The present invention pertains to an apparatus and method for treating a solution of high osmotic strength, especially seawater and solutions of greater than 20 bar osmotic pressure, by passing the solution through a vessel containing spiral wound reverse osmosis or…
Busch Markus
Process for preparing ethylene copolymers in the presence of free-radical polymerization initiator at pressures in the range of from 160 MPa to 350 MPa and temperatures in the range of from 100°C to 350°C in a tubular reactor by copolymerizing ethylene, a bi- or multifunctional…
Process for preparing ethylene homopolymers or copolymers in the presence of free-radical polymerization initiator and at least one chain transfer agent at pressures in the range of from 110 MPa to 350 MPa and temperatures in the range of from 100°C to 350°C in a tubular reactor…
The present invention pertains to an apparatus and method for treating a solution of high osmotic strength, especially seawater and solutions of greater than 20 bar osmotic pressure, by passing the solution through a vessel containing spiral wound reverse osmosis or…
Process for preparing ethylene homopolymers or copolymers in the presence of free-radical polymerization initiator and at least one chain transfer agent at pressures in the range of from 110 MPa to 350 MPa and temperatures in the range of from 100° C. to 350° C. in a tubular…
Process for preparing ethylene copolymers in the presence of free-radical polymerization initiator at pressures in the range of from 160 MPa to 350 MPa and temperatures in the range of from 100° C. to 350° C. in a tubular reactor by copolymerizing ethylene, a bi- or…
A process for preparing an ethylene homopolymer or copolymer in the presence of a free radical polymerization initiator and at least one chain transfer agent at a pressure of from 110MPa to 350MPa and a temperature of from 100 ℃ to 350 ℃ in a tubular reactor having at least two…
Provided is a process for preparing ethylene copolymers in the presence of free-radical polymerization initiator at pressures in the range of from 160 MPa to 350 MPa and temperatures in the range of from 100 DEG C to 350 DEG C in a tubular reactor, by copolymerizing ethylene, a…
A polymer composition may include a polymer produced from ethylene, one or more branched vinyl ester monomers, and optionally, vinyl acetate; wherein the polymer has a number average molecular weight ranging from 5 to 10,000 kDa, and a molecular weight distribution ranging from…
Process for preparing ethylene copolymers in the presence of free-radical polymerization initiator at pressures in the range of from 160 MPa to 350 MPa and temperatures in the range of from 100° C. to 350° C. in a tubular reactor by copolymerizing ethylene, a bi- or…
A process for preparing an ethylene copolymer in the presence of free-radical polymerization initiator at pressures from 150 MPa to 350 MPa and temperatures from 100° C. to 350° C., by copolymerizing ethylene and a comonomer having a C≡C bond and optionally further comonomers,…
A polymer composition may include a polymer produced from ethylene, one or more branched vinyl ester monomers, and optionally, vinyl acetate; wherein the polymer has a number average molecular weight ranging from 5 to 10,000 kDa, and a molecular weight distribution ranging from…
A polymer composition may include a polymer produced from ethylene, and one or more vinyl carbonyl monomers having the general structure (I): where R 1 , R 2 and R 3 are independently selected from a group consisting of hydrogen, halogen, hydroxyl, alkyl, substituted alkyl,…
본 발명은, 자유-라디칼 중합 개시제 및 하나 이상의 사슬 이동제의 존재 하에, 상이한 농도의 사슬 이동제를 갖는 둘 이상의 반응 구역을 갖는 튜브형 반응기에서 110 MPa 내지 350 MPa 범위의 압력 및 100℃ 내지 350℃ 범위의 온도에서 에틸렌 단일중합체 또는 공중합체를 제조하는 방법으로서, 이때 제 1 반응 구역에서의 사슬 이동제 농도가 최고 농도의 사슬 이동제를 갖는 반응 구역에서의 사슬 이동제 농도의 70% 미만인 방법, 이러한 방법에 의해 수득가능한 에틸렌 단일중합체 또는…
The present invention is directed toward a multi-pass hyperfiltration system (38) including at least two passes (42,44) of spiral wound modules positioned in series along a fluid pathway; including: a first pass is located upstream along the fluid pathway with respect to a…
The invention provides a process for preparing an ethylene copolymer by copolymerizing ethylene and at least one comonomer at pressures in the range of from 150 MPa to 350 MPa and temperatures in the range of from 50°C to 350°C by: (i) a process in the presence of a system…
The invention relates to a process for preparing a graft copolymer comprising polyethylene, comprising the steps of: A) providing an ethylene copolymer comprising side chains having C≡C bond and B) reacting the ethylene copolymer of step A) with an azide compound in the presence…
The present invention relates to a kind of methods being used to prepare the graft copolymer comprising polyethylene, the described method comprises the following steps:A) ethylene copolymer for including the side chain with C ≡ C keys is provided, and B) make step A) the…
A polymer composition may include a polymer produced from ethylene, one or more branched vinyl ester monomers, and optionally, vinyl acetate; wherein the polymer has a number average molecular weight ranging from 5 to 10,000 kDa, and a molecular weight distribution ranging from…
The present invention pertains to an apparatus and method for treating a solution of high osmotic strength, especially seawater and solutions of greater than 20 bar osmotic pressure, by passing the solution through a vessel containing spiral wound reverse osmosis or…
Process for preparing ethylene copolymers in the presence of free-radical polymerization initiator at pressures in the range of from 160 MPa to 350 MPa and temperatures in the range of from 100°C to 350°C in a tubular reactor by copolymerizing ethylene, a bi- or multifunctional…
Process for preparing ethylene homopolymers or copolymers in the presence of free-radical polymerization initiator and at least one chain transfer agent at pressures in the range of from 110 MPa to 350 MPa and temperatures in the range of from 100°C to 350°C in a tubular reactor…
A process for preparing an ethylene copolymer in the presence of free-radical polymerization initiator at pressures from 150 MPa to 350 MPa and temperatures from 100° C. to 350° C., by copolymerizing ethylene and a comonomer having a C≡C bond and optionally further comonomers,…