The method consists in that the aluminum-silicon alloy is first treated with flux at a temperature not under 1,500*C, then it is treated with more of the same flux at 900*-1,200*C.
Inventor / Author Profile
Brusakov J
2Total Forward Citations
3Indexed Patents
1Patent H-Index
Frequent Co-Inventors: Alivoivodich M Avdeev M Berezhnoi I Cheltsov V Chernyakhovsky L Eltsova Z Kiselev V Kulikov A Livshits I Marin S Medvedeva L Volpin P
In an electric furnace relationship between the bath diameter ''''d,'''' the lining height ''''h'''' and the distance between the electrode axes ''''1'''' is such as to form a common…