STABILIZING COMPOSITIONS COMPRISING AT LEAST ONE TRIARYL PHOSPHITE, TRIALKYL PHOSPHITE OR MIXTURES THEREOF AND AT LEAST ONE MODIFIED LIGNIN, THE WEIGHT RATIO OF THE PHOSPHITE TO MODIFIED LIGNIN IS FROM 97/3 TO 10/90. THE MODIFIED LIGNINS ARE PRODUCED BY HEAT TREATING LIGNINS IN…
Inventor / Author Profile
Braddon D
8Total Forward Citations
3Indexed Patents
1Patent H-Index
ELASTOMERS MAY BE PROTECTED AGAINST ATMOSPHERIC DEGRADATION BY THE ADDITION THERETO OF 0.01 TO 5.0 PARTS BY WEIGHT, PREFERABLY 0.25 TO 2.0 PARTS, PER 100 PARTS OF ELASTOMER OF A MODIFIED LIGNIN STABILIZER. THE MODIFIED LIGNIN STABILIZERS ARE PRODUCED BY HEAT TREATING TECHNICAL…