierreAssignee: Francais CimentsFiled 2002-10-15

A sulfo-aluminous clinker contains: <??>(a) more than 55 % by wt of calcium sulfo-aluminate phase (C4A3S'); <??>(b) more than 10 % by wt of belite phase (C2S); <??>(c) less than 10 % by wt of anhydrite (CS'); <??>(d) containing practically no…

US 6,419,738 B1#6076361 Most Cited · 15 citations0.6/yr · PR 4.34ExpiredUS · Utility
Process for rendering waste inert by cladding in a hydraulic binder and pre-mix for practicing this process
Inventors: Classen Bruno, Le Rolland Bruno, Colombet PierreAssignee: Francais CimentsFiled 2000-07-31 · Granted 2002-07-16

Waste is rendered inert, by cladding the waste in a cement base hydraulic binder including sulfoaluminate cement comprised by at least 30% by weight of the phase 3CaO.3Al 2 O 3 .CaSO 4 (C 4 A 3 S). The hydraulic binder can be either essentially constituted by sulfoaluminate…

US 2003183131 A1#10585933 Most Cited · 10 citations0.4/yr · PR 1.94PendingUS · Application
Sulfoaluminous clinker without iron and without free lime, its process of preparation and its use in white binders
Inventors: Classen Bruno, Colombet PierreAssignee: Bruno Classen, Pierre ColombetFiled 2002-10-24

The lightly colored sulfoaluminous clinker contains: more than 55% by weight of calcium sulfoaluminate phase (C 4 A 3 S) more than 10% by weight of belite phase (C 2 S) less than 10% by weight of anhydrite (CS ) and contains practically no ferrite phase, nor a gehlenite phase (C…

FR 2,796,934 A1#24848895 Most Cited · 4 citations0.2/yr · PR 1.37PendingFR · Application
Procede d'inertage de dechets par enrobage dans un liant hydraulique et premix pour la mise en oeuvre de ce procede
Inventors: Classen Bruno, Le Rolland Bruno, Colombet PierreAssignee: Francais CimentsFiled 1999-07-30

La présente invention concerne un procédé d'inertage de déchets par enrobage desdits déchets dans un liant hydraulique, à base de ciment, le liant hydraulique d'inertage comprenant du ciment sulfoalumineux composé d'au moins 30 % en poids de la phase 3CaO. 3Al2 O3 .…

FR 2,831,161 A1#45895154 Most Cited · 1 citations0.0/yr · PR 1.44PendingFR · Application
Sulfo-aluminous clinker for the preparation of white binders in association with Portland cement and calcium sulfate, that is essential iron and lime free
Inventors: Classen Bruno, Colombet PierreAssignee: Francais CimentsFiled 2001-10-24

A sulfo-aluminous clinker contains: (a) more than 55 % by wt of calcium sulfo-aluminate phase (C4A3S'); (b) more than 10 % by wt of belite phase (C2S); (c) less than 10 % by wt of anhydrite (CS'); (d) containing practically no ferrite phase, nor any gehlenite phase…

CA 2,314,820 A1#105163629 Most Cited · 0 citations0.0/yr · PR 0.56PendingCA · Application
Process for rendering waste inert by coating it with a hydraulic binder and premix for implementing this process
Inventors: Classen Bruno, Colombet Pierre, Le Rolland BrunoAssignee: Francais CimentsFiled 2000-07-05

The invention concerns a process for inerting waste by coating it with a cement-based hydraulic binder, the inerting hydraulic binder comprising sulfoaluminate cement including at least 30% by weight of the phase 3CaO.3Al2O3.CaSO4(C4A3S). The hydraulic binder can be essentially…

CA 2,314,820 C#104225008 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Process for rendering waste inert by coating it with a hydraulic binder and premix for implementing this process
Inventors: Colombet Pierre, Le Rolland Bruno, Classen BrunoAssignee: Francais CimentsFiled 2000-07-05 · Granted 2007-05-08

The invention concerns a process for inerting waste by coating it with a cement-based hydraulic binder, the inerting hydraulic binder comprising sulfoaluminate cement including at least 30% by weight of the phase 3CaO.3Al2O3.CaSO4(C4A3S). The hydraulic binder can be essentially…

CA 2,409,252 C#140479838 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCA · Utility
Sulphoaluminous clinker without iron or free lime, preparation process of same, and use of same for colorless binders
Inventors: Classen Bruno, Colombet PierreAssignee: Francais CimentsFiled 2002-10-21 · Granted 2007-10-02

Le clinker sulfoalumineux faiblement coloré renferme - plus de 55 % en poids de phase sulfoaluminate de calcium (C4A3 S~) - plus de 10 % en poids de phase bélite (C2S) - moins de 10 % en poids d'anhydrite (C S~) et ne renferme pratiquement pas de phase ferrite, ni de phase…

EP 1,072,567 A1#149466883 Most Cited · 0 citations0.0/yr · PR 0.56PendingEP · Application
Method for rendering inert waste materials by encapsulation in an hydraulic binder and premix for carrying out this method
Inventors: Classen Bruno, Le Rolland BrunoAssignee: Francais CimentsFiled 2000-07-19

Cement-based hydraulic binder (25-100 parts) used to encapsulate municipal waste incineration residues (100 parts) comprises a sulfo-aluminous cement containing 30 weight % or more of the phase 3CaO.3Al2O3.CaSO4(C4A3S), and, optionally, a filler based on one or more zeolites. At…

ES 2,184,685 T3#64686866 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredES · Utility
Procedimiento de inactivacion de desechos mediante encapsulado en un ligante hidraulico y premezcla para la realizacion de este procedimiento.
Inventors: Classen Bruno, Le Rolland Bruno, Colombet PierreAssignee: Francais CimentsFiled 2000-07-19 · Granted 2003-04-16

Procedimiento de inactivación de desechos por encapsulado de los indicados desechos en un ligante hidráulico, a base de cemento, caracterizado porque el ligante hidráulico de inactivación comprende cemento sulfoaluminoso compuesto por al menos un 30 % en peso de la fase…

ES 2,341,846 T3#117101353 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredES · Utility
Clinker sulfoaluminoso sin hierro y sin cal libre, su procedimiento depreparacion y su utilizacion en aglomerantes blancos.
Inventors: Classen Bruno, Colombet PierreAssignee: Francais CimentsFiled 2002-10-15 · Granted 2010-06-29

Clinker sulfoaluminoso que contiene: - más de 55% en peso de fase sulfoaluminato de calcio (C4A3S), - de 10% a 20% en peso de fase belita (C2S), - menos de 10% en peso de anhidrita (C\S), - menos de 5% en peso de fase gelenita (C2AS), una cantidad de cal libre inferior a 0,2% en…