The blends comprise (a) thermoplastic polyurethane having a Shore hardness of from 60 A to 50 D and (b) ethylene-propylene (EPM) rubbers and/or modified ethylene-propylene (EPM) rubbers, where the weight ratio of (a):(b) is from 3:1 to 999:1.
Chlosta Andreas
PROBLEM TO BE SOLVED: To obtain the subject polyurethane excellent in reactivity and mechanical characteristics, by reacting an isocyanate with a polyol containing a polyether polyalcohol having a specific structural unit, molecular weight and degree of unsaturation. SOLUTION:…
A process for the production of thermoplastic polyurethanes (TPU) comprises reacting (a) isocyanates with (b) compounds with a molecular weight of 500-10000 which react with isocyanates, optionally in the presence of (c) chain extenders with a molecular weight of less than 500,…
Polyurethane (PU) elastomers (I) contg. bis (methoxyethoxyethyl) phthalate (II) are used as plasticisers. (I) is prepd. by reacting (A) organic polyisocyanates with (B) polyhydroxy cpds. of mol.wt. 500-8,000 and (C) chain lengthening and/or crosslinking agents of mol.wt. 60-400,…
Use is claimed of 24-34C fatty acids (and/or their amides and/or esters) in the production of polyisocyanate-polyaddition products with reduced tendency to absorb and/or desorb substances, the production comprising reacting (a) a polyisocyanate with (b) an NCO-reactive compound…
The blends comprise(a) thermoplastic polyurethane having a Shore hardness of from 60 A to 50 D and(b) ethylene-propylene (EPM) rubbers and/or modified ethylene-propylene (EPM) rubbers,where the weight ratio of (a):(b) is from 3:1 to 999:1.
PROBLEM TO BE SOLVED: To obtain an excellent abrasion resistance by compounding, at a specific wt. ratio, a thermoplastic polyurethane having a specific Shore hardness as well as an ethylene/propylene rubber, a modified ethylene/propylene rubber or a mixture thereof. SOLUTION:…
Blend with a Shore Hardness of 60 A to 54 D contains (a) thermoplastic polyurethane (TPU) with a Shore hardness of 60 A to 50 D and (b) ethylene-propylene rubber (EPM) and/or modified EPM in an (a):(b) weight ratio of (3-999):1.
The blends comprise(a) thermoplastic polyurethane having a Shore hardness of from 60 A to 50 D and(b) ethylene-propylene (EPM) rubbers and/or modified ethylene-propylene (EPM) rubbers,where the weight ratio of (a):(b) is from 3:1 to 999:1.
The blends comprise (a) thermoplastic polyurethane having a Shore hardness of from 60 A to 50 D and (b) ethylene-propylene (EPM) rubbers and/or modified ethylene-propylene (EPM) rubbers, where the weight ratio of (a):(b) is from 3:1 to 999:1.
In a process for preparing thermoplastic polyurethanes by reacting (a) isocyanates with (b) compounds reactive toward isocyanates and having a molecular weight of from 500 to 10,000 g/mol, in the presence or absence of (c) chain extenders having a molecular weight of less than…
The blends comprise(a) thermoplastic polyurethane having a Shore hardness of from 60 A to 50 D and(b) ethylene-propylene (EPM) rubbers and/or modified ethylene-propylene (EPM) rubbers,where the weight ratio of (a):(b) is from 3:1 to 999:1.
The blends comprise (a) thermoplastic polyurethane having a Shore hardness of from 60 A to 50 D and (b) ethylene-propylene (EPM) rubbers and/or modified ethylene-propylene (EPM) rubbers, where the weight ratio of (a):(b) is from 3:1 to 999:1.
The blends comprise(a) thermoplastic polyurethane having a Shore hardness of from 60 A to 50 D and(b) ethylene-propylene (EPM) rubbers and/or modified ethylene-propylene (EPM) rubbers,where the weight ratio of (a):(b) is from 3:1 to 999:1.
Die Erfindung betrifft Verfahren zur Herstellung von thermoplastischen Polyurethanen durch Umsetzung von (a) Isocyanaten mit (b) gegenüber Isocyanaten reaktiven Verbindungen mit einem Molekulargewicht von 500 bis 10000 g/mol, gegebenenfalls in Gegenwart von (c)…
The blends comprise(a) thermoplastic polyurethane having a Shore hardness of from 60 A to 50 D and(b) ethylene-propylene (EPM) rubbers and/or modified ethylene-propylene (EPM) rubbers,where the weight ratio of (a):(b) is from 3:1 to 999:1.