<P>PROBLEM TO BE SOLVED: To provide an inexpensive adsorbent material having excellent mechanical strength, little load on the environment and capable of improving adsorption performances in water and directly using an adsorption column, regeneration equipment etc., for…
Cho Ryu
<P>PROBLEM TO BE SOLVED: To provide a method for efficiently treating hexavalent chromium-containing liquid, and a reduction adsorbent of hexavalent chromium. <P>SOLUTION: A particulate adsorbent where a graft chain is introduced into a particulate substrate…
PROBLEM TO BE SOLVED: To provide a noble metal absorbent capable of selectively adsorbing a noble metal at low material cost and a low cost for production process, and to provide a method for adsorbing selectively adsorbing only the noble metals such as gold and platinum using…
<P>PROBLEM TO BE SOLVED: To provide an anion exchanger having sufficient ion exchange quantity and a high adsorption rate. <P>SOLUTION: This method for producing the anion exchanger includes a process for irradiating a polymer base material, which comprises a…
<P>PROBLEM TO BE SOLVED: To provide a granular anion exchanger having sufficient ion exchange quantity, mechanical strength and chemical stability, and exhibiting a high adsorption rate of ionic species. <P>SOLUTION: In this granular anion exchanger, a substituent…
PROBLEM TO BE SOLVED: To provide an adsorbent capable of obtaining the adsorbing ability of noble metals, method for producing the same, and a method for recovering the noble metals.SOLUTION: An adsorbent has a granular base material and a graft chain introduced into the base…
The present application relates to a display device. The display device includes: a substrate; and pad terminals arranged on the substrate in a first direction in the pad region, and including a first pad terminal provided at an outer side and an i-th pad terminal provided at an…
A stone-grinding wheel is manufactured by mixing homogeneously 25-35 wt.% magnesium oxide, 20-28 wt.% magnesium chloride or sulfate, 40-50 wt.% water, adding 1-10 wt.% silundum or titanium oxide, and hardening at room temperature for 5-9 days.