US 3,656,364 A#6011121 Most Cited · 15 citations0.3/yr · PR 6.94ExpiredUS · Utility
Rack and holder
Inventors: Cable H Edward, Cable John AAssignee: Weld Tooling CorpFiled 1970-12-02 · Granted 1972-04-18

An improved rack and rack holder for cutting and welding torches, etc. wherein the rack includes a pair of tapered grooves throughout its length and the rack includes a pair of tapered elements cooperatively engaging said grooves.

US 3,985,495 A#11614496 Most Cited · 9 citations0.2/yr · PR 2.11ExpiredUS · Utility
Method and apparatus for fast firing glazed ceramic tile trim pieces
Inventors: Cable John A, Cable Stephen J, Falbo Richard RAssignee: Us Ceramic Tile CompanyFiled 1975-05-12 · Granted 1976-10-12

The method and apparatus for fast firing glazed ceramic tile trim pieces includes passing the trim pieces through a firing chamber by means of ceramic rollers which are designed to move the trim pieces in substantially a straight line through the chamber. The rollers include…

US 3,884,619 A#27818347 Most Cited · 3 citations0.1/yr · PR 1.90ExpiredUS · Utility
Method for fast firing glazed ceramic tile trim pieces
Inventors: Cable John A, Cable Stephen J, Falbo Richard RAssignee: Us Ceramic Tile CompanyFiled 1974-04-26 · Granted 1975-05-20

The method for fast firing glazed ceramic tile trim pieces includes passing the trim pieces through a firing chamber by means of ceramic rollers which are designed to move the trim pieces in substantially a straight line through the chamber. The rollers include trim piece…

DE 2,505,636 A1#149840530 Most Cited · 0 citations0.0/yr · PR 0.56PendingDE · Application
Firing glazed ceramic tiles - in roller hearth kiln and removing glaze from driven rolls
Inventors: Cable John A, Cable Stephen J, Falbo Richard RAssignee: Spartek IncFiled 1975-02-11

Deposits such as glaze formed on the driven rolls of a roller hearth furnace during firing of glazed ceramic tiles are removed without cooling the kiln by feeding absorbent low thermal expansion refractory shapes through the hot kiln. The kiln is preferably 50-350 degrees F…