A semiconductor device ( 200 ) having support structures ( 218, 226, 236 ) beneath wirebond regions ( 214 ) of contact pads ( 204 ) and a method of forming same. Low modulus dielectric layers ( 216, 222, 232 ) are disposed over a workpiece ( 212 ). Support structures ( 218, 226,…
Burrell Lloyd
A method for sealing an exposed surface of a wire bond pad with a material that is capable of preventing a possible chemical attack during electroless deposition of Ni/Au pad metallurgy is provided. Specifically, the present invention provides a method whereby a TiN/Ti or TiN/Al…
A sensor for measuring cracks in a semiconductor device, such as a wafer and, more particularly, to a BEOL wirebond crack sensor for low-k dies or wafers, and a method of providing the wirebond crack sensor for low-k wafers or the like structures.
A process for forming fusible links in an integrated circuit includes forming the fusible link in the last metallization layer. The process can be employed in the fabrication of integrated circuits employing copper metallization and low k dielectric materials. The fusible link…
A sensor for measuring cracks in a semiconductor device, such as a wafer and, more particularly, to a BEOL wirebond crack sensor for low-k dies or wafers, and a method of providing the wirebond crack sensor for low-k wafers or the like structures.
A semiconductor device ( 200 ) having support structures ( 218, 226, 236 ) beneath wirebond regions ( 214 ) of contact pads ( 204 ) and a method of forming same. Low modulus dielectric layers ( 216, 222, 232 ) are disposed over a workpiece ( 212 ). Support structures ( 218, 226,…
A process for forming fusible links in an integrated circuit includes forming the fusible link in the last metallization layer. The process can be employed in the fabrication of integrated circuits employing copper metallization and low k dielectric materials. The fusible link…
A semiconductor device, and a method of fabricating the device, having a copper wiring level and an aluminum bond pad above the copper wiring level. In addition to a barrier layer which is normally present to protect the copper wiring level, there is a composite layer between…
Tungsten studs of a size comparable to vias are provided to integrate and interface between copper and aluminum metallization layers in an integrated circuit and/or package therefor by lining a via opening, preferably with layers of tantalum nitride and PVD tungsten as a barrier…
A semiconductor device, and a method of fabricating the device, having a copper wiring level and an aluminum bond pad above the copper wiring level. In addition to a barrier layer which is normally present to protect the copper wiring level, there is a composite layer between…
Tungsten studs of a size comparable to vias are provided to integrate and interface between copper and aluminum metallization layers in an integrated circuit and/or package therefor by lining a via opening, preferably with layers of tantalum nitride and PVD tungsten as a barrier…
Economical methods for forming a co-planar multi-chip wafer-level packages are proposed. Partial wafer bonding and partial wafer dicing techniques are used to create chips as well as pockets. The finished chips are then mounted in the corresponding pockets of a carrier…
A method for sealing an exposed surface of a wire bond pad with a material that is capable of preventing a possible chemical attack during electroless deposition of Ni/Au pad metallurgy is provided. Specifically, the present invention provides a method whereby a TiN/Ti or TiN/Al…
Economical methods for forming a co-planar multi-chip wafer-level packages are proposed. Partial wafer bonding and partial wafer dicing techniques are used to create chips as well as pockets. The finished chips are then mounted in the corresponding pockets of a carrier…
A method for sealing an exposed surface of a wire bond pad with a material that is capable of preventing a possible chemical attack during electroless deposition of Ni/Au pad metallurgy is provided. Specifically, the present invention provides a method whereby a TiN/Ti or TiN/Al…
Economical methods for forming a co-planar multi-chip wafer-level packages are proposed. Partial wafer bonding and partial wafer dicing techniques are used to create chips as well as pockets. The finished chips are then mounted in the corresponding pockets of a carrier…
Tungsten studs of a size comparable to vias are provided to integrate and interface between copper and aluminum metallization layers in an integrated circuit and/or package therefor by lining a via opening, preferably with layers of tantalum nitride and PVD tungsten as a barrier…
Economical methods for forming a co-planar multi-chip wafer-level packages are proposed. Partial wafer bonding and partial wafer dicing techniques are used to create chips as well as pockets. The finished chips are then mounted in the corresponding pockets of a carrier…
Economical methods for forming a co-planar multi-chip wafer-level packages are proposed. Partial wafer bonding and partial wafer dicing techniques are used to create chips as well as pockets. The finished chips are then mounted in the corresponding pockets of a carrier…
Tungsten studs of a size comparable to vias are provided to integrate and interface between copper and aluminum metallization layers in an integrated circuit and/or package therefor by lining a via opening, preferably with layers of tantalum nitride and PVD tungsten as a barrier…
A semiconductor device (200) having support structures (218, 226, 236) beneath wirebond regions (214) of contact pads (204) and a method of forming same. Low modulus dielectric layers (216, 222, 232) are disposed over a workpiece (212). Support structures (218, 226, 236) are…
Es werden eine Bondstruktur für ein Halbleitersubstrat und ein entsprechendes Verfahren bereitgestellt. Die Bondstruktur umfasst eine erste Oxidschicht auf dem Halbleitersubstrat und eine zweite Oxidschicht auf der ersten Oxidschicht, wobei die zweite Oxidschicht zum Verbinden…
Bondstruktur (100) für ein Halbleitersubstrat (114), wobei die Bondstruktur (100) umfasst:eine erste Oxidschicht (110) auf dem Halbleitersubstrat (114); undeine zweite Oxidschicht (120) auf der ersten Oxidschicht (110), wobei die zweite Oxidschicht (120) zum Verbinden mit einer…
Ein Prozeß zum Ausbilden von Schmelzsicherungen in einer integrierten Schaltung beinhaltet das Ausbilden der Schmelzsicherung in der letzten Metallisierungsschicht. Der Prozeß kann bei der Herstellung von integrierten Schaltungen verwendet werden, bei denen Kupfermetallisierung…
Economical methods for forming a co-planar multi-chip wafer-level packages are proposed. Partial wafer bonding and partial wafer dicing techniques are used to create chips as well as pockets. The finished chips are then mounted in the corresponding pockets of a carrier…