Patents
US 4,031,033 A#6555786 Most Cited · 14 citations0.3/yr · PR 7.48ExpiredUS · Utility
Method for producing powdered wetproofed material useful in making gas-diffusion electrodes

Powdered wetproofed materials, useful for the manufacture of gas-diffusion electrodes, are produced by forming a suspension of an electroconductive powder in a liquid which is water or an organic solvent in the presence of a wetproofing agent and recovering the wetproofed…

US 4,959,396 A#8084611 Most Cited · 12 citations0.3/yr · PR 3.26ExpiredUS · Utility
Composition for microporous separators and method for its preparation
Inventors: Yankov Lyuben K, Filipova Stefka K, Zlatanov Ivo Y, Budevski Evgeni BAssignee: Centralen Inst Chimitcheska PrFiled 1990-01-23 · Granted 1990-09-25

The composition comprises polyolefins, fillers and a plasticizer. It contains 0.2 to 20 wt. % etoxysiloxane, 5 to 60 wt. % polyolefin, 10 to 60 wt. % white black filler, and 10 to 75 wt. % polyethyleneglycol, petroleum oil or dioctylphtalate. The polyolefin can be high-density…

CN 1,032,772 A#18672754 Most Cited · 6 citations0.2/yr · PR 1.34ExpiredCN · Utility
The method and apparatus of electrochemical catalytic oxidation of sulphur dioxide

Sulfurous gas is become the vitriolic method with electrochemical catalytic oxidation, this method contacts with electrolytic solution-water or sulphuric acid soln on catalyst surface under 10 ℃~80 ℃ temperature of reaction based on the gaseous mixture that will contain 0.01~50…

EP 0,302,224 A2#19968585 Most Cited · 5 citations0.1/yr · PR 1.73PendingEP · Application
Process and apparatus for the electrochemical, catalytic oxidation of sulphur dioxide to sulphuric acid

The electrochemical, catalytic oxidation of sulphur dioxide to sulphuric acid is carried out by bringing a gas mixture having a sulphur dioxide content of 0.01 to 50% by volume simultaneously into contact with oxygen and an electrolyte - water or a solution of sulphuric acid -…

GB 2,212,509 A#61551180 Most Cited · 1 citations0.0/yr · PR 0.75ExpiredGB · Utility
Moulding composition for producing microporous battery separators

Microporous battery separators with an average pore size below 0.05 mu m and with satisfactory high physical/mechanical properties are produced from moulding compositions comprising 5 to 60% by weight of a polyolefin, from 10 to 60% by weight of finely divided silica, from 10 to…

BG 47,242 A1#115543729 Most Cited · 0 citations0.0/yr · PR 0.56PendingBG · Application
Method and device for electrochemical catalyst oxidation of sulphur dioxide

The electrochemical, catalytic oxidation of sulphur dioxide to sulphuric acid is carried out by bringing a gas mixture having a sulphur dioxide content of 0.01 to 50% by volume simultaneously into contact with oxygen and an electrolyte - water or a solution of sulphuric acid -…

CN 87,100,756 A#133705919 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCN · Utility
Lamp using electrochemical current

The invention relates to an active metal-air lamp using an electrochemical current source, comprising a housing 1 and a movable core A, which is firmly inserted into the housing and divides it into two equal parts. The core a comprises an air chamber with two air electrodes 6,…

CS 208,688 B2#85635549 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredCS · Utility
Method of making the powder material impregnated against the humidity,determinated for production of electrodes by the diffusing gas

1392341 Wetproofed carbon powder ZLEHIT PRI BAN 16 March 1972 [29 March 1971] 12445/72 Heading C1A [Also in Divisions D1 and H1] A method for producing powdered wetproofed materials, suitable for the production of gas diffusion electrodes, comprises mixing a…

DD 267,893 A7#73350466 Most Cited · 0 citations0.0/yr · PR 0.56ExpiredDD · Utility
Zusammensetzung fuer mikroporoese separatoren und verfahren fuer ihre herstellung

Die vorgeschlagene Zusammensetzung fuer mikroporoese Separatoren enthaelt von 5 bis 60 Gew.-% Polyolefin, von 10 bis 60 Gew.-% Weussruss, Weichmachungsmittel von 10 bis 75 Gew.-% und Aethoxysiloxan von 0,2 bis 20 Gew.-%. Das Aethoxysiloxan kann Tetraaethooxysiloxan oder…