hottub.patents
EP 2,518,097 A3#519166 Most Cited · 0 citations0.0/yr · PR 0.97ActiveEP · Utility
Modified polyesters and processes for manufacturing the same

Disclosed herein are processes for manufacturing modified polyesters. An esterification reaction of diacid, diol and a branching agent having at least three carboxyl groups is carried out at a temperature of about 180 to 300°C and a pressure of about 1 to 4 bar to obtain a…

TW 201,525,058 A#497309 Most Cited · 0 citations0.0/yr · PR 0.97ActiveTW · Utility
Modified furan polyester and copolymerization method thereof

A modified furan polyester and a copolymerization method thereof is provided. In the copolymerization process, two-stage esterification method is used to increase the polymerization rate and solve the yellowing problem.

US 2023331823 A1#699961 Most Cited · 0 citations0.0/yr · PR 0.97PendingUS · Application
Shark-derived binding molecules for sars-cov-2 coronavirus and uses thereof

Disclosed herein are shark-derived antibodies and binding molecules with high binding affinity for SARS-CoV-2 coronavirus and the use thereof. Some of the shark-derived antibodies and binding molecules also demonstrate cross-reactivity with and neutralization of other related…

US 2024181376 A1#1694254 Most Cited · 0 citations0.0/yr · PR 0.97PendingUS · Application
Manufacturing method of meltblown fiber membrane
Inventors: Lin Ying-chi, Chen Wei-hungAssignee: Taiwan Textile Res InstFiled 2023-11-29

A manufacturing method of a meltblown fiber membrane includes the following step. A meltblown film is made to pass between a first pressing roller and a second pressing roller, such that a calendering process is performed on the meltblown film, in which the meltblown film…